# US 2022/0287195 A1 · Foldable apparatus, ribbons, and methods of making

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0287195 A1
- Document ID: US20220287195A1
- Status: Published application
- Kind: A1
- Application number: 17/637,929
- Filed: 2020-08-28
- Published: 2022-09-08
- Earliest claimed: 2019-08-29
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: NAIGENG CHEN; MATTHEW WADE FENTON; TIMOTHY MICHAEL GROSS; YUHUI JIN; DHANANJAY JOSHI; KUAN-TING KUO; YOUSEF KAYED QAROUSH
- Web page: https://patentgrep.com/patent/US20220287195A1

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- H05K 5/03: Covers
- B32B 3/263: {characterised by a layer having non-uniform thickness}
- B32B 7/06: permitting easy separation
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 17/06: comprising glass as the main or only constituent of a layer, next to another layer of a specific {material}
- G06F 1/1652: {the display being flexible, e.g. mimicking a sheet of paper, or rollable}
- H04M 1/0214: {Foldable telephones, i.e. with body parts pivoting to an open position around an axis parallel to the plane they define in closed position (combined with translation movement H04M1/0235)}
- H04M 1/0268: {including a flexible display panel}
- H05K 5/0017: {with operator interface units}
- B32B 2307/732: Dimensional properties
- B32B 2457/20: Displays, e.g. liquid crystal displays, plasma displays
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- G06F: ELECTRIC DIGITAL DATA PROCESSING (computer systems based on specific computational models G06N)
- H04M: TELEPHONIC COMMUNICATION (circuits for controlling other apparatus via a telephone cable and not involving telephone switching apparatus G08)

## Abstract

Foldable apparatus can comprise a foldable substrate comprising a substrate thickness and a central portion positioned between a first portion and a second portion. The central portion can comprise a central thickness less than the substrate thickness. A first maximum tensile stress of a first tensile stress region in the first portion and a second maximum tensile stress of the second tensile stress region in the second portion can be less than a third maximum tensile stress of a central tensile stress region in the central portion. Ribbons can comprise a ribbon thickness and a central portion positioned between a first portion and a second portion. The central portion can comprise a first central compressive stress region and a second central compressive stress region. In some embodiments, methods of processing a ribbon can comprise masking the first portion, masking the second portion, and chemically strengthening the central portion.

## Claims

### Claim 1

A ribbon comprising:
a ribbon thickness defined between a first major surface and a second major surface opposite the first major surface;
a first portion comprising a first depth of layer from the first major surface from 0% to about 5% of the ribbon thickness and a second depth of layer from the second major surface from 0% to about 5% of the ribbon thickness;
a second portion comprising a third depth of layer from the first major surface from 0% to about 5% of the ribbon thickness and a fourth depth of layer from the second major surface from 0% to about 5% of the ribbon thickness; and
a central portion comprising a first central depth of layer from the first major surface of about 10% or more of the ribbon thickness, a first central compressive stress region extending to a first central depth of compression from the first major surface, a second central depth of layer from the second major surface of about 10% or more of the ribbon thickness, and a second central compressive stress region extending to a second central depth of compression from the second major surface,
wherein the central portion is positioned between the first portion and the second portion in a direction of a length of the ribbon.

### Claim 2 (depends on 1)

The ribbon of claim 1, wherein the first central depth of compression is in a range from about 10% to about 30% of the ribbon thickness.

### Claim 3 (depends on 1)

The ribbon of claim 1, further comprising a width defined between a first edge of the ribbon and a second edge of the ribbon opposite the first edge, the first edge extending between the first major surface and the second major surface, the second edge extending between the first major surface and the second major surface, and the first central compressive stress region and the second central compressive stress region each extends from the first edge to the second edge.

