# US 2022/0293311 A1 · R-t-b permanent magnet material and preparation method therefor and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293311 A1
- Document ID: US20220293311A1
- Status: Published application
- Kind: A1
- Application number: 17/637,522
- Filed: 2020-07-07
- Published: 2022-09-15
- Earliest claimed: 2019-11-21
- Assignees: Xiamen Tungsten Co., Ltd.; Fujian Changting Golden Dragon Rare-Earth Co., Ltd
- Applicants: Xiamen Tungsten Co., Ltd.; Fujian Changting Golden Dragon Rare-Earth Co., Ltd
- Inventors: Gang FU; Jiaying HUANG; Jixiang HUANG; Qichen QUAN
- Web page: https://patentgrep.com/patent/US20220293311A1

## CPC

- C22C 38/008: {containing tin}
- H01F 1/0577: {sintered}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/06: containing aluminium
- C22C 38/10: containing cobalt
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/32: with boron
- H01F 41/0293: {diffusion of rare earth elements, e.g. Tb, Dy or Ho, into permanent magnets}
- C22C 2202/02: Magnetic
- H01F 1/0573: {obtained by reduction or by hydrogen decrepitation or embrittlement}
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

An R-T-B permanent magnet material and a preparation method therefor and a use thereof. The R-T-B permanent magnet material comprises the following components: R′, which is between 29.5 wt. % and 33.0 wt. %, the R comprising R, Pr, and Nd, R being a rare earth element other than Pr and Nd, the Pr content being greater than or equal to 8.85 wt. %, the mass ratio of Nd to R being less than 0.5; N, which is greater than 0.05 wt. %, and less than or equal to 4.1 wt. %, the N being Ti, Zr, or Nb; B, which is between 0.90 wt. % and 1.2 wt. %; and Fe, which is between 62.0 wt. % and 68.0 wt. %. A sintered permanent magnet product having a high coercive force and a stable temperature coefficient is prepared by using a formulation having a high Pr content. The described formulation can maximally exert the advantage of Pr, and effectively reduce production costs.

## Claims

### Claim 1

An R-T-B permanent magnet material, which comprises the following components by mass percentage:
R′: 29.5-33.0 wt. %, R′ comprising R and Pr, Nd; wherein: R is a rare earth element other than Pr and Nd, the content of Pr is ≥8.85 wt. %, the mass ratio of Nd to R′ is <0.5;
N: ≥0.05 wt. %, and <4.1 wt. %, N being Ti, Zr or Nb;
B: 0.90-1.2 wt. %;
Fe: 62.0-68.0 wt. %.

### Claim 2 (depends on 1)

The R-T-B permanent magnet material according to claim 1,
wherein, the content of R′ is 30-33 wt. %, the percentage refers to the mass percentage in the R-T-B permanent magnet material;
or, the content of Nd is 11-15 wt. % the percentage refers to the mass percentage in the R-T-B permanent magnet material;
or, the mass ratio of Nd to R′ is ≥0.3 and <0.5;
or, the content of B is 0.9-1.0 wt. %, the percentage refers to the mass percentage in the R-T-B permanent magnet material;
or, the content of Fe is 62.3-68.0 wt. %, the percentage refers to the mass percentage in the R-T-B permanent magnet material.

