# US 2022/0285156 A1 · Apparatus and method for wafer bonding

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0285156 A1
- Document ID: US20220285156A1
- Status: Published application
- Kind: A1
- Application number: 17/826,097
- Filed: 2022-05-26
- Published: 2022-09-08
- Earliest claimed: 2016-01-15
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company Ltd.
- Inventors: YEONG-JYH LIN; YEUR-LUEN TU; CHIN-WEI LIANG
- Web page: https://patentgrep.com/patent/US20220285156A1

## CPC

- H10P 10/128: {by direct semiconductor to semiconductor bonding}
- H10P 70/12: {by dry cleaning only (H10P70/52 takes precedence)}
- H10P 70/27: {during, before or after processing of conductive materials, e.g. polysilicon or amorphous silicon layers}
- H10P 72/0464: {characterised by the construction of the transfer chamber}
- H10W 80/00: Direct bonding of chips, wafers or substrates
- H10W 90/00: Package configurations
- H10P 72/0428: {Apparatus for mechanical treatment or grinding or cutting}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

An apparatus for wafer bonding includes a transfer module and a plasma module. The transfer module is configured to transfer a semiconductor wafer. The plasma module is configured to apply a first type of plasma to perform a reduction operation upon a surface of the semiconductor wafer at a temperature within a predetermined temperature range to convert metal oxides on the surface of the semiconductor wafer to metal, and apply a second type of plasma to perform a plasma operation upon the surface of the semiconductor wafer at a room temperature outside the predetermined temperature range to activate a surface of the semiconductor wafer.

## Claims

### Claim 1

A plasma module, comprising:
a first chamber, configured to accommodate a semiconductor wafer; and
a heating stage, located in the first chamber, the heating stage configured to selectively control a temperature, at which an operation is performed in the first chamber, to fall within a predetermined temperature range, each value in the predetermined temperature range being greater than a value of a room temperature, a surface of the semiconductor wafer being activated at the room temperature,
wherein when a first type of plasma is applied to the first chamber to perform a reduction operation upon the surface of the semiconductor wafer to convert metal oxides on the surface of the semiconductor wafer to metal, the heating stage located in the first chamber is configured to control a temperature at which the reduction operation is performed to fall within the predetermined temperature range; when a second type of plasma comprising Cl2 plasma is applied to the first chamber to clean a sidewall of the first chamber, the heating stage is configured to control a temperature, at which the second type of plasma is applied to the first chamber for cleaning the sidewall, to fall within the predetermined temperature range and reach the temperature at which the reduction operation is performed; the second type of plasma is different from the first type of plasma.

### Claim 2 (depends on 1)

The plasma module of claim 1, wherein the predetermined temperature range is from approximately 100 Celsius (° C.) to approximately 400° C.

### Claim 3 (depends on 1)

The plasma module of claim 1, wherein the plasma module is configured to perform the reduction operation under a pressure in a range from approximately 0.1 Torr to approximately 50 Torr.

### Claim 4 (depends on 1)

The plasma module of claim 1, wherein the first type of plasma is H2 or NH3 plasma.

### Claim 5 (depends on 1)

The plasma module of claim 1, further comprising:
a power source, located in the first chamber, the power source being configured to ionize a first type of gas to generate the first type of plasma.

### Claim 6 (depends on 5)

The plasma module of claim 5, further comprising:
a gas input, arranged to receive the first type of gas, wherein the first type of gas is applied to the first chamber through the gas input at a flow rate in a range from 100 sccm to 2500 sccm.

### Claim 7 (depends on 1)

The plasma module of claim 1, further comprising:
a power source, configured to ionize a first type of gas to generate the first type of plasma; and
a second chamber, wherein the power source is located in the second chamber, and the generated first type of plasma is transferred from the second chamber to the first chamber and applied to the semiconductor wafer.

### Claim 8 (depends on 7)

The plasma module of claim 7, further comprising:
a gas input, arranged to receive the first type of gas, wherein the first type of gas is applied to the second chamber through the gas input at a flow rate in a range from 100 sccm to 2500 sccm.

### Claim 9

A plasma module, comprising:
a first chamber for accommodating a semiconductor wafer; and
a heater, located in the first chamber, the heater configured to selectively control a temperature, at which an operation is performed upon the semiconductor wafer, to fall within a predetermined temperature range,
wherein each value in the predetermined temperature range is greater than a value of a room temperature, and a surface of the semiconductor wafer is activated at the room temperature; when a first type of plasma comprising NH3 plasma is applied to the first chamber to perform the operation to convert metal oxides on the surface of the semiconductor wafer to metal, the heater located in the first chamber is configured to control the temperature to rise above a room temperature and fall within the predetermined temperature range.

### Claim 10 (depends on 9)

The plasma module of claim 9, wherein the predetermined temperature range is from approximately 100 Celsius (° C.) to approximately 400° C.

### Claim 11 (depends on 9)

The plasma module of claim 9, wherein the plasma module is configured to perform the operation to convert the metal oxides on the surface to the metal under a pressure in a range from approximately 0.1 Torr to approximately 50 Torr.

### Claim 12 (depends on 9)

The plasma module of claim 9, wherein when a second type of plasma different from the first type of plasma is applied to the first chamber, the plasma module is configured to perform the operation to activate dielectric material on the surface of the semiconductor wafer.

### Claim 13 (depends on 12)

The plasma module of claim 12, wherein the second type of plasma comprises at least one of N2 plasma, N2H2 plasma and Ar plasma.

### Claim 14 (depends on 9)

The plasma module of claim 9, further comprising:
a power source, located in the first chamber, the power source being configured to ionize a first type of gas to generate the first type of plasma.

### Claim 15 (depends on 14)

The plasma module of claim 14, further comprising:
a gas input, arranged to receive the first type of gas, wherein the first type of gas is applied to the first chamber through the gas input at a flow rate in a range from 100 sccm to 2500 sccm.

### Claim 16 (depends on 9)

The plasma module of claim 9, further comprising:
a power source, configured to ionize a first type of gas to generate the first type of plasma; and
a second chamber, wherein the power source is located in the second chamber, and the generated first type of plasma is transferred from the second chamber to the first chamber and applied to the semiconductor wafer.

### Claim 17 (depends on 16)

The plasma module of claim 16, further comprising:
a gas input, arranged to receive the first type of gas, wherein the first type of gas is applied to the second chamber through the gas input at a flow rate in a range from 100 sccm to 2500 sccm.

### Claim 18

A method for wafer bonding, comprising:
applying a first type of plasma to perform a reduction operation upon conductive pads on a surface of a semiconductor wafer to convert metal oxides on the conductive pads to metal;
utilizing a heater located within a chamber accommodating the semiconductor wafer to control a temperature, at which the metal oxides on the conductive pads are converted to the metal to fall within a predetermined temperature range, wherein each value in the predetermined temperature range is greater than a value of a room temperature;
applying a second type of plasma to comprising Cl2 plasma to clean a sidewall of the chamber;
utilizing the heater to control a temperature, at which the second type of plasma is applied for cleaning the sidewall, to fall within the predetermined temperature range and reach the temperature at which the metal oxides are converted to the metal; and
applying a third type of plasma to activate dielectric material on the surface of the semiconductor wafer at the room temperature.

### Claim 19 (depends on 18)

The method of claim 18, wherein the first type of plasma comprises at least one of H2 plasma and NH3 plasma.

### Claim 20 (depends on 18)

The method of claim 18, wherein the third type of plasma comprises at least one of N2 plasma, N2H2 plasma and Ar plasma.