# US 2022/0285238 A1 · Bonded substrate and bonded substrate manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285238 A1
- Document ID: US20220285238A1
- Status: Published application
- Kind: A1
- Application number: 17/752,937
- Filed: 2022-05-25
- Published: 2022-09-08
- Earliest claimed: 2019-12-03
- Assignees: NGK Insulators, Ltd.
- Applicants: Ngk Insulators, Ltd.
- Inventors: Takashi EBIGASE; Izumi MASUDA; Takeshi KAKU
- Web page: https://patentgrep.com/patent/US20220285238A1

## CPC

- C04B 37/026: {consisting of metals or metal salts}
- H10W 70/692: Ceramics or glasses
- B23K 1/00: Soldering, e.g. brazing, or unsoldering (B23K3/00 takes precedence)
- C04B 35/584: based on silicon nitride
- C04B 35/645: Pressure sintering
- H05K 1/0306: {Inorganic insulating substrates, e.g. ceramic, glass}
- H10W 40/255: {having a laminate or multilayered structure, e.g. direct bond copper [DBC] ceramic substrates}
- H10W 70/02: of conductive package substrates serving as an interconnection, e.g. of metal plates (manufacture or treatment of leadframes H10W70/04)
- C04B 2235/85: Intergranular or grain boundary phases
- C04B 2237/125: based on noble metals, e.g. silver
- C04B 2237/127: The active component for bonding being a refractory metal
- C04B 2237/368: Silicon nitride
- C04B 2237/407: Copper
- C04B 2237/59: Aspects relating to the structure of the interlayer
- C04B 2237/61: Joining two substrates of which at least one is porous by infiltrating the porous substrate with a liquid, such as a molten metal, causing bonding of the two substrates, e.g. joining two porous carbon substrates by infiltrating with molten silicon
- C04B 2237/708: of one or more of the interlayers
- H05K 3/022: {Processes for manufacturing precursors of printed circuits, i.e. copper-clad substrates}
- H05K 3/38: Improvement of the adhesion between the insulating substrate and the metal
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

The bonded substrate includes the silicon nitride ceramic substrate, a copper plate, the bonding layer, and penetrating regions. The copper plate and the bonding layer are patterned into a predetermined shape, and are disposed over a main surface of the silicon nitride ceramic substrate. The bonding layer bonds the copper plate to the main surface of the silicon nitride ceramic substrate. The penetrating regions each include one or more penetrating portions penetrating continuously from the main surface of the substrate into the silicon nitride ceramic substrate to a depth of 3 μm or more and 20 μm or less, and contain silver, and the number of penetrating regions present per square millimeter of the main surface of the substrate is one or more and 30 or less.

## Claims

### Claim 1

A bonded substrate comprising:
a silicon nitride ceramic substrate;
a copper plate disposed over a main surface of the silicon nitride ceramic substrate, and patterned into a predetermined shape;
a bonding layer disposed on the main surface according to the shape into which the copper plate is patterned, and bonding the copper plate to the main surface; and
a plurality of penetrating regions each including one or more penetrating portions penetrating continuously from the main surface into the silicon nitride ceramic substrate to a depth of 3 μm or more and 20 μm or less, wherein
the penetrating regions contain silver, and the number of penetrating regions present per square millimeter of the main surface is one or more and 30 or less.

### Claim 2 (depends on 1)

The bonded substrate according to claim 1, wherein
in a portion in which the main surface is not exposed, the one or more penetrating portions penetrate continuously from the bonding layer.

### Claim 3 (depends on 1)

The bonded substrate according to claim 1, wherein
the bonding layer contains at least one type of active metal selected from the group consisting of titanium and zirconium, and
the penetrating portions further contain at least one type of metal selected from the group consisting of copper, indium, and tin.

### Claim 4 (depends on 1)

The bonded substrate according to claim 1, wherein
a projected area of the penetrating regions in the silicon nitride ceramic substrate imaginarily projected onto the main surface is greater than an area of the penetrating regions actually present at the main surface.

### Claim 5 (depends on 1)

The bonded substrate according to claim 1, wherein
spacing between laminates of patterned portions of the copper plate and patterned portions of the bonding layer is 0.5 mm to 1.5 mm.