### Claim 3 (depends on 1)

The R-T-B permanent magnetic material according to claim 1, wherein, the R-T-B permanent magnet material comprises the following components: R′: 29.5-33.0 wt. %, Pr≥17.00 wt. %, N: 0.1-4.01 wt. %, Cu: 0.30-0.55 wt. %, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt %; the percentage refers to the mass the percentage in the R-T-B permanent magnet material;
or, the R-T-B permanent magnet material comprises the following components: R′: 29.5-33.0 wt. %, Pr≥17.00 wt. %, N: 0.2-0.6 wt. %, Al: 0-0.8 wt. %, but not 0, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt. %; the percentage refers to the mass percentage in the R-T-B permanent magnet material;
or, the R-T-B permanent magnet material comprises the following components: R′: 29.5-33.0 wt. %, Pr≥17.00 wt. %, N: 0.2-0.6 wt. %, Ga: 0-0.81 wt. %, but not 0, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt. %; the percentage refers to the mass percentage in the R-T-B permanent magnet material;
or, the R-T-B permanent magnet material comprises the following components: R′: 29.5-33.0 wt. %, Pr≥17.00 wt. %, N: 0.2-0.6 wt. %, Cu: 0.30-0.55 wt. %, Al: 0-0.8 wt. %, but not 0, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt. %, the percentage refers to the mass percentage in the R-T-B permanent magnet material;
or, the R-T-B permanent magnet material comprises the following components: R′: 29.5-33.0 wt. %, Pr≥17.00 wt. %, N: 0.25-0.35 wt. %, Cu: 0.30-0.55 wt. %, Al: 0.45-0.7 wt. %, Ga: 0.2-0.6 wt. %, Co: 0.5-3.0 wt. %, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt. %, the percentage refers to the mass percentage in the R-T-B permanent magnet material;
or, the R-T-B permanent magnet material comprises the following components: R′: 29.5-33.0 wt. %, Pr≥17.00 wt. %, N: 0.25-0.35 wt. %, Cr: 0-0.15 wt. %, Cu: 0.30-0.55 wt. %, Al: 0.45-0.7 wt. %, Ga: 0.2-0.6 wt. %, Co: 0.5-3.0 wt. %, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt. %, the percentage refers to the mass percentage in the R-T-B permanent magnet material;
or, the R-T-B permanent magnet material comprises the following components: R′: 29.5-33.0 wt. %, Pr≥17.00 wt. %, RH: 1.0-2.5 wt. %, N: 0.25-0.35 wt. %, Cu: 0.30-0.55 wt. %, Al:
0.45-0.7 wt. %, Ga: 0.2-0.6 wt. %, Co: 0.5-3.0 wt. %, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt. %, the percentage refers to the mass percentage in the R-T-B permanent magnet material.

### Claim 4

A raw material composition of R-T-B permanent magnet material, which comprises the following components by mass percentage:
R′: 29.5-32.0 wt. %, R′ comprising R and Pr, Nd; wherein: R is a rare earth element other than Pr and Nd, the content of Pr is ≥8.85 wt. %, the mass ratio of Nd to R′ is <0.5;
N: ≥0.05 wt. %, and <4.0 wt. %, N being Ti, Zr or Nb;
B: 0.90-1.2 wt. %;
Fe: 62.0-68.0 wt. %.

### Claim 5 (depends on 4)

The raw material composition of R-T-B permanent magnet material according to claim 4, wherein, the content of R′ is 30.0-32.0 wt. %, the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, the content of Nd is 11.00-15.00 wt. %, the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, the mass ratio of Nd to R′ is ≥0.3 and <0.5;
or, the content of B is ≥0.985 wt. %;
or, the content of Fe is 62.81-67.92 wt. %, the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material.

### Claim 6 (depends on 4)

The raw material composition of R-T-B permanent magnet material according to claim 4, the raw material composition of R-T-B permanent magnet material comprises the following components: R′: 29.5-32.0 wt. %, Pr≥17.15 wt. %, N: 0.3-0.6 wt. %, Cu: 0.34-0.55 wt. %, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt. %; the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, the raw material composition of R-T-B permanent magnet material comprises the following components: R′: 29.5-32.0 wt. %, Pr≥17.15 wt. %, N: 0.2-0.6 wt. %, Al: 0-0.8 wt. %, but not 0, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt. %; the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, the raw material composition of R-T-B permanent magnet material comprises the following components: R′: 29.5-32.0 wt. %, Pr≥17.15 wt. %, N: 0.3-0.4 wt. %, Ga: 0.2-0.8 wt. %, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt. %; the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, the raw material composition of R-T-B permanent magnet material comprises the following components: R′: 29.5-32.0 wt. %, Pr≥17.15 wt. %, N: 0.2-0.6 wt. %, Cu: 0.30-0.5 wt. %, Al: 0-0.8 wt. %, but not 0, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt. %; the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, the raw material composition of R-T-B permanent magnet material comprises the following components: R′: 29.5-32.0 wt. %, Pr≥17.15 wt. %, N: 0.25-0.35 wt. %, Cu: 0.3-0.5 wt. %, Al: 0.5-0.7 wt. %, Ga: 0.2-0.6 wt. %, Co: 0.5-3.0 wt. %, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt. %; the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, the raw material composition of R-T-B permanent magnet material comprises the following components: R′: 29.5-32.0 wt. %, Pr≥17.15 wt. %, N: 0.25-0.35 wt. %, Cu: 0.3-0.5 wt. %, Al: 0.5-0.7 wt. %, Ga: 0.2-0.6 wt. %, Co: 0.5-3.0 wt. %, Cr: 0-0.15 wt. %, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt. %, the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, the raw material composition of R-T-B permanent magnet material comprises the following components: R′: 29.5-32.0 wt. %, Pr≥17.15 wt. %, RH: 1.0-2.5 wt. %, N: 0.25-0.35 wt. %, Cu: 0.30-0.55 wt. %, Al: 0.45-0.7 wt. %, Ga: 0.2-0.6 wt. %, Co: 0.5-3.0 wt. %, B: 0.9-1.0 wt. %, Fe: 62.0-68.0 wt. %, the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material.

