# US 2022/0285613 A1 · Phase-change random access memory device and method of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285613 A1
- Document ID: US20220285613A1
- Status: Published application
- Kind: A1
- Application number: 17/826,350
- Filed: 2022-05-27
- Published: 2022-09-08
- Earliest claimed: 2020-02-07
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company Limited
- Inventors: Jau-Yi WU
- Web page: https://patentgrep.com/patent/US20220285613A1

## CPC

- H10N 70/231: {based on solid-state phase change, e.g. between amorphous and crystalline phases, Ovshinsky effect}
- G11C 13/0004: {comprising amorphous/crystalline phase transition cells}
- G11C 13/003: {Cell access}
- G11C 13/0035: {Evaluating degradation, retention or wearout, e.g. by counting writing cycles}
- H10B 63/30: {comprising selection components having three or more electrodes, e.g. transistors}
- H10N 70/021: {Formation of switching materials, e.g. deposition of layers}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/8828: {Tellurides, e.g. GeSbTe}
- G11C 2213/79: Array wherein the access device being a transistor
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- G11C: STATIC STORES (semiconductor memory devices H10B)
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A phase-change memory device and method of manufacturing the same, the memory device including: a substrate; a bottom electrode disposed over the substrate; a top electrode disposed over the bottom electrode; and a phase-change layer disposed between the top and bottom electrodes. The phase change layer includes a chalcogenide Ge—Sb—Te (GST) material that includes at least 30 at % Ge and that is doped with a dopant including N, Si, Sc, Ga, C, or any combination thereof.

## Claims

### Claim 1

A memory device comprising:
a bottom electrode;
a top electrode disposed over the bottom electrode; and
a phase-change layer disposed between the top electrode and bottom electrode, the phase change layer comprising:
an upper sublayer comprising a chalcogenide germanium (Ge)-antimony (At)-tellurium (Te) (GST) material that comprises at least 30 at % Ge;
a lower sublayer comprising a GST material; and
a middle sublayer disposed between the upper sublayer and the lower sublayer and comprising a GST material,
wherein the lower sublayer directly contacts the bottom electrode, a Ge content of the lower sublayer is from about 10 at % to about 30 at % greater than a Ge content of the upper sublayer, and a Ge content of the middle sublayer is greater than the Ge content of the upper sublayer and is less than the Ge content of the lower sublayer.

### Claim 2 (depends on 1)

The memory device of claim 1, wherein the phase-change layer has a crystallization temperature of at least 200° C.

### Claim 3 (depends on 1)

The memory device of claim 1, further comprising:
a first conductive line electrically connected to the bottom electrode; and
a second conductive line electrically connected to the top electrode,
wherein the first conductive line and the second conductive line are different ones of a word line and a bit line.

### Claim 4 (depends on 3)

The memory device of claim 3, wherein:
the top electrode and the bottom electrode comprise titanium nitride (TiN); and
the first conductive line and the second conductive line comprise Cu.

### Claim 5 (depends on 1)

The memory device of claim 1, further comprising:
a barrier electrode disposed on the phase-change layer; and
a selector layer disposed between the barrier electrode and the top electrode.

### Claim 6 (depends on 1)

The memory device of claim 1, further comprising:
a field effect transistor that is electrically connected to the bottom electrode; and
a dielectric layer comprising a through-hole,
wherein the bottom electrode is disposed in the through-hole.

### Claim 7 (depends on 1)

The memory device of claim 1, further comprising a dielectric material that surrounds the top electrode, the bottom electrode, and the phase-change layer,
wherein the top electrode directly contacts the phase-change layer.

### Claim 8 (depends on 1)

The memory device of claim 1, wherein the upper sublayer, the lower sublayer and the middle sublayer are doped with a dopant comprising nitrogen (N), silicon (Si), scandium (Sc), gallium (Ga), carbon (C), or any combination thereof.

