# US 2022/0285312 A1 · Semiconductor package

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285312 A1
- Document ID: US20220285312A1
- Status: Published application
- Kind: A1
- Application number: 17/804,110
- Filed: 2022-05-26
- Published: 2022-09-08
- Earliest claimed: 2020-05-26
- Assignees: Samsung Electronics Co., Ltd.
- Applicants: Samsung Electronics Co., Ltd.
- Inventors: Jihwan HWANG; Unbyoung KANG; Sangsick PARK; Jihwan SUH; Soyoun LEE; Teakhoon LEE
- Web page: https://patentgrep.com/patent/US20220285312A1

## CPC

- H10W 72/073: {of die-attach connectors}
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 90/00: Package configurations
- H10W 90/701: {characterised by the relative positions of pads or connectors relative to package parts}
- H10P 72/7428: {used to support diced chips prior to mounting}
- H10W 70/611: {for connecting multiple chips together}
- H10W 72/01325: {in solid form}
- H10W 72/0198: {batch processes}
- H10W 72/0711: {Apparatus therefor}
- H10W 72/07125: {Means for controlling the bonding environment, e.g. valves or vacuum pumps}
- H10W 72/07141: {Means for applying energy, e.g. ovens or lasers}
- H10W 72/072: {of bump connectors}
- H10W 72/07252: {changes in structures or sizes}
- H10W 72/07254: {changes in dispositions}
- H10W 72/07304: {the auxiliary member being temporary, e.g. a sacrificial coating}
- H10W 72/07331: {Connecting techniques}
- H10W 72/07338: {hardening the adhesive by curing, e.g. thermosetting}
- H10W 72/07341: {Controlling the bonding environment, e.g. atmosphere composition or temperature}
- H10W 72/07353: {changes in shapes}
- H10W 72/07354: {changes in dispositions}
- H10W 72/221: {Structures or relative sizes}
- H10W 72/222: {Multilayered bumps, e.g. a coating on top and side surfaces of a bump core}
- H10W 72/227: {Multiple bumps having different sizes}
- H10W 72/242: {relative to the surface, e.g. recessed, protruding}
- H10W 72/247: {Dispositions of multiple bumps}
- H10W 72/334: {Cross-sectional shape, i.e. in side view}
- H10W 72/347: {Dispositions of multiple die-attach connectors}
- H10W 72/823: {Interconnections through encapsulations, e.g. pillars through molded resin on a lateral side a chip}
- H10W 72/877: {Bump connectors and die-attach connectors}
- H10W 74/142: {the encapsulations exposing the passive side of the semiconductor body}
- H10W 74/15: on active surfaces of flip-chip devices, e.g. underfills
- H10W 90/20: Configurations of stacked chips
- H10W 90/22: the stacked chips being on both top and bottom sides of a package substrate, interposer or RDL
- H10W 90/26: the stacked chips being of the same size without any chips being laterally offset, e.g. chip stacks having a rectangular shape
- H10W 90/28: the stacked chips having different sizes, e.g. chip stacks having a pyramidal shape
- H10W 90/291: {characterised by containers, encapsulations, or other housings for the stacked chips}
- H10W 90/297: {characterised by the through-semiconductor vias [TSVs] in the stacked chips}
- H10W 90/401: {characterised by multiple insulating or insulated package substrates, interposers or RDLs}
- H10W 90/722: {between stacked chips}
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/732: {between stacked chips}
- H10W 90/734: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor package includes a base chip and at least one semiconductor chip disposed on the base chip. An adhesive film is disposed between the base chip and the at least one semiconductor chip and is configured to fix the at least one semiconductor chip on the base chip. The adhesive film includes an inner film portion that overlaps the at least one semiconductor chip in a thickness direction of the base chip, and an outer film portion that does not overlap the at least one semiconductor chip in the thickness direction of the base chip. A width of the outer film portion in a direction perpendicular to a lateral edge of the at least one semiconductor chip is substantially uniform within a deviation range of 20% of an average width of the outer film portion.

## Claims

### Claim 1

A method of manufacturing a semiconductor package comprising:
arranging a wafer on an electrostatic chuck, the wafer including a plurality of base chips;
pre-bonding at least one semiconductor chip on the wafer using an adhesive film;
performing a foil lamination process to cover the at least one semiconductor chip on the wafer with a foil;
performing a pressurized reflow process, wherein the pressurized reflow process is a process of reflowing the adhesive film by applying heat while maintaining a constant pressure in a process chamber; and
removing the foil.

### Claim 2 (depends on 1)

The method of claim 1,
wherein after the pressurized reflow process, the adhesive film includes an inner film portion that overlaps the at least one semiconductor chip in a thickness direction of the base chip, and an outer film portion that does not overlap the at least one semiconductor chip in the thickness direction of the base chip, and
wherein a width of the outer film portion in a direction perpendicular to a lateral edge of the at least one semiconductor chip is substantially uniform within a deviation range of 20% of an average width of the outer film portion.

