# US 2022/0285237 A1 · Bonded substrate, and bonded substrate manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285237 A1
- Document ID: US20220285237A1
- Status: Published application
- Kind: A1
- Application number: 17/752,935
- Filed: 2022-05-25
- Published: 2022-09-08
- Earliest claimed: 2019-12-03
- Assignees: NGK Insulators, Ltd.
- Applicants: Ngk Insulators, Ltd.
- Inventors: Takashi EBIGASE
- Web page: https://patentgrep.com/patent/US20220285237A1

## CPC

- H10W 70/692: Ceramics or glasses
- C04B 35/584: based on silicon nitride
- C04B 37/026: {consisting of metals or metal salts}
- H05K 1/0306: {Inorganic insulating substrates, e.g. ceramic, glass}
- H10W 40/255: {having a laminate or multilayered structure, e.g. direct bond copper [DBC] ceramic substrates}
- H10W 70/02: of conductive package substrates serving as an interconnection, e.g. of metal plates (manufacture or treatment of leadframes H10W70/04)
- C04B 2237/125: based on noble metals, e.g. silver
- C04B 2237/127: The active component for bonding being a refractory metal
- C04B 2237/368: Silicon nitride
- C04B 2237/407: Copper
- H05K 3/022: {Processes for manufacturing precursors of printed circuits, i.e. copper-clad substrates}
- H05K 3/38: Improvement of the adhesion between the insulating substrate and the metal
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

A bonded substrate includes a ceramic substrate, a copper plate, and a bonding layer. The ceramic substrate has a main surface having a flat region having a maximum height Rz of 10 μm or less. The ceramic substrate has a particle-defect hole being exposed to the main surface, imparting flatness lower than flatness of the flat region to a part of the main surface, and having a depth of 10 μm or more and 60 μm or less. The copper plate includes a first portion disposed over the flat region and a second portion filling the particle-defect hole. The bonding layer includes a third portion covering the flat region and a fourth portion filling the particle-defect hole, and the second portion and the fourth portion fill 80% or more of a volume of the particle-defect hole. The bonding layer bonds the copper plate to the main surface.

## Claims

### Claim 1

A bonded substrate comprising:
a ceramic substrate having a main surface and a particle-defect hole, the main surface having a flat region having a maximum height Rz of 10 μm or less, the particle-defect hole being exposed to the main surface, imparting flatness lower than flatness of the flat region to a part of the main surface, and having a depth of 10 μm or more and 60 μm or less;
a copper plate including a first portion disposed over the flat region and a second portion filling the particle-defect hole; and
a bonding layer including a third portion covering the flat region and a fourth portion filling the particle-defect hole, and bonding the copper plate to the main surface, wherein
the second portion and the fourth portion fill 80% or more of a volume of the particle-defect hole.

### Claim 2 (depends on 1)

The bonded substrate according to claim 1, wherein
the particle-defect hole has a depth of 30 μm or less.

### Claim 3 (depends on 1)

The bonded substrate according to claim 1, wherein
the particle-defect hole has an inner surface, and
the fourth portion covers the inner surface.

### Claim 4 (depends on 3)

The bonded substrate according to claim 3, wherein
the fourth portion covers 80% or more of an area of the inner surface.

### Claim 5 (depends on 1)

The bonded substrate according to claim 1, wherein
the ceramic substrate comprises a silicon nitride ceramic substrate.

### Claim 6

A bonded substrate manufacturing method comprising:
a) preparing a ceramic substrate having a main surface and a particle-defect hole, the main surface having a flat region having a maximum height Rz of 10 μm or less, the particle-defect hole being exposed to the main surface, imparting flatness lower than flatness of the flat region to a part of the main surface, and having a depth of 10 μm or more and 60 μm or less;
b) forming a brazing material layer on the main surface;
c) disposing a copper plate on the brazing material layer to obtain an intermediate product including the ceramic substrate, the brazing material layer, and the copper plate; and
d) hot pressing the intermediate product to cause a portion of the copper plate to enter the particle-defect hole so that the copper plate is deformed to include a first portion disposed over the flat region and a second portion filling the particle-defect hole, and to cause a portion of the brazing material layer to enter the particle-defect hole so that the brazing material layer is changed into a bonding layer including a third portion covering the flat region and a fourth portion filling the particle-defect hole, and bonding the copper plate to the main surface, wherein
in step d), the second portion and the fourth portion fill 80% or more of a volume of the particle-defect hole.

### Claim 7 (depends on 6)

The bonded substrate manufacturing method according to claim 6, wherein
the hot pressing comprises heating the intermediate product in accordance with a temperature profile having a maximum temperature of 800° C. or more and 900° C. or less while pressurizing the intermediate product along a thickness direction of the ceramic substrate in accordance with a contact pressure profile having a maximum contact pressure of 5 MPa or more and 30 MPa or less.

### Claim 8 (depends on 2)

The bonded substrate according to claim 2, wherein
the particle-defect hole has an inner surface, and
the fourth portion covers the inner surface.

### Claim 9 (depends on 8)

The bonded substrate according to claim 8, wherein
the fourth portion covers 80% or more of an area of the inner surface.

### Claim 10 (depends on 2)

The bonded substrate according to claim 2, wherein
the ceramic substrate comprises a silicon nitride ceramic substrate.

### Claim 11 (depends on 3)

The bonded substrate according to claim 3, wherein
the ceramic substrate comprises a silicon nitride ceramic substrate.

### Claim 12 (depends on 4)

The bonded substrate according to claim 4, wherein
the ceramic substrate comprises a silicon nitride ceramic substrate.

### Claim 13 (depends on 8)

The bonded substrate according to claim 8, wherein
the ceramic substrate comprises a silicon nitride ceramic substrate.

### Claim 14 (depends on 9)

The bonded substrate according to claim 9, wherein
the ceramic substrate comprises a silicon nitride ceramic substrate.