# US 2022/0291113 A1 · Method for evaluating delayed fracture of metal material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0291113 A1
- Document ID: US20220291113A1
- Status: Published application
- Kind: A1
- Application number: 17/635,876
- Filed: 2020-06-10
- Published: 2022-09-15
- Earliest claimed: 2019-08-16
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Naho INOUE; Shinji OTSUKA; Daisuke MIZUNO; Nobuyuki ISHIKAWA
- Web page: https://patentgrep.com/patent/US20220291113A1

## CPC

- G01N 17/02: Electrochemical measuring systems for weathering, corrosion or corrosion-protection measurement
- G01N 17/006: {of metals}
- G01N 17/002: {Test chambers}
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

A method for evaluating a delayed fracture characteristic of a metal material that performs a step including a step (A) and a step (B) below once or a plurality of times to evaluate the delayed fracture characteristic of the metal material having been processed. Step (A): a step that brings an aqueous solution which includes a chloride ion into contact with a surface of the metal material to cause chloride of 1000 to 100000 mg/m2 in chloride amount to deposit to the surface. Step (B): a step in which the metal material to which the chloride has deposited in the step (A) is left stationary in an air atmosphere at a temperature from −50 to 10° C. and at a relative humidity higher than or equal to a deliquescence humidity of the chloride.

## Claims

### Claim 1

A method for evaluating a delayed fracture characteristic of a metal material, the method comprising:
bringing an aqueous solution comprising a chloride ion into contact with a surface of the metal material such that chloride in an amount of from 1000 to 100000 mg/m2 is deposited on the surface thereof, and
leaving the metal material stationary in an air atmosphere at a temperature from −50 to 10° C. and at a relative humidity higher than or equal to a deliquescence humidity of the chloride,
wherein the bringing and the leaving are performed once or a plurality of times to evaluate the delayed fracture characteristic of the metal material.

### Claim 2 (depends on 1)

The method according to claim 1, wherein,
the bringing comprises depositing the chloride to the metal material in less than ten minutes by at least one selected from the group consisting of immersion, atomizing, showering, spraying, and dripping.

### Claim 3 (depends on 1)

The method according to claim 1, wherein a humidity in the air atmosphere is maintained at the relative humidity higher than or equal to a deliquescence humidity of the chloride during the leaving.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the method does not include a drying step where a humidity in the air atmosphere is lower than the deliquescence humidity of the chloride.