# US 2022/0291436 A1 · Polarizing plate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0291436 A1
- Document ID: US20220291436A1
- Status: Published application
- Kind: A1
- Application number: 17/635,657
- Filed: 2020-09-21
- Published: 2022-09-15
- Earliest claimed: 2019-09-23
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Eun Je Kim; Je Hyuk Yoo; Woo Yong Cho; Yun Ki Park; Byeong Won Lee
- Web page: https://patentgrep.com/patent/US20220291436A1

## CPC

- G02B 1/11: Anti-reflection coatings
- G02B 1/14: Protective coatings, e.g. hard coatings
- G02B 5/3016: {involving passive liquid crystal elements (optical properties of liquid crystals G02F1/0063; polarising elements associated with active liquid crystal devices G02F1/133528)}
- G02B 5/3083: {Birefringent or phase retarding elements (G02B5/3008, G02B5/3016 take precedence; systems for polarisation control G02B27/286; manufacturing phase modulating patterns by lithographic processes G03F7/001)}
- H10K 59/8791: {Arrangements for improving contrast, e.g. preventing reflection of ambient light}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

The present application can provide a thin polarizing plate having excellent antireflection performance in all directions including the side as well as the front, and having excellent folding durability and durability against short wavelengths. In addition, the present application can provide an organic light-emitting display device to which the polarizing plate is applied and a display device comprising the same.

## Claims

### Claim 1

A polarizing plate comprising:
a polarizing film;
a hard coating layer formed on top of the polarizing film; and
a retardation layer formed on bottom of the polarizing film.

### Claim 2 (depends on 1)

The polarizing plate according to claim 1, wherein the hard coating layer is formed directly on the top of the polarizing film without interposing other layers.

### Claim 3 (depends on 1)

The polarizing plate according to claim 1, wherein the hard coating layer has pencil hardness of 0.5H or more.

### Claim 4 (depends on 1)

The polarizing plate according to claim 1, wherein the hard coating layer has a thickness of 1 μm to 10 μm.

### Claim 5 (depends on 1)

The polarizing plate according to claim 1, wherein the polarizing plate has a total thickness of 45 μm or less.

### Claim 6 (depends on 1)

The polarizing plate according to claim 1, wherein the retardation layer comprises:
a first retardation layer located on the bottom of the polarizing film, having in-plane retardation according to Equation 1 below of 100 to 150 nm based on a wavelength of 550 nm, and disposed so that a small angle of angles formed by a slow axis with an absorption axis of the polarizing film forms an angle of 35 degrees to 55 degrees; and
a second retardation layer located on a bottom of the first retardation layer and having thickness direction retardation according to Equation 2 below of 30 to 150 nm based on a wavelength of 550 nm:
Rin=d×(nx−ny) [Equation 1]
Rth=d×(nz−ny) [Equation 2]
wherein, Rin is the in-plane retardation, Rth is the thickness direction retardation, d is the thickness of a first or second retardation layer, nx is the refractive index of the first or second retardation layer in the slow axis direction, ny is the refractive index of the first or second retardation layer in the fast axis direction, and nz is the refractive index of the first or second retardation layer in the thickness direction.

### Claim 7 (depends on 6)

The polarizing plate according to claim 6, wherein the first retardation layer has a dispersion coefficient of less than 1 according to Equation 3 below.
Dispersion coefficient=Rin(450)/Rin(550) [Equation 3]
wherein, Rin(450) is the in-plane retardation of the first retardation layer based on a wavelength of 450 nm, and Rin(550) is the in-plane retardation of the first retardation layer based on a wavelength of 550 nm.

### Claim 8 (depends on 1)

The polarizing plate according to claim 1, further comprising an isotropic layer, wherein the retardation layer is formed on a first surface of the isotropic layer, and a second surface of the isotropic layer is attached to the polarizing film.

### Claim 9 (depends on 1)

The polarizing plate according to claim 1, wherein the ratio (H/S) of a thickness (H) of the hard coating layer to a thickness (S) of the polarizing film is 0.01 to 1.5.

### Claim 10 (depends on 1)

The polarizing plate according to claim 1, wherein the ratio (H/T) of a thickness (H) of the hard coating layer to a thickness (T) of the retardation layer is 0.1 to 5.

### Claim 11 (depends on 8)

The polarizing plate according to claim 8, wherein the ratio (H/P) of a thickness (H) of the hard coating layer to a thickness (P) of the isotropic layer is 0.01 to 1.5.

### Claim 12 (depends on 1)

The polarizing plate according to claim 1, wherein a reflective color value change (ΔE*ab) according to Equation 4 below is 10 or less.
ΔE*ab=[(ΔL*)2+(Δa*)2+(Δb*)2]1/2 [Equation 4]
wherein, ΔL* is L*a-L*i, Δa* is a*a-a*i, Δb* is b*a-b*i, and L*a, a*a and b*a are color coordinates L*, a* and b* before exposing the polarizing plate to light having a wavelength of 420 nm in a light quantity of 0.75 to 0.85 W/m2 at a temperature of 25° C. for 50 hours, respectively, and L*i, a*i and b*i are color coordinates L*, a* and b* after exposing the polarizing plate to light having a wavelength of 420 nm in a light quantity of 0.75 to 0.85 W/m2 at a temperature of 25° C. for 50 hours.

### Claim 13 (depends on 1)

The polarizing plate according to claim 1, further comprising a pressure-sensitive adhesive layer formed only on a bottom of the retardation layer.

### Claim 14 (depends on 1)

An organic light-emitting display device comprising the polarizing plate of claim 1.

### Claim 15 (depends on 14)

A display device comprising the organic light-emitting display device of claim 14.