# US 2022/0282388 A1 · Roughened nickel-plated material and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282388 A1
- Document ID: US20220282388A1
- Status: Published application
- Kind: A1
- Application number: 17/630,274
- Filed: 2020-07-27
- Published: 2022-09-08
- Earliest claimed: 2019-07-26
- Assignees: Toyo Kohan Co., Ltd.
- Applicants: Toyo Kohan Co., Ltd.
- Inventors: Shinichirou HORIE; Etsuro TSUTSUMI; Toshifumi KOYANAGI; Shunki OBATA; Michio KAWAMURA; Koh YOSHIOKA; Naoharu HARADA; Tsuyoshi IRIE; Yonosuke YOSHII
- Web page: https://patentgrep.com/patent/US20220282388A1

## CPC

- C25D 3/12: of nickel or cobalt
- B21B 1/22: for rolling {plates, strips,} bands or sheets of indefinite length (B21B1/42 takes precedence)
- C25D 5/14: two or more layers being of nickel or chromium, e.g. duplex or triplex layers
- C25D 5/48: After-treatment of electroplated surfaces
- C25D 5/605: {Surface topography of the layers, e.g. rough, dendritic or nodular layers}
- C23G 1/00: Cleaning or pickling metallic material with solutions or molten salts (with organic solvents C23G5/02)
- C23G 1/081: {solutions containing H2SO4}
- C25D 5/36: of iron or steel
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- C23G: CLEANING OR DE-GREASING OF METALLIC MATERIAL BY CHEMICAL METHODS OTHER THAN ELECTROLYSIS

## Abstract

[Object] To provide a roughened nickel-plated material in which the formation unevenness such as generation of the unevenness or grooves in a roughened nickel plated layer is restrained. [Solving Means] A roughened nickel-plated material including a base material that is a rolled material, and a roughened nickel plated layer formed on at least one surface of the base material, in which SRzjis of the surface of the roughened nickel plated layer is equal to or more than 2 μm, and, letting a maximum height of the roughened nickel plated layer be SRz, a valley region B in a given virtual planer region A as observed at a height position of SRz×0.25 satisfies the following (i). (i) The length of the valley region B in the rolling direction RD of the base material is less than 40 μm in a direct distance.

## Claims

### Claim 1

A roughened nickel-plated material comprising:
a base material that is a metal; and
a roughened nickel plated layer formed on at least one surface of the base material,
wherein SRzjis of the surface of the roughened nickel plated layer is equal to or more than 2 μm, and,
letting a maximum height of the roughened nickel plated layer be SRz, a valley region B in a given virtual planer region A as observed at a height position of SRz×0.25 satisfies the following (i):
(i) a length of the valley region B in a rolling direction or a plate passing direction of the base material is less than 40 μm in a direct distance.

### Claim 2 (depends on 1)

The roughened nickel-plated material according to claim 1, wherein a maximum CLmax of a circumferential length CL of the valley region B is less than 500 μm.

### Claim 3

A roughened nickel-plated material comprising:
a base material that is a metal; and
a roughened nickel plated layer formed on at least one surface of the base material,
wherein Str of three-dimensional surface property parameters of the surface of the roughened nickel plated layer is equal to or more than 0.1.

### Claim 4 (depends on 3)

The roughened nickel-plated material according to claim 3, wherein, further, Sk of the three-dimensional surface property parameters of the surface of the roughened nickel plated layer is 1.0 to 4.0 μm.

### Claim 5 (depends on 3)

The roughened nickel-plated material according to claim 3, wherein, further, Vvc of the three-dimensional surface property parameters of the surface of the roughened nickel plated layer is 0.6 to 3.0 μm3/μm2.

### Claim 6 (depends on 3)

The roughened nickel-plated material according to claim 3, wherein, further, Vmc of the three-dimensional surface property parameters of the surface of the roughened nickel plated layer is 0.45 to 2.0 μm3/μm2.

### Claim 7 (depends on 1)

The roughened nickel-plated material according to claim 1, wherein the base material is a steel sheet.

### Claim 8 (depends on 1)

The roughened nickel-plated material according to claim 1, wherein brightness of color of the surface of the roughened nickel plated layer is 30 to 50 in L* value.

### Claim 9 (depends on 1)

The roughened nickel-plated material according to claim 1, wherein glossiness of the surface of the roughened nickel plated layer is 1.5 to 50 in 85° glossiness.

### Claim 10 (depends on 1)

The roughened nickel-plated material according to claim 1, further comprising:
an underlying nickel layer between the base material and the roughened nickel plated layer.

### Claim 11

A method for manufacturing a roughened nickel-plated material, the method comprising:
a base material surface treatment step of making SRzjis of a surface of a base material equal to or more than 0.5 μm and less than 1.7 μm; and
a roughened nickel plating step of forming a roughened nickel plated layer on the base material.

### Claim 12

A method for manufacturing a roughened nickel-plated material, the method comprising:
a step of providing an underlying nickel plated layer having Sku of a surface thereof equal to or more than 4.0 on a base material that is a metal; and
a roughened nickel plating step of forming a roughened nickel plated layer on the underlying nickel plated layer.

### Claim 13 (depends on 12)

The method for manufacturing a roughened nickel-plated material according to claim 12, wherein, further, Vvc of a surface of the underlying nickel plated layer is equal to or less than 0.45 μm3/μm2.

### Claim 14 (depends on 11)

The method for manufacturing a roughened nickel-plated material according to claim 11, wherein the base material surface treatment step is a cold rolling step or a temper rolling step.

### Claim 15 (depends on 14)

The method for manufacturing a roughened nickel-plated material according to claim 14, wherein surface roughness of final rolling rolls for rolling with a reduction ratio of equal to or more than 5% in the cold rolling step is 0.01 to 0.5 μm.

### Claim 16 (depends on 14)

The method for manufacturing a roughened nickel-plated material according to claim 14, wherein surface roughness of final rolling rolls for rolling with a reduction ratio of equal to or more than 0.1% and less than 5% in the temper rolling step is 0.01 to 0.5 μm.

### Claim 17 (depends on 11)

The method for manufacturing a roughened nickel-plated material according to claim 11, wherein the base material is a steel sheet.