### Claim 7 (depends on 4)

A preparation method for R-T-B permanent magnet material,
wherein, the preparation method comprises the following steps: the molten liquid of the raw material composition of the R-T-B permanent magnet material according to claim 4 is subjected to casting, hydrogen decrepitation, forming, sintering and aging.

### Claim 8 (depends on 7)

An R-T-B permanent magnet material prepared by the preparation method according to claim 7.

### Claim 9 (depends on 1)

An R-T-B permanent magnet material, wherein, the main phase crystalline particle is R″2Fe14B, the R″ comprises Pr and Nd, the mass fraction of Pr in the R″ is ≥60%;
the components of the R-T-B permanent magnet material are according to claim 1.

### Claim 10 (depends on 1)

A use of the R-T-B permanent magnet material according to claim 1 as electronic components.

### Claim 11 (depends on 1)

The R-T-B permanent magnet material according to claim 1, wherein, the content of Pr is 17.00-20.00 wt. %, the percentage refers to the mass percentage in the R-T-B permanent magnet material.

### Claim 12 (depends on 1)

The R-T-B permanent magnet material according to claim 1, wherein, the N is Zr, the content of Zr is 0.20-4.01 wt. %;
or, the N is Ti, the content of Ti is ≥0.25 wt. %;
or, the N is Nb, the content of Nb is ≥0.1 wt. %;
the percentage refers to the mass percentage in the R-T-B permanent magnet material.

### Claim 13 (depends on 1)

The R-T-B permanent magnet material according to claim 1, wherein, R′ further comprises R, R is a rare earth element other than Pr and Nd; the content of R is 0-1 wt. %, the percentage refers to the mass percentage in the R-T-B permanent magnet material;
or, R′ further comprises a heavy rare earth element RH; wherein, the kind of RH is selected from the group consisting of Dy and Tb; the content of RH is 1.0-2.5 wt. %, the percentage refers to the mass percentage of the R-T-B permanent magnet material.

### Claim 14 (depends on 1)

The R-T-B permanent magnet material according to claim 1, wherein, the R-T-B permanent magnet material further comprises Cu, the content of Cu is ≥0.30 wt. %, the percentage refers to the mass percentage in the R-T-B permanent magnet material;
or, the R-T-B permanent magnet material further comprises Al, the content of Al is 0-0.8 wt. %, but not 0, the percentage refers to the mass percentage in the R-T-B permanent magnet material;
or, the R-T-B permanent magnet material further comprises Ga, the content of Ga is 0.0-0.85 wt. %, but not 0, the percentage refers to the mass percentage in the R-T-B permanent magnet material;
or, the R-T-B permanent magnet material further comprises Co, the content of Co is 0.0-3.0 wt. %, but not 0, the percentage refers to the mass percentage in the R-T-B permanent magnet material;
or, the R-T-B permanent magnet material further comprises addition element M, and M is one or more of Ni, Zn, Ag, In, Sn, Bi, V, Cr, Hf, Ta, and W; the content of M is 0-0.15 wt. %, but not 0, the percentage refers to the mass percentage in the R-T-B permanent magnet material.

