# US 2022/0285662 A1 · Method of manufacturing an electrode for an all-solid-state battery and an electrode for an all-solid-state battery manufactured thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285662 A1
- Document ID: US20220285662A1
- Status: Published application
- Kind: A1
- Application number: 17/509,894
- Filed: 2021-10-25
- Published: 2022-09-08
- Earliest claimed: 2021-03-08
- Assignees: Hyundai Motor Company; Kia Corporation
- Applicants: Hyundai Motor Company; Kia Corporation
- Inventors: Kyung Yup Song; Dae Yang Oh
- Web page: https://patentgrep.com/patent/US20220285662A1

## CPC

- H01M 4/0435: {Rolling or calendering}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/139: Processes of manufacture
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/052: Li-accumulators
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 10/0562: Solid materials
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of manufacturing an electrode for an all-solid-state battery is performed in a dry manner using first and second rollers. An electrode for an all-solid-state battery having an electrode layer with a desired thickness and a desired density of a mixture material may be manufactured by adjusting conditions of the first and the second rollers. The manufacturing speed may be accelerated, because there is no drying process, so that the efficiency of the manufacturing is improved. The process of thickening an electrode is realized by using the method and the porosity of the electrode for an all-solid-state battery manufactured thereby is excellent.

## Claims

### Claim 1

A method of manufacturing an electrode for an all-solid-state battery, the method comprising:
preparing a mixture for an electrode, the mixture including a solid electrolyte and an active material;
manufacturing an electrode sheet by compressing the mixture for an electrode with at least one pair of first rollers;
manufacturing a composite sheet by providing a current collector sheet on the electrode sheet; and
obtaining an electrode for an all-solid-state battery by compressing the composite sheet with at least one pair of second rollers,
wherein a diameter of each of the second rollers is 4 to 10 times larger than a diameter of each of the first rollers, and the electrode for an all-solid-state battery comprises:
a current collecting layer; and
an electrode layer positioned on the current collecting layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the diameter of each of the first rollers is 1 cm to 5 cm.

### Claim 3 (depends on 1)

The method of claim 1, wherein the number of the first rollers is 1 pair to 7 pairs.

### Claim 4 (depends on 3)

The method of claim 3, wherein a rolling rate of one of the pairs of first rollers is 10% to 30%.

### Claim 5 (depends on 3)

The method of claim 3, wherein a distance between the pairs of first rollers is 10 cm or less.

### Claim 6 (depends on 1)

The method of claim 1, wherein a thickness ratio of the electrode sheet is 120% to 130% when a thickness of the electrode layer in the electrode for an all-solid-state battery is set to 100%.

### Claim 7 (depends on 1)

The method of claim 1, wherein a thickness of the electrode sheet is 150 μm to 500 μm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the diameter of each of the second rollers is 4 cm to 50 cm.

### Claim 9 (depends on 1)

The method of claim 1, wherein a rolling rate of the second rollers is 15% to 30%.

### Claim 10 (depends on 1)

The method of claim 1, wherein the number of the second rollers is 1 pair to 2 pairs.

### Claim 11 (depends on 1)

The method of claim 1, wherein a temperature of each of the first rollers and each of the second rollers is 150° C. or less.

### Claim 12 (depends on 1)

An electrode for an all-solid-state battery manufactured according to the method of claim 1, the electrode comprising:
a current collecting layer; and
an electrode layer positioned on the current collecting layer.

### Claim 13 (depends on 12)

The electrode of claim 12, wherein a thickness of the electrode layer is 200 μm to 400 μm.