### Claim 4 (depends on 1)

The ribbon of claim 1, further comprising:
a first tensile stress region positioned between the first compressive stress region and the second compressive stress region, the first tensile stress region comprising a first maximum tensile stress;
a second tensile stress region positioned between the third compressive stress region and the fourth compressive stress region, the second tensile stress region comprising a second maximum tensile stress; and
a central tensile stress region positioned between the first central compressive stress region and the second central compressive stress region, the central tensile stress region comprising a central maximum tensile stress,
wherein the central maximum tensile stress is greater than the first maximum tensile stress and the central maximum tensile stress is greater than the second maximum tensile stress.

### Claim 5 (depends on 1)

The ribbon of claim 1, further comprising a central tensile stress region positioned between the first central compressive stress region and the second central compressive stress region, the central tensile stress region comprising a central maximum tensile stress ranging from about 10 MegaPascals to about 375 MegaPascals.

### Claim 6 (depends on 1)

The ribbon of claim 1, wherein the ribbon comprises a minimum bend radius less than 10 millimeters.

### Claim 7 (depends on 6)

The ribbon of claim 6, wherein the ribbon achieves a bend radius of 5 millimeters.

### Claim 8 (depends on 6)

The ribbon of claim 6, wherein a length of the central portion in the direction of the length of the ribbon is about 5 times the minimum bend radius or more.

### Claim 9 (depends on 1)

The ribbon of claim 1, wherein a length of the central portion in the direction of the length of the ribbon is in a range from about 5 millimeters to about 55 millimeters.

### Claim 10 (depends on 1)

The ribbon of claim 1, wherein the ribbon thickness is in a range from about 25 micrometers to about 150 micrometers.

### Claim 11 (depends on 1)

The ribbon of claim 1, wherein the ribbon exhibits a warp relative to a first plane defined by the first major surface in a range from about 10 nanometers to about 2 micrometers.

### Claim 12 (depends on 1)

The ribbon of claim 1, wherein the ribbon comprises a glass-based material.

### Claim 13 (depends on 1)

A foldable apparatus comprising:
the ribbon of claim 1;
an optically clear adhesive; and
a release liner, wherein the optically clear adhesive is positioned between the ribbon and the release liner.

### Claim 14 (depends on 1)

A consumer electronic product comprising:
a housing comprising a front surface, a back surface, and side surfaces;
electrical components at least partially within the housing, the electrical components comprising a controller, a memory, and a display, the display at or adjacent the front surface of the housing; and
a cover substrate disposed over the display, at least one of a portion of the housing or the cover substrate comprises the ribbon of claim 1.

### Claim 15

A method of processing a ribbon comprising:
masking a first portion of the ribbon comprising a first surface area of a first major surface of the ribbon and a second surface area of a second major surface of the ribbon opposite the first major surface;
masking a second portion of the ribbon comprising a third surface area of the first major surface and a fourth surface area of the second major surface; and
chemically strengthening a central portion of the ribbon to achieve a first central compressive stress region extending to a first central depth of compression from a central portion of the first major surface and a second central compressive stress region extending to a second central depth of compression from a central portion of the second major surface, wherein the central portion of the ribbon is positioned between the first portion and the second portion.

### Claim 16 (depends on 15)

The method of claim 15, wherein the chemically strengthening comprises:
disposing a salt solution on the central portion at the first major surface;
disposing the salt solution on the central portion at the second major surface; and
heating the ribbon at a temperature in a range from about 300° C. to about 500° C. for a time in a range from about 15 minutes to about 12 hours.

### Claim 17 (depends on 16)

The method of claim 16, wherein the first portion and the second portion are each unmasked before the heating the ribbon.

### Claim 18 (depends on 16)

The method of claim 16, wherein the salt solution comprises an organic binder, potassium nitrate and potassium phosphate.

### Claim 19 (depends on 16)

The method of claim 16, wherein the first central depth of compression is in a range from about 10% to about 30% of the ribbon thickness.

### Claim 20 (depends on 16)

The method of claim 16, wherein a length of the central portion of the ribbon in a direction of a length of the ribbon is in a range from about 5 millimeters to about 55 millimeters.