### Claim 15 (depends on 1)

The R-T-B permanent magnet material according to claim 1, wherein,
the content of Pr is 17.00-20.00 wt. %;
N is Ti or Zr;
when the N is Zr, the content of Zr is 1.49-4.01 wt. %;
when the N is Ti, the content of Ti is 1.51-4.01 wt. %;
the main phase crystalline particle of the R-T-B permanent magnet material is R″2Fe14B, the R″ comprises Pr and Nd, the mass fraction of Pr in the R″ is ≥60%;
Zr and Ti are dispersed in the main phase and grain boundary phase of in the R-T-B permanent magnet material.

### Claim 16 (depends on 4)

The raw material composition of R-T-B permanent magnet material according to claim 4, wherein, the content of Pr is 17.15-19.15 wt. %;
or, the N is Zr, the content of Zr is 0.25-4.0 wt. %;
or, the N is Ti, the content of Ti is ≥0.3 wt. %,
or, the N is Nb, the content of Nb is 0.15-0.30 wt. %;
the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material.

### Claim 17 (depends on 4)

The raw material composition of R-T-B permanent magnet material according to claim 4, wherein, R′ further comprises R, R is a rare earth element other than Pr and Nd, the content of R is 0-1 wt. %, the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, R′ further comprises a heavy rare earth element RH; the kind of RH is selected from the group consisting of Dy and Tb; the content of RH is 1.0-2.5 wt. %, the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, the raw material composition of R-T-B permanent magnet material further comprises Cu, the content of Cu is ≥0.34 wt. %, the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, the raw material composition of R-T-B permanent magnet material further comprises Al, the content of Al is 0.042-0.7 wt. %, the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, the raw material composition of R-T-B permanent magnet material further comprises Ga, the content of Ga is 0.0-0.8 wt. %, but not 0, the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, the raw material composition of R-T-B permanent magnet material further comprises Co, the content of Co is 0.0-3.0 wt. %, but not 0, the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material;
or, the raw material composition of R-T-B permanent magnet material further comprises addition element M, M is one or more of Ni, Zn, Ag, In, Sn, Bi, V, Cr, Hf, Ta, and W; the content of M is 0-0.15 wt. %, but not 0, the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material.

### Claim 18 (depends on 4)

The raw material composition of R-T-B permanent magnet material according to claim 4, wherein,
the content of Pr is 17.15-19.15 wt. %;
N is Ti or Zr;
when the N is Zr, the content of Zr is 1.5-4.0 wt. %;
when the N is Ti, the content of Ti is 1.5-4.0 wt. %;
the percentage refers to the mass percentage in the raw material composition of R-T-B permanent magnet material.

### Claim 19 (depends on 7)

The preparation method for R-T-B permanent magnet material according to claim 7, wherein, the molten liquid of the raw material composition of R-T-B permanent magnet material is prepared by the following method: melting in a high frequency vacuum induction melting furnace; the vacuum degree of the melting furnace is 5×10−2 Pa; the melting temperature is 1500° C. or less;
the casting process is carried out as follows: cooling at a rate of 102° C./s −104° C./s in an Ar atmosphere;
the hydrogen decrepitation process comprises hydrogen absorption, dehydrogenation and cooling treatment, the hydrogen absorption is carried out under the hydrogen pressure of 0.15 MPa;
the sintering process is carried out as follows: preheating, sintering and cooling under vacuum condition; the temperature of the preheating is 300-600° C., the time of the preheating is 1-2 h; the temperature of the sintering is 1040-1090° C.;
in the aging treatment, the temperature of the secondary aging is 500-650° C.; in the secondary aging, the temperature is increased to 500-650° C. with a heating rate of 3-5° C./min.

### Claim 20 (depends on 7)

The preparation method for R-T-B permanent magnet material according to claim 7, wherein, the grain boundary diffusion treatment is further carried out after sintering and before the aging treatment; the grain boundary diffusion treatment is carried out according to the following steps, attaching a substance selected from substance containing Tb and substance containing Dy to the surface of the R-T-B permanent magnet material by evaporating, coating or sputtering, then carrying out diffusion heat treatment; the temperature of the diffusion heat treatment is 800-900° C.; the time of the diffusion heat treatment is 12-48 h.