# US 2022/0285723 A1 · Method And System For Safety Of Silicon Dominant Anodes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285723 A1
- Document ID: US20220285723A1
- Status: Published application
- Kind: A1
- Application number: 17/193,850
- Filed: 2021-03-05
- Published: 2022-09-08
- Earliest claimed: 2021-03-05
- Applicants: Enevate Corporation
- Inventors: Benjamin Park; Hong Zhao; Heidi Anderson; Mya Le Thai
- Web page: https://patentgrep.com/patent/US20220285723A1

## CPC

- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/625: {Carbon or graphite}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/056: characterised by the materials used as electrolytes, e.g. mixed inorganic/organic electrolytes
- H01M 10/0562: Solid materials
- H01M 50/417: Polyolefins
- H01M 50/434: Ceramics
- H01M 50/451: comprising layers of only organic material and layers containing inorganic material
- H01M 2004/027: {Negative electrodes}
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- H01M 2300/008: Halides
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY

## Abstract

Systems and methods provide for safety of silicon dominant anodes in a battery. The battery may include an anode comprising an anode active material layer on a metal current collector, where the anode active material layer comprises pyrolyzed binder, conductive additives, and 50% or more silicon by weight. The battery may further include a separator, an electrolyte, a cathode, and a solid electrolyte interface between the anode active material layer and the electrolyte, and has a thermal runaway temperature of greater than 260° C. The conductive additives may comprise between 1% and 40% of the active material layer. The anode active material layer may comprise between 20% to 95% silicon. The separator may comprise ceramic-coated polyolefin or polymer-coated polyolefin. The electrolyte may comprise Lithium hexafluorophosphate (LiPF6) and/or lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) in one or more electrolyte solvents. The metal current collector may comprise copper.

## Claims

### Claim 1

A battery comprising:
an anode comprising an anode active material layer on a metal current collector, the anode active material layer comprising pyrolyzed binder, conductive additives, and 50% or more silicon by weight;
a separator;
an electrolyte;
a cathode; and
a solid electrolyte interface between the anode active material layer and the electrolyte;
wherein a composition of one or both of the anode and the electrolyte and/or a formation process of the battery are configured such that the battery has a thermal runaway temperature of greater than 200° C.

### Claim 2 (depends on 1)

The battery according to claim 1, wherein the conductive additives comprise between 1% and 40% of the active material layer by weight.

### Claim 3 (depends on 1)

The battery according to claim 1, wherein the anode active material layer comprises between 20% to 95% silicon by weight.

### Claim 4 (depends on 1)

The battery according to claim 1, wherein the separator comprises ceramic-coated polyolefin.

### Claim 5

(canceled)

### Claim 6 (depends on 1)

The battery according to claim 1, wherein the electrolyte comprises 20% or more FEC by weight.

### Claim 7 (depends on 1)

The battery according to claim 1, wherein upon heating, the anode does not go into thermal runaway before the cathode.

### Claim 8

(canceled)

### Claim 9 (depends on 1)

The battery according to claim 1, wherein the battery does not go into thermal runaway when punctured by a nail.

### Claim 10 (depends on 1)

The battery according to claim 1, wherein a temperature of the battery when punctured by a nail does not rise by more than 2° C.

### Claim 11 (depends on 1)

The battery according to claim 1, wherein the battery has a thermal runaway temperature of greater than 260° C.

### Claim 12

A method for battery safety, the method comprising providing a battery comprising an anode comprising an anode active material layer on a metal current collector, the anode active material layer comprising pyrolyzed binder, conductive additives, and 50% or more silicon by weight;
a separator;
an electrolyte;
a cathode; and
a solid electrolyte interface between the anode active material layer and the electrolyte;
wherein a composition of one or both of the anode and the electrolyte and/or a formation process of the battery are configured such that the battery has a thermal runaway temperature of greater than 200° C.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the conductive additives comprise between 1% and 40% of the active material layer by weight.

### Claim 14 (depends on 12)

The method according to claim 12, wherein the anode active material layer comprises between 20% to 95% silicon by weight.

### Claim 15 (depends on 12)

The method according to claim 12, wherein the separator comprises ceramic-coated polyolefin.

### Claim 16

(canceled)

### Claim 17 (depends on 12)

The method according to claim 12, wherein the electrolyte comprises 20% or more FEC by weight.

### Claim 18

(canceled)

### Claim 19 (depends on 12)

The method according to claim 12, wherein upon heating, the anode does not go into thermal runaway before the cathode.

### Claim 20 (depends on 12)

The method according to claim 12, wherein the battery does not go into thermal runaway when punctured by a nail.

### Claim 21 (depends on 12)

The method according to claim 12, wherein a temperature of the battery when punctured by a nail does not rise by more than 2° C.

### Claim 22 (depends on 12)

The method according to claim 12, wherein the battery has a thermal runaway temperature of greater than 260° C.

### Claim 23

(canceled)

### Claim 24 (depends on 1)

The battery according to claim 1, wherein:
wherein the electrolyte comprises lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) in one or more electrolyte solvents; and
the LiTFSI is present at concentration of about 0 to 2.0 molar (M).

### Claim 25 (depends on 12)

The method according to claim 12, wherein:
wherein the electrolyte comprises lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) in one or more electrolyte solvents; and
providing the LiTFSI such that when present the LiTFSI is at concentration of about 0 to 2.0 molar (M).

### Claim 26 (depends on 1)

The battery according to claim 1, wherein upon heating, the solid electrolyte interface does not begin to decompose until 60+/−5° C.

### Claim 27 (depends on 12)

The method according to claim 12, wherein upon heating, the solid electrolyte interface does not begin to decompose until 60+/−5° C.