# US 2022/0285670 A9 · Methods of forming electrochemical cells

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285670 A9
- Document ID: US20220285670A9
- Status: Published application
- Kind: A9
- Application number: 16/749,851
- Filed: 2020-01-22
- Published: 2022-09-08
- Earliest claimed: 2017-12-07
- Assignees: Enevate Corporation
- Applicants: Enevate Corporation
- Inventors: Benjamin Yong Park; Ian Russell Browne; Heidi Leighette Anderson
- Web page: https://patentgrep.com/patent/US20220285670A9

## CPC

- H01M 4/0447: {of complete cells or cells stacks}
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 50/46: Separators, membranes or diaphragms characterised by their combination with electrodes
- H01M 4/364: {as mixtures}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/625: {Carbon or graphite}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY

## Abstract

Methods of forming electrochemical cells are described. In some implementations, the method can include providing an electrochemical cell having an electrode including electrochemically active material with at least about 20% to about 100% by weight of silicon. The method can include charging the electrochemical cell by providing a formation charge current at about 1 C or greater to the electrochemical cell. The method can also include discharging the electrochemical cell. In various implementations, substantially no rest of greater than about 5 minutes occurs between charging and discharging.

## Claims

### Claim 1

A method of forming an electrochemical cell, the method comprising:
providing an electrochemical cell comprising:
a first electrode and a second electrode, wherein at least the first electrode comprises electrochemically active material having at least about 20% to about 100% by weight of silicon;
a separator between the first electrode and the second electrode; and
an electrolyte in contact with the first electrode, the second electrode, and the separator, wherein the electrochemical cell has a rated capacity of 1 C;
charging the electrochemical cell by providing a formation charge current at about 1 C or greater to the electrochemical cell; and
discharging the electrochemical cell, wherein substantially no rest of greater than about 5 minutes occurs between charging and discharging.

### Claim 2 (depends on 1)

The method of claim 1, wherein no rest occurs between the charging and discharging.

### Claim 3 (depends on 1)

The method of claim 1, wherein the formation charge current is provided at less than or equal to about 20 C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the formation charge current is provided at greater than about 2 C.

### Claim 5 (depends on 4)

The method of claim 4, wherein the formation charge current is provided at 4 C or greater.

### Claim 6 (depends on 5)

The method of claim 5, wherein the formation charge current is provided at less than or equal to about 20 C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the formation charge current is provided for about 3 minutes to about 60 minutes.

### Claim 8 (depends on 1)

The method of claim 1, wherein providing the formation charge current comprises charging to partial State of Charge (SOC).

### Claim 9 (depends on 8)

The method of claim 8, wherein charging to partial SOC comprises charging to about 10% to about 90% of total capacity of the electrochemical cell.

### Claim 10 (depends on 9)

The method of claim 9, wherein charging to partial SOC comprises charging to about 20% to about 70% of the total capacity of the electrochemical cell.

### Claim 11 (depends on 10)

The method of claim 10, wherein charging to partial SOC comprises charging to about 30% to about 50% of the total capacity of the electrochemical cell.

### Claim 12 (depends on 1)

The method of claim 1, wherein the formation charge current is provided at about 1 C to about 10 C up to a State of Charge (SOC) of about 10% to about 50%.

### Claim 13 (depends on 12)

The method of claim 12, wherein the formation charge current is provided at about 2 C to about 6 C up to an SOC of about 20% to about 40%.

### Claim 14 (depends on 1)

The method of claim 1, wherein providing the formation charge current comprises providing a substantially constant formation charge current.

### Claim 15 (depends on 1)

The method of claim 1, wherein providing the formation charge current comprises providing the formation charge current at a charge voltage from about 3 volts to about 6 volts.

### Claim 16 (depends on 1)

The method of claim 1, wherein the electrochemical cell is a lithium-ion battery and providing the formation charge current comprises providing the formation charge current with substantially no lithium plating.

### Claim 17 (depends on 1)

The method of claim 1, wherein the first electrode is an anode.

### Claim 18 (depends on 1)

The method of claim 1, wherein the first electrode comprises a silicon-dominant electrode.

### Claim 19 (depends on 1)

The method of claim 1, wherein the first electrode comprises the electrochemically active material having the silicon at about 30% to about 100% by weight.

### Claim 20 (depends on 19)

The method of claim 19, wherein the first electrode comprises the silicon at about 40% to about 100% by weight.

### Claim 21 (depends on 20)

The method of claim 20, wherein the first electrode comprises the silicon at about 50% to about 100% by weight.

### Claim 22 (depends on 21)

The method of claim 21, wherein the first electrode comprises the silicon at about 60% to about 100% by weight.

### Claim 23 (depends on 22)

The method of claim 22, wherein the first electrode comprises the silicon at about 70% to about 100% by weight.

### Claim 24 (depends on 23)

The method of claim 23, wherein the first electrode comprises the silicon at about 80% to about 100% by weight.

### Claim 25 (depends on 1)

The method of claim 1, wherein the first electrode comprises a silicon-carbon composite material film.

### Claim 26 (depends on 25)

The method of claim 25, wherein the composite material film is a self-supported composite structure.

### Claim 27 (depends on 25)

The method of claim 25, wherein the film is attached to a current collector.

### Claim 28 (depends on 1)

The method of claim 1, wherein the second electrode comprises Lithium Nickel-Cobalt-Manganese oxide (NCM).

### Claim 29 (depends on 1)

The method of claim 1, wherein the first electrode further comprises graphite.