# US 2022/0283089 A1 · Methods for imaging transparent two-dimensional sheets by fluorescence quenching microscopy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0283089 A1
- Document ID: US20220283089A1
- Status: Published application
- Kind: A1
- Application number: 17/630,417
- Filed: 2020-09-18
- Published: 2022-09-08
- Earliest claimed: 2019-09-19
- Assignees: Northwestern University
- Applicants: Northwestern University
- Inventors: Jiaxing Huang; SonBinh T. Nguyen; Zhizhi Kong
- Web page: https://patentgrep.com/patent/US20220283089A1

## CPC

- G01N 21/6458: {Fluorescence microscopy (fluorescence microscopes per se G02B21/0076 and G02B21/16)}
- G01N 21/17: Systems in which incident light is modified in accordance with the properties of the material investigated (where the material investigated is optically excited causing a change in wavelength of the incident light G01N21/63)
- G01N 21/6428: {Measuring fluorescence of fluorescent products of reactions or of fluorochrome labelled reactive substances, e.g. measuring quenching effects, using measuring "optrodes" (in vivo A61B5/00; immunoassay G01N33/53)}
- G01N 21/8422: {Investigating thin films, e.g. matrix isolation method}
- G01N 2021/6432: {Quenching}
- G01N 2021/8427: {Coatings}
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

Methods of imaging a 2D sheet are provided. In embodiments, such a method comprises illuminating a sample with light having a wavelength 1, the sample comprising a quenching substrate; a transparent, non-quenching 2D sheet on the quenching substrate; and a fluorescent layer comprising fluorescent dye molecules on the transparent, non-quenching 2D sheet and the quenching substrate, providing background domains and 2D sheet domains in the sample, wherein the light induces fluorescence of the dye molecules in the fluorescent layer. The method further comprises detecting fluorescence from the sample to provide an image of the transparent, non-quenching 2D sheet, wherein an intensity IB of the detected fluorescence from the background domains is less than an intensity I2DSs of the detected fluorescence from the 2D sheet domains, thereby providing contrast in the image.

## Claims

### Claim 1

A method of imaging a 2D sheet, the method comprising:
(a) illuminating a sample with light having a wavelength X, the sample comprising
a quenching substrate;
a transparent, non-quenching 2D sheet on the quenching substrate; and
a fluorescent layer comprising fluorescent dye molecules on the transparent, non-quenching 2D sheet and the quenching substrate, providing background domains and 2D sheet domains in the sample, wherein the light induces fluorescence of the dye molecules in the fluorescent layer; and
(b) detecting fluorescence from the sample to provide an image of the transparent, non-quenching 2D sheet, wherein an intensity IB of the detected fluorescence from the background domains is less than an intensity I2DS of the detected fluorescence from the 2D sheet domains, thereby providing contrast in the image.

### Claim 2 (depends on 1)

The method of claim 1, wherein the contrast is (I2DS−IB)/I2DS and is greater than 50%.

### Claim 3 (depends on 1)

The method of claim 1, wherein a mixture of the transparent, non-quenching 2D sheet and a reference dye molecule has a peak fluorescence intensity within 10% that of the fluorescent dye molecule alone.

### Claim 4 (depends on 3)

The method of claim 3, wherein the reference dye molecule is fluorescein.

### Claim 5 (depends on 3)

The method of claim 3, wherein the reference dye molecule is one of the fluorescent dye molecules.

### Claim 6 (depends on 1)

The method of claim 1, wherein the transparent, non-quenching 2D sheet is selected from the group consisting of boron nitride, a clay, a metal oxide, and combinations thereof.

### Claim 7 (depends on 6)

The method of claim 6, wherein the clay is hectorite and the metal oxide is TiO2.

### Claim 8 (depends on 1)

The method of claim 1, wherein the transparent, non-quenching 2D sheets comprise at least two different types of transparent, non-quenching 2D sheets.

### Claim 9 (depends on 1)

The method of claim 1, the sample further comprising a transparent, quenching 2D sheet on the quenching substrate.

### Claim 10 (depends on 9)

The method of claim 9, wherein the transparent, quenching 2D sheet is selected from the group consisting of a graphene-based sheet, a metal dichalcogenide sheet, and combinations thereof.

### Claim 11 (depends on 1)

The method of claim 1, wherein a layer of a reference dye molecule on the quenching substrate has a peak photoluminescence intensity of no more than 50% that of the layer on uncoated glass.

### Claim 12 (depends on 11)

The method of claim 11, wherein the reference dye molecule is fluorescein.

### Claim 13 (depends on 11)

The method of claim 11, wherein the reference dye molecule is one of the fluorescent dye molecules.

### Claim 14 (depends on 1)

The method of claim 1, wherein the quenching substrate is selected from doped silicon, a metal, metal-coated glass, or indium tin oxide (ITO)-coated glass.

### Claim 15 (depends on 1)

The method of claim 1, wherein the fluorescent layer further comprises a polymer.

### Claim 16 (depends on 1)

The method of claim 1, wherein the fluorescent layer has a thickness in a range of from 5 nm to 20 nm.

### Claim 17 (depends on 1)

The method of claim 1, wherein the transparent, non-quenching 2D sheet is in a stack comprising a transparent 2D sheet having a different quenching ability as compared to the transparent, non-quenching 2D sheet, the method further comprising determining a stacking order of the transparent, non-quenching 2D sheet and the transparent 2D sheet having the different quenching ability.