# US 2022/0285715 A1 · Ionomer dispersion having high dispersion stability, method for producing same, and polymer electrolyte membrane produced using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285715 A1
- Document ID: US20220285715A1
- Status: Published application
- Kind: A1
- Application number: 17/628,345
- Filed: 2020-09-29
- Published: 2022-09-08
- Earliest claimed: 2019-09-30
- Assignees: Kolon Industries, Inc.
- Applicants: Kolon Industries, Inc.
- Inventors: Na Young KIM; Dong Hoon LEE; Eun Su LEE; Jung Hwa PARK; Seung Jib YUM; Chang Hoon OH; Hye Song LEE
- Web page: https://patentgrep.com/patent/US20220285715A1

## CPC

- C09D 127/18: Homopolymers or copolymers of tetrafluoroethene
- H01M 8/1039: halogenated, e.g. sulfonated polyvinylidene fluorides
- C08F 214/262: {with fluorinated vinyl ethers}
- C08J 5/2237: {containing fluorine}
- C08L 81/06: Polysulfones; Polyethersulfones
- H01M 8/1004: characterised by membrane-electrode assemblies [MEA] (H01M8/12 takes precedence)
- H01M 8/1067: characterised by their physical properties, e.g. porosity, ionic conductivity or thickness
- C08J 2327/18: Homopolymers or copolymers of tetrafluoroethylene
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed are: an ionomer dispersion having high dispersion stability while also containing high content of ionomer solids, thus optimizing the ionomer morphology in a polymer electrolyte membrane to allow both the ion conductivity and durability of the polymer electrolyte membrane to be improved; a method for producing the ionomer dispersion; and a polymer electrolyte membrane produced using the method.

## Claims

### Claim 1

An ionomer dispersion comprising:
a dispersion medium; and
an ionomer solid in the dispersion medium,
wherein a concentration of the ionomer solid in the ionomer dispersion is 20% by weight or more, and
when a viscosity of the ionomer dispersion is measured using a rheometer while a shear rate is increasing from 0.001 s−1 to 1,000 s−1 and then decreasing from 1,000 s−1 to 0.001 s−1, a viscosity ratio of the ionomer dispersion defined by the following Equation 1 is 1.7 or less:
Viscosity ratio=η2/η1 Equation 1:
wherein η1 is a first viscosity of the ionomer dispersion, measured while the shear rate is increasing, when the shear rate is 1 s−1, and
η2 is a second viscosity of the ionomer dispersion, measured while the shear rate is decreasing, when the shear rate is 1 s−1.

### Claim 2 (depends on 1)

The ionomer dispersion according to claim 1, wherein the first viscosity and the second viscosity are 1 Pa·s or less.

### Claim 3 (depends on 1)

The ionomer dispersion according to claim 1, wherein, when a shear stress of the ionomer dispersion is measured using a rheometer while the shear rate is increasing from 0.001 s−1 to 1,000 s−1 and then decreasing from 1,000 s−1 to 0.001 s−1, a shear stress ratio of the ionomer dispersion defined by the following Equation 2 is 1.5 or less:
Shear stress ratio=σ2/σ1 Equation 2:
wherein σ1 is a first shear stress which is a shear stress of the ionomer dispersion, measured while the shear rate is increasing, when the shear rate is 1 s−1, and
σ2 is a second shear stress which is a shear stress of the ionomer dispersion, measured while the shear rate is decreasing, when the shear rate is 1 s−1.

### Claim 4 (depends on 3)

The ionomer dispersion according to claim 3, wherein the first shear stress and the second shear stress are 1 Pa·s or less.

### Claim 5 (depends on 1)

The ionomer dispersion according to claim 1, wherein the ionomer solid comprises a fluorinated ionomer, a hydrocarbon-based ionomer, or a mixture thereof.

### Claim 6 (depends on 1)

The ionomer dispersion according to claim 1, wherein the ionomer solid comprises a perfluorinated sulfonic acid-based ionomer (PFSA-based ionomer).

### Claim 7 (depends on 1)

The ionomer dispersion according to claim 1, wherein the concentration of the ionomer solid in the ionomer dispersion is 20 to 50% by weight.

### Claim 8

A method for preparing an ionomer dispersion comprising:
adding an ionomer to a dispersion medium such that a content of an ionomer solid is adjusted to 20% by weight or more; and
mixing the dispersion medium with the ionomer using a resonant acoustic method.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the mixing comprises applying acoustic energy with a frequency of 10 to 100 Hz to the dispersion medium and the ionomer, whereby subjecting the dispersion medium and the ionomer to resonant vibration at an acceleration of 50 G to 100 G, wherein G is gravitational acceleration.

### Claim 10 (depends on 8)

The method according to claim 8, wherein the mixing is performed for 5 to 60 minutes.

### Claim 11 (depends on 8)

The method according to claim 8, further comprising applying a pressure of 500 to 1,000 bar to a mixture of the dispersion medium and the ionomer, obtained through the mixing.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the pressure is applied to the mixture when the mixture is flowing.

### Claim 13 (depends on 1)

A polymer electrolyte membrane comprising:
a porous support having a plurality of pores; and
an ionomer formed by impregnating and coating the porous support with the ionomer dispersion according to claim 1, and then removing the dispersion medium from the ionomer dispersion.

### Claim 14 (depends on 13)

A membrane-electrode assembly comprising:
an anode;
a cathode; and
the polymer electrolyte membrane according to claim 13, interposed between the anode and the cathode.