# US 2022/0285564 A1 · Buried Zener Design

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285564 A1
- Document ID: US20220285564A1
- Status: Published application
- Kind: A1
- Application number: 17/192,060
- Filed: 2021-03-04
- Published: 2022-09-08
- Earliest claimed: 2021-03-04
- Assignees: NXP B.V.
- Applicants: NXP B.V.
- Inventors: Saumitra Raj Mehrotra; Kejun Xia
- Web page: https://patentgrep.com/patent/US20220285564A1

## CPC

- H10D 8/25: Zener diodes
- H10D 8/022: {of Zener diodes}
- H10D 62/128: {Anode regions of diodes}
- H10D 62/129: {Cathode regions of diodes}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/21: {of electrically active species}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10D 62/834: further characterised by the dopants
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for manufacturing a Zener diode includes implanting an N-type Buried Layer (NBL) with an N-type dopant in a first epitaxial layer, wherein the NBL comprises an NBL opening excluding the N-type dopant. A P-type Buried Layer (PBL) having a peak PBL doping concentration below the NBL is implanted. A second epitaxial layer is grown over the NBL. A P-type region (Plink) is implanted to couple to the PBL above the NBL opening, and to couple the Plink to an Anode electrode. An N-type region (Nlink) is implanted to couple the NBL to a Cathode electrode.

## Claims

### Claim 1

A method for manufacturing a Zener diode comprising:
implanting an N-type Buried Layer (NBL) in a first epitaxial layer;
implanting a P-type Buried Layer (PBL) having a peak PBL doping concentration below the NBL;
laterally diffusing the PBL;
growing a second epitaxial layer over the NBL;
implanting a P-type region (Plink) for coupling the PBL to an Anode electrode; and
implanting an N-type region (Nlink) for coupling the NBL to a Cathode electrode.

### Claim 2 (depends on 1)

The method of claim 1 wherein implanting the NBL comprises implanting with at least one of Antimony and Arsenic, to form a Zener junction between the NBL and the PBL.

### Claim 3 (depends on 2)

The method of claim 2 further comprising implanting the NBL with Phosphorous to connect the Nlink to the NBL through diffusion of the Phosphorous towards to Nlink.

### Claim 4 (depends on 2)

The method of claim 2 wherein implanting the Nlink comprises implanting with a Phosphorous implant.

### Claim 5 (depends on 1)

The method of claim 1 wherein implanting the PBL comprises implanting with a Boron implant.

### Claim 6 (depends on 1)

The method of claim 1 further comprising connecting the Plink to the PBL through the second epitaxial layer, wherein the second epitaxial layer comprises a P-type dopant having a lower first dopant concentration than a second dopant concentration of the Plink.

### Claim 7 (depends on 1)

The method of claim 1 wherein the Plink is physically connected to the PBL.

### Claim 8 (depends on 1)

The method of claim 1 further comprising laterally separating the Cathode electrode from the Anode electrode with a Salicide block layer deposited over the second epitaxial layer.

### Claim 9 (depends on 1)

The method of claim 1 further comprising forming the first epitaxial layer over a Bulk Oxide formed over a Silicon layer.

### Claim 10

A Zener diode comprising:
an N-type Buried Layer (NBL) in a first epitaxial layer;
a P-type Buried Layer (PBL) having a peak PBL doping concentration below the NBL;
a second epitaxial layer over the NBL;
a P-type region (Plink) coupled to the PBL and to an Anode electrode; and
an N-type region (Nlink) coupled to the NBL and to a Cathode electrode.

### Claim 11 (depends on 10)

The apparatus of claim 10 wherein the NBL comprises at least one of Antimony and Arsenic to form a Zener junction between the NBL and the PBL.

### Claim 12 (depends on 10)

The apparatus of claim 10 wherein the NBL comprises Phosphorous to connect the NBL to the Nlink through diffusion of the Phosphorous towards the Nlink.

### Claim 13 (depends on 10)

The apparatus of claim 10 wherein the Nlink physically contacts the NBL.

### Claim 14 (depends on 10)

The apparatus of claim 10 wherein the PBL comprises Boron.

### Claim 15 (depends on 10)

The apparatus of claim 10 wherein the Plink couples to the PBL through the second epitaxial layer, wherein the second epitaxial layer comprises a P-type dopant having a lower first dopant concentration than a second dopant concentration of the Plink.

### Claim 16 (depends on 10)

The apparatus of claim 10 wherein an opening in the NBL is formed to couple the Plink to the PBL.

### Claim 17

A method for manufacturing a Zener diode comprising:
implanting an N-type Buried Layer (NBL) with an N-type dopant in a first epitaxial layer, wherein the NBL comprises an NBL opening excluding the N-type dopant;
implanting a P-type Buried Layer (PBL) having a peak PBL doping concentration below the NBL;
growing a second epitaxial layer over the NBL;
implanting a P-type region (Plink) to couple to the PBL above the NBL opening, and to couple the Plink to an Anode electrode; and
implanting an N-type region (Nlink) to couple the NBL to a Cathode electrode.

### Claim 18 (depends on 17)

The method of claim 17 wherein implanting the NBL comprises implanting with at least one of Antimony and Arsenic, to form a Zener junction between the NBL and the PBL.

### Claim 19 (depends on 18)

The method of claim 18 further comprising implanting the NBL with Phosphorous to connect the Nlink to the NBL through diffusion of the Phosphorous towards to Nlink.

### Claim 20 (depends on 17)

The method of claim 17 further comprising thermally annealing the Zener diode to laterally diffuse the PBL.