# US 2022/0285164 A1 · Plasma Etching Apparatus Component for Manufacturing Semiconductor Comprising Composite Sintered Body and Manufacturing Method Therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285164 A1
- Document ID: US20220285164A1
- Status: Published application
- Kind: A1
- Application number: 17/628,515
- Filed: 2020-07-13
- Published: 2022-09-08
- Earliest claimed: 2019-07-22
- Applicants: Korea Institute of Materials Science
- Inventors: Young Jo PARK; Ha Neul KIM; Jae Woong KO; Mi Ju KIM; Hyeon Myeong OH
- Web page: https://patentgrep.com/patent/US20220285164A1

## CPC

- H10P 50/242: {of Group IV materials}
- B22F 3/10: Sintering only
- C04B 35/053: Fine ceramics
- C04B 35/505: based on yttrium oxide
- H01J 37/32: Gas-filled discharge tubes (heating by discharge H05B)
- H01J 37/32009: {Arrangements for generation of plasma specially adapted for examination or treatment of objects, e.g. plasma sources (plasma generation in general H05H1/24)}
- H10P 72/00: Handling or holding of wafers, substrates or devices during manufacture or treatment thereof
- C04B 35/645: Pressure sintering
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/661: Multi-step sintering
- C04B 2235/77: Density
- C04B 2235/785: Submicron sized grains, i.e. from 0,1 to 1 micron
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- C04B 2235/963: Surface properties, e.g. surface roughness
- C04B 2235/9669: Resistance against chemicals, e.g. against molten glass or molten salts
- H01J 2237/334: Etching
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Provided is a plasma etching apparatus component for manufacturing a semiconductor characterized by including a composite sintered body which contains 30 vol % to 70 vol % of yttria (Y2O3) and 30 vol % to 70 vol % of magnesia (MgO) and having plasma resistance. The plasma etching apparatus component for manufacturing a semiconductor provided in one aspect of the present invention has excellent corrosion resistance to plasma, and may have good corrosion resistance to plasma even when the composite sintered body is sintered at a relatively low relative density. In addition, the composite sintered body has a small crystal grain size and a small increase in surface roughness after etching, so that there is an effect that contaminant particles may be reduced. Furthermore, the plasma etching apparatus component for manufacturing a semiconductor has excellent strength compared to a typical plasma-resistant material, is inexpensive, and is excellent in terms of economic feasibility and utilization.

## Claims

### Claim 1

A plasma etching apparatus component for manufacturing a semiconductor, the component comprising:
a composite sintered body including 30 vol % to 70 vol % of yttria (Y2O3); and
30 vol % to 70 vol % of magnesia (MgO), and the component having plasma resistance.

### Claim 2 (depends on 1)

The plasma etching apparatus component for manufacturing a semiconductor of claim 1, wherein the composite sintered body has a crystal grain size of 100 nm to 1 μm.

### Claim 3 (depends on 1)

The plasma etching apparatus component for manufacturing a semiconductor of claim 1, wherein the composite sintered body has a crystal grain size of 100 nm to 500 nm.

### Claim 4 (depends on 1)

The plasma etching apparatus component for manufacturing a semiconductor of claim 1, wherein the composite sintered body has a relative density of 90% or higher.

### Claim 5 (depends on 1)

The plasma etching apparatus component for manufacturing a semiconductor of claim 1, wherein when the composite sintered body is exposed to CF4/02 plasma of 500 W output and 100 W bias for 3 hours, the surface roughness (Ra) of the composite sintered body increases by 5 times or less.

### Claim 6 (depends on 1)

The plasma etching apparatus component for manufacturing a semiconductor of claim 1, wherein the composite sintered body has a surface roughness (Ra) of 2 nm or less.

### Claim 7 (depends on 1)

The plasma etching apparatus component for manufacturing a semiconductor of claim 1, wherein when the composite sintered body is exposed to CF4/02 plasma of 500 W output and 100 W bias for 3 hours, the etching depth of the composite sintered body is 200 nm or less.

### Claim 8 (depends on 1)

The plasma etching apparatus component for manufacturing a semiconductor of claim 1, wherein the composite sintered body has a biaxial strength of 200 MPa or greater.

### Claim 9 (depends on 1)

The plasma etching apparatus component for manufacturing a semiconductor of claim 1, wherein the plasma etching apparatus component for manufacturing a semiconductor is formed of a bulk material of the composite sintered body.

### Claim 10 (depends on 1)

The plasma etching apparatus component for manufacturing a semiconductor of claim 1, wherein the plasma etching apparatus component for manufacturing a semiconductor is formed by coating the composite sintered body on another material.

### Claim 11

A method for manufacturing a plasma etching apparatus component for manufacturing a semiconductor, the method comprising:
mixing 30 vol % to 70 vol % of yttria (Y2O3) and 30 vol % to 70 vol % of magnesia (MgO); and
sintering the mixed yttria (Y2O3) and magnesia (MgO).

### Claim 12 (depends on 11)

The method of claim 11, wherein the sintering of the mixed yttria (Y2O3) and magnesia (MgO) is performed at 1000° C. to 1500° C.

### Claim 13 (depends on 1)

A plasma etching apparatus for manufacturing a semiconductor including the plasma etching apparatus component of claim 1.