### Claim 6

A bonded substrate manufacturing method comprising:
a) preparing a silicon nitride ceramic substrate;
b) forming a brazing material layer on a main surface of the silicon nitride ceramic substrate;
c) disposing a copper plate on the brazing material layer to obtain an intermediate product including the silicon nitride ceramic substrate, the brazing material layer, and the copper plate;
d) heat treating the intermediate product to generate a bonding layer bonding the copper plate to the main surface, and a plurality of penetrating regions each including one or more penetrating portions penetrating continuously from the bonding layer into the silicon nitride ceramic substrate to a depth of 3 μm or more and 20 μm or less from the main surface and containing silver; and
e) patterning the copper plate and the bonding layer into a predetermined shape, wherein
in step d), the penetrating regions are formed so that the number of penetrating regions present per square millimeter of the main surface is one or more and 30 or less.

### Claim 7 (depends on 6)

The bonded substrate manufacturing method according to claim 6, wherein
the heat treatment is performed by heating the intermediate product in accordance with a temperature profile having a maximum temperature of 800° C. or more and 860° C. or less.

### Claim 8 (depends on 6)

The bonded substrate manufacturing method according to claim 6, wherein
the brazing material layer contains a hydride of at least one type of active metal selected from the group consisting of titanium and zirconium, silver, and at least one type of metal selected from the group consisting of copper, indium, and tin, and
in step d), the penetrating regions are formed by moving metal including at least silver to a void of the silicon nitride ceramic substrate through the heat treatment.

### Claim 9 (depends on 6)

The bonded substrate manufacturing method according to claim 6, wherein
the heat treatment is performed by pressurizing the intermediate product in accordance with a contact pressure profile having a maximum contact pressure of 5 MPa or more and 30 MPa or less.

### Claim 10 (depends on 2)

The bonded substrate according to claim 2, wherein
the bonding layer contains at least one type of active metal selected from the group consisting of titanium and zirconium, and
the penetrating portions further contain at least one type of metal selected from the group consisting of copper, indium, and tin.

### Claim 11 (depends on 2)

The bonded substrate according to claim 2, wherein
a projected area of the penetrating regions in the silicon nitride ceramic substrate imaginarily projected onto the main surface is greater than an area of the penetrating regions actually present at the main surface.

### Claim 12 (depends on 3)

The bonded substrate according to claim 3, wherein
a projected area of the penetrating regions in the silicon nitride ceramic substrate imaginarily projected onto the main surface is greater than an area of the penetrating regions actually present at the main surface.

### Claim 13 (depends on 10)

The bonded substrate according to claim 10, wherein
a projected area of the penetrating regions in the silicon nitride ceramic substrate imaginarily projected onto the main surface is greater than an area of the penetrating regions actually present at the main surface.

### Claim 14 (depends on 2)

The bonded substrate according to claim 2, wherein
spacing between laminates of patterned portions of the copper plate and patterned portions of the bonding layer is 0.5 mm to 1.5 mm.

### Claim 15 (depends on 3)

The bonded substrate according to claim 3, wherein
spacing between laminates of patterned portions of the copper plate and patterned portions of the bonding layer is 0.5 mm to 1.5 mm.

### Claim 16 (depends on 4)

The bonded substrate according to claim 4, wherein
spacing between laminates of patterned portions of the copper plate and patterned portions of the bonding layer is 0.5 mm to 1.5 mm.

### Claim 17 (depends on 7)

The bonded substrate manufacturing method according to claim 7, wherein
the brazing material layer contains a hydride of at least one type of active metal selected from the group consisting of titanium and zirconium, silver, and at least one type of metal selected from the group consisting of copper, indium, and tin, and
in step d), the penetrating regions are formed by moving metal including at least silver to a void of the silicon nitride ceramic substrate through the heat treatment.

### Claim 18 (depends on 7)

The bonded substrate manufacturing method according to claim 7, wherein
the heat treatment is performed by pressurizing the intermediate product in accordance with a contact pressure profile having a maximum contact pressure of 5 MPa or more and 30 MPa or less.

### Claim 19 (depends on 8)

The bonded substrate manufacturing method according to claim 8, wherein
the heat treatment is performed by pressurizing the intermediate product in accordance with a contact pressure profile having a maximum contact pressure of 5 MPa or more and 30 MPa or less.

### Claim 20 (depends on 17)

The bonded substrate manufacturing method according to claim 17, wherein
the heat treatment is performed by pressurizing the intermediate product in accordance with a contact pressure profile having a maximum contact pressure of 5 MPa or more and 30 MPa or less.