# US 2022/0285722 A1 · Electrode assembly manufacturing method, electrode assembly, and electrochemical device including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285722 A1
- Document ID: US20220285722A1
- Status: Published application
- Kind: A1
- Application number: 17/637,934
- Filed: 2020-10-16
- Published: 2022-09-08
- Earliest claimed: 2019-10-21
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: In Hyouk SUNG; Sang Joon LEE; Kyung Ryun KA
- Web page: https://patentgrep.com/patent/US20220285722A1

## CPC

- H01M 10/058: Construction or manufacture
- H01M 50/414: Synthetic resins, e.g. thermoplastics or thermosetting resins
- H01M 10/0463: {Cells or batteries with horizontal or inclined electrodes}
- H01M 10/049: {Processes for forming or storing electrodes in the battery container}
- H01M 10/446: {Initial charging measures}
- H01M 50/403: Manufacturing processes of separators, membranes or diaphragms
- H01M 50/417: Polyolefins
- H01M 50/449: having a layered structure
- H01M 50/46: Separators, membranes or diaphragms characterised by their combination with electrodes
- H01M 50/491: Porosity
- H01M 10/0427: {Button cells}
- H01M 10/052: Li-accumulators
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 50/434: Ceramics
- H01M 50/451: comprising layers of only organic material and layers containing inorganic material
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed is an electrode assembly manufacturing method, in which, in a step of stacking and pressing electrodes and a separator, the pressing is performed in that state in which pores of a porous substrate are filled with a polymer solution. The form or volume of the pores is not changed due to the polymer solution. Consequently, porosity of the separator after manufacture of an electrode assembly is similar to porosity of the separator before stacking. As a result, a battery including the electrode assembly has high ionic conductivity and excellent performance.

## Claims

### Claim 1

An electrode assembly manufacturing method comprising:
1) dissolving a polymer soluble in an electrolytic solution in a solvent to form a polymer solution;
2) filling pores of a porous substrate to be used as a separator with the polymer solution of step 1) to form a separator;
3) manufacturing a stack comprising the separator of step 2) and at least one electrode by pressing;
4) injecting a primary electrolytic solution into the stack of step 3) to discharge the polymer solution in the pores of the separator to an outside of the stack; and
5) injecting a secondary electrolytic solution into the stack of step 4).

### Claim 2 (depends on 1)

The electrode assembly manufacturing method according to claim 1, wherein the solvent of step 1) is not an electrolytic solution.

### Claim 3 (depends on 1)

The electrode assembly manufacturing method according to claim 1, wherein filling the pores of the porous substrate with the polymer solution of step 2) comprises applying the polymer solution to the porous substrate or impregnating the porous substrate with the polymer solution.

### Claim 4 (depends on 1)

The electrode assembly manufacturing method according to claim 1, further comprising drying the separator after step 2).

### Claim 5 (depends on 1)

The electrode assembly manufacturing method according to claim 1, further comprising further coating at least one surface of the separator after step 2).

### Claim 6 (depends on 1)

The electrode assembly manufacturing method according to claim 1, wherein the stack comprises a heat resistance layer in step 3).

### Claim 7 (depends on 1)

The electrode assembly manufacturing method according to claim 1, wherein the pressing of step 3) is performed at a pressure of 3 MPa to 20 MPa and a temperature of from 50° C. to 100° C.

### Claim 8 (depends on 1)

The electrode assembly manufacturing method according to claim 1, wherein the primary electrolytic solution and the secondary electrolytic solution are mixable with each other.

### Claim 9 (depends on 1)

The electrode assembly manufacturing method according to claim 1, wherein the primary electrolytic solution and the secondary electrolytic solution are identical to each other.

### Claim 10 (depends on 1)

The electrode assembly manufacturing method according to claim 1, wherein
the polymer soluble in the electrolytic solution in step 1) is a PVdF-based polymer, and
the solvent is an organic solvent.

### Claim 11 (depends on 1)

The electrode assembly manufacturing method according to claim 1, further comprising performing initial charging and discharging after step 5).

### Claim 12 (depends on 1)

An electrode assembly manufactured by the manufacturing method according to claim 1.

### Claim 13 (depends on 12)

An electrochemical device comprising the electrode assembly according to claim 12.