# US 2022/0293310 A1 · Rare-earth-based magnet powder, bonded magnet, bonded magnet compound, sintered magnet, method of manufacturing rare-earth-based magnet powder, and method of manufacturing rare-earth based permanent magnet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293310 A1
- Document ID: US20220293310A1
- Status: Published application
- Kind: A1
- Application number: 17/695,011
- Filed: 2022-03-15
- Published: 2022-09-15
- Earliest claimed: 2021-03-15
- Assignees: TDK Corporation
- Applicants: TDK Corporation
- Inventors: Ikuya KOKAWA; Yoshinori FUJIKAWA; Kenichi SUZUKI; Yasushi ENOKIDO
- Web page: https://patentgrep.com/patent/US20220293310A1

## CPC

- H01F 1/0557: {sintered}
- H01F 1/0578: {bonded together}
- H01F 1/0577: {sintered}
- H01F 7/02: Permanent magnets {[PM]}
- H01F 41/0293: {diffusion of rare earth elements, e.g. Tb, Dy or Ho, into permanent magnets}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

The rare-earth-based magnet powder has an average value of 0.65 or more as sphericity P1 defined by an equation (1) of P1=Ls/Ll. In the equation (1), Ll is a length or a long side of a rectangle that circumscribes the rare-earth-based magnet powder in a photomicrograph so that an area of the rectangle is minimized, and Ls is a length of a short side of the rectangle that circumscribes the rare-earth-based magnet powder in the photomicrograph so that the area of the rectangle is minimized.

## Claims

### Claim 1

A rare-earth-based magnet powder whose average value of sphericity P1 defined by an equation (1) of P1=Ls/Ll is 0.65 or more, wherein
Ll in the equation (1) is a length of a long side of a rectangle that circumscribes the rare-earth-based magnet powder in a photomicrograph so that an area of the rectangle is minimized:
Ls in the equation (1) is a length of a short side of the rectangle that circumscribes the rare-earth-based magnet powder in the photomicrograph so that the area of the rectangle is minimized; and
a quantity proportion of the rare-earth-based magnet powder comprising a single crystal is 65% or more.

### Claim 2 (depends on 1)

The rare-earth-based magnet powder according to claim 1, wherein
the quantity proportion of the rare-earth-based magnet powder having the sphericity P1 of 0.9 or more is 30% or more.

### Claim 3

A rare-earth-based magnet powder whose average value of sphericity P2 defined by an equation (2) of P2=Lt/Lr is 0.70 or more, wherein
Lr in the equation (2) is a perimeter length of the rare-earth-based magnet powder in a photomicrograph;
Lt in the equation (2) is a perimeter length of a perfect circle having the same area as that of the rare-earth-based magnet powder in the photomicrograph whose perimeter length Lr is calculated; and
the quantity proportion of the rare-earth-based magnet powder comprising the single crystal is 65% or more.

### Claim 4 (depends on 3)

The rare-earth-based magnet powder according to claim 3, wherein
a quantity proportion of the rare-earth-based magnet powder having the sphericity P2 of 0.8 or more is 25% or more.

### Claim 5 (depends on 1)

The rare-earth-based magnet powder according to claim 1, wherein
a mean particle diameter is 20 μm or less.

### Claim 6 (depends on 3)

The rare-earth-based magnet powder according to claim 3, wherein
a mean particle diameter is 20 μm or less.

### Claim 7 (depends on 1)

The rare-earth-based magnet powder according to claim 1, comprising
coated particles including individual particles each comprising a single main phase grain and having a surrounding surface at least partly covered with a coating layer.

### Claim 8 (depends on 3)

The rare-earth-based magnet powder according to claim 3, comprising
coated particles including individual particles each comprising a single main phase grain and having a surrounding surface at least partly covered with a coating layer.

### Claim 9 (depends on 7)

The rare-earth-based magnet powder according to claim 7, wherein
the individual particles include an entirely coated particle having the coating layer covering the entire surrounding surface of the particle.

### Claim 10 (depends on 8)

The rare-earth-based magnet powder according to claim 8, wherein
the individual particles include an entirely coated particle having the coating layer covering the entire surrounding surface of the particle.

### Claim 11 (depends on 7)

The rare-earth-based magnet powder according to claim 7, wherein
an average of the coverage ratios indicating a proportion of the surrounding surface of each of the individual particles covered with the coating layer is 50% or more.

### Claim 12 (depends on 8)

The rare-earth-based magnet powder according to claim 8, wherein
an average of the coverage ratios indicating a proportion of the surrounding surface of each of the individual particles covered with the coating layer is 50% or more.

### Claim 13 (depends on 1)

The rare-earth-based magnet powder according to claim 1, wherein
the rare-earth-based magnet powder includes an R-T-B based magnet powder.

### Claim 14 (depends on 3)

The rare-earth-based magnet powder according to claim 3, wherein
the rare-earth-based magnet powder includes an R-T-B based magnet powder.

### Claim 15 (depends on 1)

A bonded magnet including the rare-earth-based magnet powder according to claim 1.

### Claim 16 (depends on 3)

A bonded magnet including the rare-earth-based magnet powder according to claim 3.

### Claim 17 (depends on 1)

A bonded magnet compound including the rare-earth-based magnet powder according to claim 1.

### Claim 18 (depends on 3)

A bonded magnet compound including the rare-earth-based magnet powder according to claim 3.

### Claim 19

A rare-earth-based sintered magnet, wherein
a main phase and a subphase are observed in a cross section of the rare-earth-based sintered magnet and an area proportion of the subphase is 2% or less:
the main phase is R2 T14 B crystal; and
a crystal orientation calculated by dividing a residual magnetic flux density in an orientation direction by a saturation magnetic flux density is 94% or more.

### Claim 20

A method of manufacturing a rare-earth based magnet powder, comprising the steps of:
obtaining a raw material powder by pulverizing an alloy having a desired composition; and
feeding the raw material powder into a flame tip of a thermal plasma to heat the raw material powder and then rapidly cooling the heated powder so that a spheroidized powder is obtained.

### Claim 21

A method of manufacturing a rare-earth based magnet, comprising the steps of:
obtaining a raw material powder by pulverizing an alloy having a desired composition; and
feeding the raw material powder into a flame tip of a thermal plasma to heat the raw material powder and then rapidly cooling the heated powder so that a spheroidized powder is obtained; and