### Claim 9 (depends on 1)

The memory device of claim 1, wherein:
the upper sublayer comprises:
from about 35 at % to about 45 at % Ge;
from about 15 at % to about 25 at % Sb; and
from about 35 at % to about 45 at % Te;
the middle sublayer comprises:
from about 45 at % to about 55 at % Ge;
from about 13 at % to about 23 at % Sb; and
from about 27 at % to about 37 at % Te; and
the lower sublayer comprises:
from about 55 at % to about 65 at % Ge;
from about 11 at % to about 21 at % Sb; and
from about 19 at % to about 29 at % Te.

### Claim 10 (depends on 9)

The memory device of claim 9, wherein the upper sublayer directly contacts the top electrode.

### Claim 11

A memory device comprising:
a bottom electrode;
a top electrode disposed over the bottom electrode; and
a phase-change layer disposed between the top electrode and bottom electrode, the phase change layer comprising:
an upper sublayer comprising a chalcogenide germanium (Ge)-antimony (At)-tellurium (Te) (GST) material that comprises at least 30 at % Ge; and
a lower sublayer comprising a GST material,
wherein the lower sublayer directly contacts the bottom electrode, and a Ge content of the lower sublayer is from about 10 at % to about 30 at % greater than a Ge content of the upper sublayer.

### Claim 12 (depends on 11)

The memory device of claim 11, wherein:
the upper sublayer comprises:
from about 35 at % to about 45 at % Ge;
from about 15 at % to about 25 at % Sb; and
from about 35 at % to about 45 at % Te; and
the lower sublayer comprises:
from about 55 at % to about 65 at % Ge;
from about 11 at % to about 21 at % Sb; and
from about 19 at % to about 29 at % Te.

### Claim 13 (depends on 11)

The memory device of claim 11, further comprising:
a barrier electrode disposed on the phase-change layer; and
a selector layer disposed between the barrier electrode and the top electrode.

### Claim 14 (depends on 11)

The memory device of claim 11, further comprising a dielectric material that surrounds the top electrode, the bottom electrode, and the phase-change layer, wherein the top electrode directly contacts the phase-change layer.

### Claim 15 (depends on 11)

The memory device of claim 11, wherein the upper sublayer and the lower sublayer are doped with a dopant comprising nitrogen (N), silicon (Si), scandium (Sc), gallium (Ga), carbon (C), or any combination thereof.

### Claim 16 (depends on 11)

The memory device of claim 11, further comprising:
a first conductive line electrically connected to the bottom electrode; and
a second conductive line electrically connected to the top electrode,
wherein the first conductive line and the second conductive line are different ones of a word line and a bit line.

### Claim 17 (depends on 11)

The memory device of claim 11, wherein:
the phase-change layer has a crystallization temperature of at least 200° C.;
the top electrode and the bottom electrode comprise titanium nitride (TiN); and
the first conductive line and the second conductive line comprise Cu.

### Claim 18 (depends on 11)

The memory device of claim 11, further comprising:
a field effect transistor that is electrically connected to the bottom electrode; and
a dielectric layer comprising a through-hole,
wherein the bottom electrode is disposed in the through-hole.

### Claim 19

A memory device comprising:
a bottom electrode;
a top electrode disposed over the bottom electrode; and
a phase-change layer disposed between the top electrode and bottom electrode, the phase change layer comprising:
an upper sublayer comprising a chalcogenide germanium (Ge)-antimony (At)-tellurium (Te) (GST) material that comprises from about 35 at % to about 45 at % Ge; and
a lower sublayer comprising a GST material that comprises from about 55 at % to about 65 at % Ge,
wherein the lower sublayer directly contacts the bottom electrode.

### Claim 20 (depends on 19)

The memory device of claim 19, wherein:
the upper sublayer and the lower sublayer are doped with a dopant comprising nitrogen (N), silicon (Si), scandium (Sc), gallium (Ga), carbon (C), or any combination thereof;
the phase-change layer has a crystallization temperature of at least 200° C.;
the upper sublayer comprises:
from about 15 at % to about 25 at % Sb; and
from about 35 at % to about 45 at % Te; and
the lower sublayer comprises:
from about 11 at % to about 21 at % Sb; and
from about 19 at % to about 29 at % Te.