# US 2022/0285728 A1 · Sulfide solid electrolyte, method for producing sulfide solid electrolyte, electrode, and all solid state battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285728 A1
- Document ID: US20220285728A1
- Status: Published application
- Kind: A1
- Application number: 17/825,723
- Filed: 2022-05-26
- Published: 2022-09-08
- Earliest claimed: 2019-04-11
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: Hikaru SUGANUMA; Hanae SHIRATORI; Yuki KATOH
- Web page: https://patentgrep.com/patent/US20220285728A1

## CPC

- H01M 10/0562: Solid materials
- H01M 10/425: {Structural combination with electronic components, e.g. electronic circuits integrated to the outside of the casing (printed circuits H05K1/00)}
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A main object of the present disclosure is to provide a sulfide solid electrolyte with which an electrode having excellent ion transport efficiency can be obtained. The present disclosure achieves the object by providing a sulfide solid electrolyte comprising: a Li element, a P element, and a S element; wherein a tetrahydrofuran is also included; and BET specific surface area is 8.3 m2/g or more.

## Claims

### Claim 1 (depends on 1)

A method for producing a sulfide solid electrolyte, the sulfide solid electrolyte according to claim 1, the method comprising:
a precursor preparing step of mixing a raw material composition containing the constituent of the sulfide solid electrolyte with a tetrahydrofuran to obtain a precursor; and
a first burning step of volatilizing the tetrahydrofuran included in the precursor.

### Claim 2 (depends on 1)

The method for producing the sulfide solid electrolyte according to claim 1, wherein
burning temperature in the first burning step is a temperature less than the crystallization temperature of the sulfide solid electrolyte, and
the sulfide solid electrolyte is amorphous.

### Claim 3 (depends on 2)

The method for producing the sulfide solid electrolyte according to claim 2, wherein burning temperature in the first burning step is 100° C. or less.

### Claim 4 (depends on 1)

The method for producing the sulfide solid electrolyte according to claim 1, the method further comprising:
a second burning step of improving the crystallinity of the sulfide solid electrolyte after the first burning step; wherein
burning temperature in the second burning step is a temperature not less than the crystallization temperature of the sulfide solid electrolyte; and
the sulfide solid electrolyte is crystalline.

### Claim 5 (depends on 4)

The method for producing the sulfide solid electrolyte according to claim 4, wherein the burning temperature in the second burning step is 140° C. or more.

### Claim 6

An electrode to be used in an all solid state battery, the electrode comprising:
an active material and a sulfide solid electrolyte; wherein
a tetrahydrofuran is also included; and
when the volume rate of the sulfide solid electrolyte inside the electrode is regarded as ε, ion conductivity of the sulfide solid electrolyte is regarded as σSE, and ion conductivity of the electrode is regarded as σe1e, an ionic tortuosity factor obtained from ε*σSE/σe1e is 4.5 or less.

### Claim 7 (depends on 6)

An all solid state battery comprising:
a cathode active material layer, an anode active material layer, and a solid electrolyte layer formed between the cathode active material layer and the anode active material layer, wherein
at least one of the cathode active material layer and the anode active material layer is the electrode according to claim 6.