# US 2022/0285528 A1 · Formation of transistor gates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285528 A1
- Document ID: US20220285528A1
- Status: Published application
- Kind: A1
- Application number: 17/340,037
- Filed: 2021-06-06
- Published: 2022-09-08
- Earliest claimed: 2021-03-05
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Yen-Jui CHIU; Yao-Teng CHUANG; Kuei-Lun LIN
- Web page: https://patentgrep.com/patent/US20220285528A1

## CPC

- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 30/019: {of FETs having stacked nanowire, nanosheet or nanoribbon channels}
- H10D 30/501: {FETs having stacked nanowire, nanosheet or nanoribbon channels}
- H10D 62/121: {oriented parallel to substrates}
- H10D 64/01: Manufacture or treatment
- H10D 86/0221: {comprising manufacture, treatment or patterning of TFT semiconductor bodies}
- H10D 86/0231: {using masks, e.g. half-tone masks}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- H10D 30/6735: {having gates fully surrounding the channels, e.g. gate-all-around}
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A method comprises forming first and second fins each comprising alternately stacking first and second semiconductor layers; forming dummy gate structures over the first and second fins, and gate spacers on either side of the dummy gate structures; removing the dummy gate structures to form first and second gate trenches; removing the first semiconductor layers such that the second semiconductor layers are suspended in the first and second gate trenches; depositing a first dielectric layer around the second semiconductor layers and a second dielectric layer around the first dielectric layer; performing an ALD process to form a hard mask layer around the second dielectric layer, the ALD process comprising pulsing a first precursor for a first pulse time longer than about one second; patterning the hard mask layer; and etching a portion of the second gate dielectric layer in the second gate trench.

## Claims

### Claim 1

A method comprising,
forming a first fin and a second fin over a substrate, the first and second fins each comprising alternately stacking first semiconductor layers and second semiconductor layers;
forming dummy gate structures over the first and second fins, and gate spacers on either side of the dummy gate structures;
removing the dummy gate structures to form a first gate trench over the first fin and a second gate trench over the second fin;
removing the first semiconductor layers such that the second semiconductor layers are suspended in the first and second gate trenches;
depositing a first gate dielectric layer around each of the second semiconductor layers and a second gate dielectric layer around the first gate dielectric layer;
performing an atomic layer deposition (ALD) process to form a hard mask layer around the second gate dielectric layer, the ALD process comprising pulsing a first precursor into a deposition chamber for a first pulse time longer than about one second;
patterning the hard mask layer; and
with the patterned hard mask layer in place, etching a portion of the second gate dielectric layer in the second gate trench.

### Claim 2 (depends on 1)

The method of claim 1, wherein the ALD process further comprises after pulsing the first precursor into the deposition chamber, pulsing a second precursor into the deposition chamber for a second pulse time longer than about one second.

### Claim 3 (depends on 2)

The method of claim 2, wherein the first pulse time is substantially the same as the second pulse time.

### Claim 4 (depends on 2)

The method of claim 2, wherein the first precursor is oxygen-containing, and the second precursor is metal-containing.

### Claim 5 (depends on 2)

The method of claim 2, wherein the first precursor is oxygen-containing, and the second precursor is aluminum-containing.

### Claim 6 (depends on 2)

The method of claim 2, wherein the ALD process further comprises after pulsing the first precursor into the deposition chamber and before pulsing the second precursor into the deposition chamber, purging the deposition chamber for a purge time, and the purge time is at least about fifteen times the first pulse time.

### Claim 7 (depends on 2)

The method of claim 2, wherein the ALD process further comprises after pulsing the second precursor into the deposition chamber, purging the deposition chamber for a purge time, and the purge time is at least about ten times the second pulse time.

### Claim 8 (depends on 1)

The method of claim 1, wherein the second gate dielectric layer and the hard mask layer are metal oxide layers having different metal compositions.

### Claim 9 (depends on 1)

The method of claim 1, wherein the second gate dielectric layer comprises lanthanum oxide, and the hard mask layer comprises aluminum oxide.

### Claim 10 (depends on 9)

The method of claim 9, wherein the first gate dielectric layer comprises hafnium oxide.

### Claim 11 (depends on 1)

The method of claim 1, further comprising:
after etching the portion of the second gate dielectric layer in the second gate trench, removing the patterned hard mask layer; and
after removing the patterned hard mask layer, depositing one or more metal materials in the first and second gate trenches.

### Claim 12

A method comprising:
forming first and second fins over a substrate, the first and second fins each comprising alternately stacking first semiconductor layers and second semiconductor layers;
forming first and second dummy gate structures across the first and second fins;
forming first gate spacers on either side of the first dummy gate structure and second gate spacers on either side of the second dummy gate structure;
removing the first and second dummy gate structures to form a first gate trench between the first gate spacers and a second gate trench between the second gate spacers;
selectively etching the first semiconductor layers in the first and second gate trenches;
depositing a first gate dielectric layer in the first and second gate trenches and a second gate dielectric layer over the first gate dielectric layer;
forming a hard mask layer over the second gate dielectric layer by using one or more atomic layer deposition (ALD) cycles each comprising sequentially performing a first pulse step, a first purge step for a first purge time, a second pulse step, and a second purge step for a second purge time, wherein the first purge time is longer than the second purge time;
patterning the hard mask layer to expose a portion of the second gate dielectric layer; and
etching the exposed portion of the second gate dielectric layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the first pulse step pulses an oxygen-containing precursor for a pulse time shorter than both the first and second purge times.

### Claim 14 (depends on 13)

The method of claim 13, wherein the first purge time is at least about fifteen times the pulse time.

### Claim 15 (depends on 12)

The method of claim 12, wherein the second pulse step pulses an aluminum-containing precursor for a pulse time shorter than both the first and second purge times.

### Claim 16 (depends on 15)

The method of claim 15, wherein the second purge time is at least about ten times the pulse time.

### Claim 17 (depends on 12)

The method of claim 12, wherein the first pulse step continues for a first pulse time, and the second pulse step continues for a second pulse time, and a ratio of the first purge time to the first pulse time is greater than a ratio of the second purge time to the second pulse time.

### Claim 18

A method comprising:
forming a first fin and a second fin, the first and second fins each comprising alternately stacking first semiconductor layers and second semiconductor layers;
forming dummy gate structures across the first and second fins, respectively;
forming gate spacers on either side of the dummy gate structures;
removing the dummy gate structures and the first semiconductor layers to form a plurality of spaces between corresponding ones of the second semiconductor layers;
depositing in sequence a first gate dielectric layer and a second gate dielectric layer into the plurality of spaces between corresponding ones of the second semiconductor layers;
performing an atomic layer deposition (ALD) process to form a hard mask layer on the second gate dielectric layer, the ALD process comprising pulsing a first precursor into a deposition chamber for a first pulse time, and purging the first precursor from the deposition chamber for a first purge time, the first purge time being at least about fifteen times the first pulse time;
patterning the hard mask layer to expose a portion of the second gate dielectric layer; and
etching the exposed portion of the second gate dielectric layer.

### Claim 19 (depends on 18)

The method of claim 18, wherein the first pulse time is greater than about one second.

### Claim 20 (depends on 18)

The method of claim 18, wherein the ALD process further comprises after purging the first precursor from the deposition chamber, pulsing a second precursor into the deposition chamber for a second pulse time, the second pulse time being greater than about one second.