# US 2022/0285724 A1 · Method for producing solid electrolyte

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285724 A1
- Document ID: US20220285724A1
- Status: Published application
- Kind: A1
- Application number: 17/632,518
- Filed: 2020-08-06
- Published: 2022-09-08
- Earliest claimed: 2019-08-09
- Assignees: Idemitsu Kosan Co., Ltd.
- Applicants: Idemitsu Kosan Co., Ltd.
- Inventors: Shota TOTSUKA; Atsushi SATO; Hironari KIMPARA
- Web page: https://patentgrep.com/patent/US20220285724A1

## CPC

- H01B 1/10: sulfides
- H01M 10/0562: Solid materials
- C01B 25/14: Sulfur, selenium, or tellurium compounds of phosphorus
- C01P 2002/30: Three-dimensional structures
- H01M 2300/0065: Solid electrolytes
- H01M 2300/0068: inorganic
- H01M 2300/0091: in the form of mixtures
- Y02E 60/10: Energy storage using batteries
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for producing a solid electrolyte, which comprises: a step of mixing an anionic surfactant which is a monomer or an oligomer, a solvent, and a sulfide solid electrolyte to obtain a mixture; and a step of removing the solvent from the mixture.

## Claims

### Claim 1

A method for producing a solid electrolyte, comprising:
mixing an anionic surfactant which is a monomer or an oligomer, a solvent, and a sulfide solid electrolyte to obtain a mixture; and
removing the solvent from the mixture.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the surfactant comprises sulfosuccinate or benzenesulfonate.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the surfactant has an alkyl group including 5 or more carbon atoms, and the total number of carbon atoms of the alkyl groups is 5 or more and 20 or less.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the number of terminals of alkyl groups in the surfactant is 1 or more and 8 or less.

### Claim 5 (depends on 1)

The method according to claim 1, further comprising:
dehydrating a solution comprising the surfactant and using the dehydrated surfactant.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the solution comprising the surfactant comprises a polar solvent, and
the solvent comprises a nonpolar solvent.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the polar solvent is at least one selected from the group consisting of water and an alcohol.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the surfactant does not have a hydroxyl group.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the surfactant is mixed to be 0.01 to 5.0 mg/m2 per a specific surface area of the sulfide solid electrolyte.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the sulfide solid electrolyte has a crystal structure.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the sulfide solid electrolyte has an argyrodite-type crystal structure.

### Claim 12

A solid electrolyte, which comprises a sulfide solid electrolyte, and an anionic surfactant which is a monomer or an oligomer on the surface of the sulfide solid electrolyte,
wherein the amount of the surfactant is 0.01 to 5.0 mg/m2 per a specific surface area of the sulfide solid electrolyte.