# US 2022/0285161 A1 · Methods for Doping High-K Metal Gates for Tuning Threshold Voltages

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285161 A1
- Document ID: US20220285161A1
- Status: Published application
- Kind: A1
- Application number: 17/664,325
- Filed: 2022-05-20
- Published: 2022-09-08
- Earliest claimed: 2019-09-17
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd
- Inventors: Kuo-Feng Yu; Chun Hsiung Tsai; Jian-Hao Chen; Hoong Shing Wong; Chih-Yu Hsu
- Web page: https://patentgrep.com/patent/US20220285161A1

## CPC

- H10D 64/01338: {with a treatment, e.g. annealing, after the formation of the conductor}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 64/0134: {with a treatment, e.g. annealing, after the formation of the insulator and before the formation of the conductor}
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 84/0144: {Manufacturing their gate insulating layers}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/0193: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/853: {comprising FinFETs}
- H10P 50/73: {using masks for insulating materials}
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- H10P 76/4085: {characterised by the processes involved to create the masks}
- H10D 84/0177: {the gate conductors having different materials or different implants}
- H10D 84/0181: {Manufacturing their gate insulating layers}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method includes forming a first gate dielectric and a second gate dielectric over a first semiconductor region and a second semiconductor region, respectively, depositing a lanthanum-containing layer including a first portion and a second portion overlapping the first gate dielectric and the second gate dielectric, respectively, and depositing a hard mask including a first portion and a second portion overlapping the first portion and the second portion of the lanthanum-containing layer, respectively. The hard mask is free from both of titanium and tantalum. The method further includes forming a patterned etching mask to cover the first portion of the hard mask, with the second portion of the hard mask being exposed, removing the second portion of the hard mask and the second portion of the lanthanum-containing layer, and performing an anneal to drive lanthanum in the first portion of the lanthanum-containing layer into the first gate dielectric.

## Claims

### Claim 1

A method comprising:
depositing a doping-metal-containing layer comprising a first portion over a first gate dielectric;
depositing a hard mask comprising a first portion over and contacting the first portion of the doping-metal-containing layer, wherein an entirety of the hard mask is formed of a homogenous material;
forming an etching mask comprising a first portion over and contacting the first portion of the hard mask;
performing an anneal process to drive a dopant in the doping-metal-containing layer into the first gate dielectric; and
removing the doping-metal-containing layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the forming the etching mask comprises dispensing a photoresist over and contacting the hard mask, with the photoresist and the hard mask being in contact with each other, and wherein a contact angle between the photoresist and the hard mask is smaller than about 10 degrees.

### Claim 3 (depends on 1)

The method of claim 1 further comprising removing the etching mask before the anneal process.

### Claim 4 (depends on 3)

The method of claim 3 further comprising removing the hard mask before the anneal process.

### Claim 5 (depends on 1)

The method of claim 1, wherein the hard mask is removed after the anneal process.

### Claim 6 (depends on 1)

The method of claim 1, wherein the doping-metal-containing layer further comprises a second portion over a second gate dielectric, and the hard mask further comprises a second portion over the second portion of the doping-metal-containing layer, and wherein the method further comprises:
before the anneal process, removing the second portion of the hard mask; and
before the anneal process, removing the second portion of the doping-metal-containing layer.

### Claim 7 (depends on 6)

The method of claim 6, wherein the second portion of the hard mask is removed in an etching process, with the first portion of the etching mask being used to protect the first portion of the hard mask.

### Claim 8 (depends on 1)

The method of claim 1, wherein the depositing the hard mask comprises depositing an aluminum oxide layer.

### Claim 9

A method comprising:
removing a dummy gate stack to form a trench between gate spacers;
forming a high-k dielectric layer extending into the trench;
depositing a lanthanum oxide layer over the high-k dielectric layer;
depositing a hard mask over the lanthanum oxide layer, wherein the hard mask is a single-layer hard mask;
forming a patterned photoresist over and contacting the hard mask;
patterning the hard mask and the lanthanum oxide layer;
removing both of the patterned photoresist and the hard mask;
removing the lanthanum oxide layer; and
forming a gate electrode over and contacting the high-k dielectric layer.

### Claim 10 (depends on 9)

The method of claim 9, wherein both of the hard mask and the lanthanum oxide layer are patterned using the patterned photoresist as an etching mask.

### Claim 11 (depends on 9)

The method of claim 9, wherein the lanthanum oxide layer is removed in an etching process using a chemical solution comprising hydrochloride, and wherein the chemical solution is free from hydrogen peroxide therein.

### Claim 12 (depends on 9)

The method of claim 9 further comprising forming an n-type source/drain region on a side of the gate electrode, wherein the n-type source/drain region and the gate electrode are portions of a same transistor.

### Claim 13 (depends on 9)

The method of claim 9 further comprising forming a p-type source/drain region on a side of the gate electrode, wherein the p-type source/drain region and the gate electrode are portions of a same transistor.

### Claim 14 (depends on 9)

The method of claim 9 further comprising, after the removing the hard mask and before the removing the lanthanum oxide layer, performing an anneal process to drive lanthanum into the high-k dielectric layer.

### Claim 15 (depends on 14)

The method of claim 14, wherein the anneal process comprises a spike anneal process performed at a temperature in a range between about 570° C. and about 750° C.

### Claim 16 (depends on 9)

The method of claim 9, wherein the removing the lanthanum oxide layer is performed using a chemical solution comprising ammonia and hydrogen chloride dissolved therein, and wherein the chemical solution is free from hydrogen peroxide therein.

### Claim 17

A method comprising:
forming a high-k dielectric layer over a semiconductor region;
depositing a lanthanum oxide layer over the high-k dielectric layer;
depositing a hard mask over the lanthanum oxide layer, wherein an entirety of the hard mask is formed of a homogeneous material selected from the group consisting of aluminum nitride, zirconium oxide, and aluminum oxide;
forming a patterned etching mask over the hard mask, wherein the hard mask is in physical contact with both of the lanthanum oxide layer and the patterned etching mask;
etching the hard mask using the patterned etching mask to define patterns for the hard mask;
performing an anneal process on the lanthanum oxide layer;
removing the lanthanum oxide layer; and
forming a gate electrode over and contacting the high-k dielectric layer.

### Claim 18 (depends on 17)

The method of claim 17, wherein the anneal process is performed with the hard mask being on the lanthanum oxide layer.

### Claim 19 (depends on 17)

The method of claim 17, wherein the annealing process is performed after the hard mask is removed.

### Claim 20 (depends on 17)

The method of claim 17, wherein the removing the lanthanum oxide layer is also performed using the patterned etching mask.