### Claim 3 (depends on 2)

The method of claim 2,
wherein at least one semiconductor chip has a rectangular shape, and
the following Equation (1) is satisfied,
Ws−Wc≤Ws*0.2 <Equation (1)>
wherein Ws is a width of the outer film portion adjacent to the lateral edge of the at least one semiconductor chip, Wc is a width of the outer film portion adjacent to a vertex of the at least one semiconductor chip, and
Ws and Wc are greater than 0.

### Claim 4 (depends on 1)

The method of claim 1,
wherein at least one semiconductor chip is aligned with a corresponding base chip.

### Claim 5 (depends on 1)

The method of claim 1,
wherein at least one semiconductor chip is plural, and the foil has substantially the same size as the wafer.

### Claim 6 (depends on 1)

The method of claim 1,
wherein the foil comprises a polyimide (PI) film, and the removing the foil comprises removing the foil by UV irradiation.

### Claim 7 (depends on 1)

The method of claim 1,
wherein pressure applied in the pressurized reflow process is constant regardless of a direction as a hydrostatic pressure.

### Claim 8 (depends on 1)

The method of claim 1,
wherein the pressurized reflow process comprises a pre-heating section, a dwelling section, and a cooling section, the dwelling section is a peak temperature section, and wetting of a solder is performed during the dwelling section.

### Claim 9 (depends on 1)

The method of claim 1, further comprising:
sealing at least one semiconductor chip on the wafer; and
completing the semiconductor package by a singulating process.

### Claim 10 (depends on 1)

The method of claim 1, further comprising:
before the performing a foil lamination process, pre-bonding an upper semiconductor chip on at least one semiconductor chip on the wafer.

### Claim 11 (depends on 1)

The method of claim 1,
wherein the base chip includes an interface chip; and at least one semiconductor chip includes a memory chip.

### Claim 12

A method of manufacturing a semiconductor package comprising:
arranging a wafer on an electrostatic chuck, the wafer including a plurality of base chips;
pre-bonding at least one chip stack on the wafer using an adhesive film;
performing a foil lamination process to cover the at least one chip stack on the wafer with a foil;
performing a pressurized reflow process, wherein the pressurized reflow process is a process of reflowing the adhesive film by applying heat while maintaining a constant pressure in a process chamber;
removing the foil;
sealing the at least one chip stack on the wafer; and
completing the semiconductor package by a singulating process.

### Claim 13 (depends on 12)

The method of claim 12,
wherein at least one chip stack includes at least two semiconductor chips sequentially stacked.

### Claim 14 (depends on 13)

The method of claim 13,
wherein the pre-bonding at least one chip stack on the wafer comprises:
pre-bonding a semiconductor chip located at the bottom of at least one chip stack on the wafer; and
pre-bonding an upper semiconductor chip on a lower semiconductor chip.

### Claim 15 (depends on 13)

The method of claim 13,
wherein the pre-bonding at least one chip stack on the wafer comprises:
forming at least one chip stack; and
pre-bonding at least one chip stack on the wafer.

### Claim 16 (depends on 12)

The method of claim 12,
wherein after the pressurized reflow process, the adhesive film includes an inner film portion that overlaps at least one chip stack in a thickness direction of the base chip, and an outer film portion that does not overlap at least one chip stack in the thickness direction of the base chip, and
wherein a width of the outer film portion in a direction perpendicular to a lateral edge of at least one chip stack is substantially uniform within a deviation range of 20% of an average width of the outer film portion.

### Claim 17 (depends on 16)

The method of claim 16,
wherein at least one chip stack has a rectangular shape, and
the following Equation (1) is satisfied,
Ws−Wc≤Ws*0.2 <Equation (1)>
wherein Ws is a width of the outer film portion adjacent to the lateral edge of the at least one chip stack, Wc is a width of the outer film portion adjacent to a vertex of at least one chip stack, and
Ws and Wc are greater than 0.

### Claim 18

A method of manufacturing a semiconductor package comprising:
arranging a wafer on an electrostatic chuck, the wafer including a plurality of base chips;
pre-bonding at least one semiconductor chip on the wafer using an adhesive film;
performing a foil lamination process to cover at least one semiconductor chip on the wafer with a foil;
performing a pressurized reflow process, wherein the pressurized reflow process is a process of reflowing the adhesive film by applying heat while maintaining a constant pressure in a process chamber;
removing the foil;
sealing at least one semiconductor chip on the wafer; and
completing the semiconductor package by a singulating process,
wherein after the pressurized reflow process, the adhesive film includes an inner film portion that overlaps at least one semiconductor chip in a thickness direction of the base chip, and an outer film portion that does not overlap at least one semiconductor chip in the thickness direction of the base chip, and
wherein a width of the outer film portion in as direction perpendicular to as lateral edge of at least one semiconductor chip is substantially uniform within a deviation range of 20% of an average width of the outer film portion.

### Claim 19 (depends on 18)

The method of claim 18,
wherein at least one semiconductor chip is aligned with a corresponding base chip, and
the removing the foil comprises removing the foil by UV irradiation.

### Claim 20 (depends on 18)

The method of claim 18,
wherein the pressurized reflow process comprises a pre-heating section, a dwelling section, and a cooling section, the dwelling section is a peak temperature section, and wetting of a solder is performed during the dwelling section.