# US 2022/0291145 A1 · Method for characterizing defects in silicon crystal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0291145 A1
- Document ID: US20220291145A1
- Status: Published application
- Kind: A1
- Application number: 17/684,848
- Filed: 2022-03-02
- Published: 2022-09-15
- Earliest claimed: 2021-03-10
- Assignees: Zing Semiconductor Corporation; Shanghai Institute of Microsystem and Information Technology, Chinese Academy of Sciences
- Applicants: Zing Semiconductor Corporation; Shanghai Institute of Microsystem and Information Technology, Chinese Academy of Sciences
- Inventors: Xing WEI; Yun LIU; Zhongying XUE
- Web page: https://patentgrep.com/patent/US20220291145A1

## CPC

- G01N 21/9501: {Semiconductor wafers (manufacturing processes per se of semiconductor devices implementing a measuring step H10P74/20)}
- G01N 21/95607: {using a comparative method}
- C30B 29/06: Silicon
- G01N 1/32: Polishing; Etching
- G01N 21/95692: {Patterns showing hole parts, e.g. honeycomb filtering structures}
- G01N 2021/8477: {Investigating crystals, e.g. liquid crystals}
- G01N 2021/8864: {Mapping zones of defects}
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

The present application provides a method for characterizing defects in silicon crystal comprising the following steps: etching a surface of the silicon crystal to remove a predicted thickness of the silicon crystal; conducting a LLS scanning to a surface of the etched silicon crystal to obtain a LLS map of the surface, a LSE size of defects, and defect bulk density; based on at least one of the LLS map of the surface, the LSE size of defects and the defect bulk density, determining a type of defect existing in the silicon crystal and/or a defect zone of each type of defect on the surface. By applying the method, the characterizing period and the characterizing cost can be reduced, plural defects such as vacancy, oxygen precipitate and dislocation can be characterized simultaneously, the characterizing accuracy can be enhanced, and the defect type and the defect zone can be determined with high reliability. In addition, the method can be applied to all crystal defect types, is easy to operate, and is an environmentally friendly method for determination of grown-in defects.

## Claims

### Claim 1

A method for characterizing defects in silicon crystal comprising the following steps:
etching a surface of the silicon crystal to remove a predicted thickness of the silicon crystal;
conducting a localized light scattering (LLS) scanning to a surface of the etched silicon crystal to obtain a LLS map of the surface, a latex sphere equivalent (LSE) size of defects, and defect bulk density; and
determining a type of defect existing in the silicon crystal and/or a defect zone of each type of defect on the surface based on at least one of the LLS map of the surface, the LSE size of defects and the defect bulk density.

### Claim 2 (depends on 1)

The method of claim 1, wherein the step of etching comprising:
conducting a pretreatment to the silicon crystal surface to remove an oxidation layer on the silicon crystal surface;
etching the surface of the silicon crystal under atmosphere of a hydride of Group VII, at temperature of 700° C. or higher, for time period of 1 second (sec)-1000 sec, and with a flow rate of an etching gas of 100 sccm-1000 sccm.

### Claim 3 (depends on 1)

The method of claim 1, wherein the defect bulk density is calculated based on a number of defects caused by the etching and the predicted thickness.

### Claim 4 (depends on 1)

The method of claim 1, wherein the LLS scanning is conducted to obtain the LSE size of each defect, and determining the defect type based on the LSE size.

### Claim 5 (depends on 4)

The method of claim 4, wherein the step of determining the defect type based on the LSE size comprises:
before characterizing, establishing a relationship between the LSE size and the defect type;
during characterizing, obtaining the LSE size of a sample by the LLS scanning; and
comparing the obtained LSE size and the relationship to determining the defect type.

### Claim 6 (depends on 4)

The method of claim 4, wherein the LLS scanning is conducted to obtain a location of each defect on the surface, thereby to obtain the defect bulk density distributed along a radius; and
the defect zone of each type of defect is determined based on the defect type determined by the LSE size and the defect bulk density of each defect type, wherein each defect type has a number range of the defect bulk density.

### Claim 7 (depends on 6)

The method of claim 6, wherein the defect type has different number ranges of the defect bulk density at different thickness of the silicon crystal, such that the method further comprises obtaining the number range of the defect bulk density of the defect type at different thickness of the silicon crystal.

### Claim 8 (depends on 6)

The method of claim 6, wherein the defect zone of each defect type is determined based on the defect type, the defect bulk density of each defect type, and a regular pattern of adjacent defects.

### Claim 9 (depends on 1)

The method of claim 1, wherein the type of defect comprises a vacancy, an oxygen precipitate, a self-interstitial atom aggregation, and a dislocation.

### Claim 10 (depends on 1)

The method of claim 1, wherein the defect zone comprises a vacancy accumulation area, an oxidation-induced stacking fault area, a pure vacancy area, a pure self-interstitial atom area, and a self-interstitial atom aggregation area.

### Claim 11 (depends on 1)

The method of claim 1, wherein the defect type and the defect zone are determined based on the LLS map of the surface and a regular pattern of adjacent defects.