# US 2022/0285669 A1 · Electrochemical slurry compositions and methods for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285669 A1
- Document ID: US20220285669A1
- Status: Published application
- Kind: A1
- Application number: 17/825,826
- Filed: 2022-05-26
- Published: 2022-09-08
- Earliest claimed: 2012-06-13
- Assignees: 24M Technologies, Inc.
- Applicants: 24M Technologies, Inc.
- Inventors: Tristan DOHERTY; Pimpa LIMTHONGKUL; Asli BUTROS; Mihai DUDUTA; James C. CROSS, III
- Web page: https://patentgrep.com/patent/US20220285669A1

## CPC

- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- C22B 26/12: Obtaining lithium
- H01G 11/30: characterised by their material
- H01G 11/38: Carbon pastes or blends; Binders or additives therein
- H01G 11/46: Metal oxides
- H01G 11/86: specially adapted for electrodes (carbonisation or activation of carbon for the manufacture of electrodes H01G11/34)
- H01M 4/02: Electrodes composed of, or comprising, active material
- H01M 4/0411: {by extrusion}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02E 60/13: Energy storage using capacitors
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Embodiments described herein generally relate to semi-solid suspensions, and more particularly to systems and methods for preparing semi-solid suspensions for use as electrodes in electrochemical devices such as, for example batteries. In some embodiments, a method for preparing a semi-solid electrode includes combining a quantity of an active material with a quantity of an electrolyte to form an intermediate material. The intermediate material is then combined with a conductive additive to form an electrode material. The electrode material is mixed to form a suspension having a mixing index of at least about 0.80 and is then formed into a semi-solid electrode.

## Claims

### Claim at position 1

1-49. (canceled)

### Claim 50

A method comprising:
mixing an active material with an electrolyte and a conductive additive via twin screw extrusion to form a semi-solid electrode material having a homogeneous composition;
controlling a temperature of the semi-solid electrode material during mixing to control the homogeneous composition of the semi-solid electrode material;
forming the semi-solid electrode material into a first electrode;
forming a second electrode; and
combining the first electrode and the second electrode to form an electrochemical cell.

### Claim 51 (depends on 50)

The method of claim 50, wherein the semi-solid electrode material is a suspension of the active material and the conductive additive in the electrolyte.

### Claim 52 (depends on 50)

The method of claim 50, further comprising:
mixing the semi-solid electrode material until the semi-solid electrode material has an electronic conductivity of at least about 10−6 S/cm.

### Claim 53 (depends on 50)

The method of claim 50, further comprising:
mixing the semi-solid electrode material until the semi-solid electrode material has an apparent viscosity of less than about 100,000 Pa-s at an apparent shear rate of 1,000 s−1.

### Claim 54 (depends on 50)

The method of claim 50, wherein the active material is about 20% to about 75% by volume of the semi-solid electrode material.

### Claim 55 (depends on 50)

The method of claim 50, wherein the electrolyte is about 25% to about 70% by volume of the semi-solid electrode material.

### Claim 56 (depends on 50)

The method of claim 50, wherein the conductive additive is about 0.5% to about 25% by volume of the semi-solid electrode material.

### Claim 57 (depends on 50)

The method of claim 50, wherein the semi-solid electrode material has a percolating conductive network and a mixing index of at least about 0.8.

### Claim 58 (depends on 50)

The method of claim 50, wherein temperature of the semi-solid electrode material is controlled during mixing to control a rate of evaporation of the electrolyte from the semi-solid electrode.

### Claim 59 (depends on 50)

The method of claim 50, wherein the mixing of the active material with the electrolyte and the conductive additive is performed with a mixing energy of at least about 90 J/g.

### Claim 60

A method comprising:
mixing an active material and an electrolyte with a conductive additive via twin screw extrusion to form a semi-solid electrode material having a homogeneous composition; and
controlling a temperature of the semi-solid electrode material during mixing to control the homogeneous composition of the semi-solid electrode material.

### Claim 61 (depends on 60)

The method of claim 60, wherein the active material is about 20% to about 75% by volume of the semi-solid electrode material, the conductive additive is about 0.5% to about 25% by volume of the semi-solid electrode material, and the electrolyte is about 25% to about 70% by volume of the semi-solid electrode material.

### Claim 62 (depends on 60)

The method of claim 60, wherein the semi-solid electrode material has a percolating conductive network and a mixing index of at least about 0.8.

### Claim 63 (depends on 60)

The method of claim 60, wherein temperature of the semi-solid electrode material is controlled during mixing to control a rate of evaporation of the electrolyte from the semi-solid electrode.

### Claim 64 (depends on 60)

The method of claim 60, wherein the mixing of the active material with the electrolyte and the conductive additive is performed with a mixing energy of at least about 90 J/g.

### Claim 65

A method comprising:
mixing an active material and an electrolyte with a conductive additive in a twin screw extruder to form a semi-solid electrode material having a homogeneous composition;
controlling a predetermined temperature of the semi-solid electrode material during mixing to control the homogeneous composition of the semi-solid electrode material; and
forming the semi-solid electrode material into an electrode,
wherein the twin screw extruder is configured to impart a specific mixing energy to the semi-solid electrode material.

### Claim 66 (depends on 65)

The method of claim 65, wherein the vessel of the mixer is cooled to the predetermined temperature of lower than 10 degrees Celsius during mixing.

### Claim 67 (depends on 65)

The method of claim 65, wherein the semi-solid electrode material has a percolating conductive network and a mixing index of at least about 0.8.

### Claim 68 (depends on 65)

The method of claim 65, wherein temperature of the semi-solid electrode material is controlled during mixing to control a rate of evaporation of the electrolyte from the semi-solid electrode.

### Claim 69 (depends on 65)

The method of claim 65, wherein the mixing of the active material with the electrolyte and the conductive additive is performed with a mixing energy of at least about 90 J/g.