# US 2022/0285667 A1 · Cathode active material for lithium secondary battery and lithium secondary battery including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285667 A1
- Document ID: US20220285667A1
- Status: Published application
- Kind: A1
- Application number: 17/534,202
- Filed: 2021-11-23
- Published: 2022-09-08
- Earliest claimed: 2021-03-08
- Assignees: SK Innovation Co., Ltd.
- Applicants: SK Innovation Co., Ltd.
- Inventors: Sang Min PARK; Tae Kyoung Lee; Sang Bok Kim; Jik Soo Kim; Sang Hye Shin; Yu Na Shim; Jeong Bae Yoon
- Web page: https://patentgrep.com/patent/US20220285667A1

## CPC

- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- C01G 53/42: containing alkali metals, e.g. LiNiO2
- C01G 53/82: Compounds containing nickel, with or without oxygen or hydrogen, and containing two or more other elements
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/52: containing elements as dopants
- C01P 2002/54: one element only
- C01P 2004/04: obtained by TEM, STEM, STM or AFM
- C01P 2004/45: Aggregated particles or particles with an intergrown morphology
- C01P 2006/40: Electric properties
- C01P 2006/80: Compositional purity
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The cathode active material for a lithium secondary battery according to embodiments of the present invention includes lithium-transition metal composite oxide particles including a plurality of primary particles, and the lithium-transition metal composite oxide particles have a lithium-potassium-containing portion formed between the primary particles. Thereby, it is possible to improve life-span properties and capacity properties by preventing the layer structure deformation of the primary particles and removing residual lithium.

## Claims

### Claim 1

A cathode active material for a lithium secondary battery comprising:
a lithium-transition metal composite oxide particle including a plurality of primary particles,
wherein the lithium-transition metal composite oxide particle comprises a lithium-potassium-containing portion formed between the primary particles.

### Claim 2 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein the lithium-potassium-containing portion comprises a lithium-potassium-sulfur-containing portion including lithium, potassium and sulfur.

### Claim 3 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein the primary particles have a hexagonal close-packed structure.

### Claim 4 (depends on 3)

The cathode active material for a lithium secondary battery according to claim 3, wherein the lithium-transition metal composite oxide particle has no primary particle having a face centered cubic structure.

### Claim 5 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein a sulfur content of the lithium-transition metal composite oxide particle measured through a carbon-sulfur (CS) analyzer is 1,100 to 4,500 ppm based on a total weight of the lithium-transition metal composite oxide particle.

### Claim 6 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein a potassium concentration of the lithium-potassium-containing portion measured through energy dispersive spectroscopy (EDS) is greater than the potassium concentration in the primary particles measured through the EDS.

### Claim 7 (depends on 6)

The cathode active material for a lithium secondary battery according to claim 6, wherein an average potassium signal value of the lithium-potassium-containing portion measured through the EDS is 1.2 to 4 times greater than the average potassium signal value in the primary particles measured through the EDS.

### Claim 8 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein a content of lithium carbonate (Li2CO3) remaining on the surface of the lithium-transition metal composite oxide particle is 2,500 ppm or less, and a content of lithium hydroxide (LiOH) remaining on the surface of the lithium-transition metal composite oxide particle is 2,500 ppm or less.

### Claim 9

A method of manufacturing a cathode active material for a lithium secondary battery, comprising:
preparing a preliminary lithium-transition metal composite oxide particle;
mixing the preliminary lithium-transition metal composite oxide particle with a potassium compound aqueous solution; and
performing a heat treatment on the mixed preliminary lithium-transition metal composite oxide particle and the potassium compound aqueous solution, to prepare a lithium-transition metal composite oxide particle comprising a plurality of primary particles and a lithium-potassium-containing portion formed between the primary particles.

### Claim 10 (depends on 9)

The method of manufacturing a cathode active material for a lithium secondary battery according to claim 9, wherein the potassium compound aqueous solution is formed by mixing a solvent with potassium compound powder, and
an input amount of the potassium compound powder is 0.2 to 1.9% by weight based on a total weight of the preliminary lithium-transition metal composite oxide particle.

### Claim 11 (depends on 10)

The method of manufacturing a cathode active material for a lithium secondary battery according to claim 10, wherein an input amount of the solvent is 2 to 15% by weight based on the total weight of the preliminary lithium-transition metal composite oxide particle.

### Claim 12 (depends on 10)

The method of manufacturing a cathode active material for a lithium secondary battery according to claim 10, wherein the potassium compound powder is potassium hydrogen sulfate (KHSO4) powder.

### Claim 13 (depends on 9)

The method of manufacturing a cathode active material for a lithium secondary battery according to claim 9, wherein the heat treatment is performed at 200 to 400° C. under an oxygen atmosphere.

### Claim 14 (depends on 9)

The method of manufacturing a cathode active material for a lithium secondary battery according to claim 9, wherein the preliminary lithium-transition metal composite oxide particle is mixed with the potassium compound aqueous solution without water washing treatment.

### Claim 15 (depends on 1)

A lithium secondary battery comprising:
a cathode comprising a cathode active material layer including the cathode active material for a lithium secondary battery according to claim 1; and