# US 2022/0282375 A1 · Depositing Coatings On and Within A Housing, Apparatus, or Tool Using a Coating System Positioned Therein

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282375 A1
- Document ID: US20220282375A1
- Status: Published application
- Kind: A1
- Application number: 17/751,085
- Filed: 2022-05-23
- Published: 2022-09-08
- Earliest claimed: 2019-03-15
- Assignees: Halliburton Energy Services, Inc.
- Applicants: Halliburton Energy Services, Inc.
- Inventors: James M. PRICE
- Web page: https://patentgrep.com/patent/US20220282375A1

## CPC

- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 16/0236: {by etching with a reactive gas}
- C23C 16/042: {using masks}
- C23C 16/45536: {Use of plasma, radiation or electromagnetic fields}
- C23C 16/45544: {characterized by the apparatus}
- C23C 16/45551: {for relative movement of the substrate and the gas injectors or half-reaction reactor compartments}
- C23C 16/45555: {applied in non-semiconductor technology}
- C23C 16/50: using electric discharges {(generation and control of plasma in discharge tubes for surface treatment H01J37/32, H01J37/34)}
- C23C 16/545: {for coating elongated substrates}
- C23C 16/56: After-treatment
- H01J 37/32394: {Treating interior parts of workpieces}
- H01J 37/32357: {Generation remote from the workpiece, e.g. down-stream}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

A method of coating an interior surface of a housing defining a volume includes partitioning the volume into a first zone and a second zone, the first zone isolated from fluid communication with the second zone; introducing one or more reactant gases, plasma, ions, or a combination thereof to the first zone and the second zone; and forming one or more coating layers on all or a portion of the interior surface within the first and second zones via reaction of the reactant gases, the plasma, or the combination thereof. A device for coating an interior surface of a housing is also provided.

## Claims

### Claim 1

A method of coating an interior surface adjacent an interior volume of a housing, wherein the interior volume has an inlet, the method comprising: partitioning the interior volume of the housing into a first zone and a second zone, the first zone isolated from fluid communication with the second zone; introducing one or more reactant gases, plasma, or both to the first zone and the second zone; forming one or more coating layers on all or a portion of the surface adjacent the interior volume of the housing within the first zone and the surface adjacent the interior volume of the housing within the second zone via reaction of the reactant gases, optionally in the presence of the plasma; and optionally, evacuating an unreacted portion of the one or more reactant gases from the first zone, the second zone, or both.

### Claim 2 (depends on 1)

The method of claim 1, wherein the reaction comprises a chemical vapor deposition (CVD) reaction, an atomic layer deposition (ALD) reaction, or both, such that the one or more coating layers respectively comprise an ALD layer, a CVD layer, or both.

### Claim 3 (depends on 2)

The method of claim 2, further comprising: (i) forming the ALD layer by: introducing a first reactant gas into a reaction zone selected from the first zone and the second zone, such that at least a portion of the first reactant gas chemically bonds with the surface adjacent the interior volume within the reaction zone, to form a reactive layer; removing unreacted first reactant gas and/or gaseous byproducts from the reaction zone; introducing a second reactant gas into the reaction zone, such that at least some of the second reactant gas bonds with the reactive layer to form the ALD layer; and optionally removing unreacted second reactant gas and/or gaseous byproducts from the reaction zone; (ii) forming the CVD layer by: introducing at least a third reactant gas into the a reaction zone selected from the first zone and the second zone, such that the at least the third reactant gas chemically reacts with the surface adjacent the interior volume of the housing within the reaction zone to form the CVD layer; or (iii) both forming an ALD layer via (i) and a CVD layer via (ii), wherein forming both an ALD layer and a CVD layer comprises forming an ALD layer on the surface adjacent the interior volume of the housing within the reaction zone and subsequently forming the CVD layer on the ALD layer or forming the CVD layer on the surface adjacent the interior volume of the housing within the reaction zone and subsequently forming the ALD layer on the CVD layer.

### Claim 4 (depends on 3)

The method of claim 3, further comprising performing an atomic layer etching (ALE) process to pre-treat the surface adjacent the interior volume of the housing within the reaction zone prior to the forming of the one or more coating layers on the all or the portion of the surface adjacent the interior volume of the housing within the reaction zone and/or to reduce a thickness of at least one of the one or more coating layers.

### Claim 5 (depends on 4)

The method of claim 4, wherein the ALE process comprises: applying an etching gas to the surface in the interior volume of the housing within the reaction zone, such that the surface chemically reacts with and adsorbs the etching gas; purging the etching gas and any gaseous byproducts from the reaction zone; applying low-energy ions to the portions of the surface that chemically reacted with the etching gas to etch away said portions; and optionally purging byproducts.

### Claim 6 (depends on 3)

The method of claim 3, further comprising flowing a topical reagent to at least one of the one or more coating layers, the topical reagent configured to react with the coating layer and thereby adjust a material characteristic of the coating layer.

### Claim 7 (depends on 6)

The method of claim 6, wherein the flowing of the topical reagent to at least one of the one or more coating layers includes flowing the topical reagent to a topmost coating layer on the all or the portion of the surface adjacent the interior volume of the housing within the first zone and/or a topmost coating layer on the all or the portion of the surface adjacent the interior volume of the housing within the second zone, wherein the topmost coating layer is a one of the one or more coating layers farthest from the surface adjacent the interior volume of the housing.

### Claim 8 (depends on 1)

The method of claim 1, further comprising: introducing a first reactant gas and/or plasma into the first zone and a second reactant gas and/or plasma into the second zone, the first reactant gas and/or plasma and the second reactant gas and/or plasma being the same or different; translating and/or rotating the elongated member and/or the housing; and introducing a third reactant gas and/or plasma into the first reaction zone and/or a fourth reactant gas and/or plasma into the second zone to form an initial coating layer on the surface adjacent the interior volume within the first zone and an initial coating on the surface adjacent the interior volume within the second zone, the initial coating layer on the surface adjacent the interior volume of the housing within the first zone being the same or different from the initial coating on the surface adjacent the interior volume of the housing within the second zone; and/or subsequent forming the one or more coating layers on the all or the portion of the surface adjacent the first zone and the second zone, translating and/or rotating the elongated member within the interior volume and/or translating and/or rotating the housing about the elongated member to provide a third zone and optionally a fourth zone, introducing one or more reactant gases, plasma, or both to the third zone and/or the fourth zone, and forming one or more coating layers on all or a portion of the surface adjacent the interior volume of the housing within the third zone and/or the surface adjacent the interior volume of the housing within the fourth zone via reaction of the reactant gases, optionally in the presence of the plasma.

### Claim 9 (depends on 1)

The method of claim 1, wherein the housing comprises a furnace tube, an aircraft component, a component of a water supply/treatment system; a component of a vehicle fuel system; a well tool; a heat exchanger or component thereof; a pump or component thereof; a reactor or component thereof; a distillation column or component thereof; a condenser or component thereof; a reboiler or component thereof; an interior volume of a storage vessel; an interior volume of a transportation vessel; or another housing.

### Claim 10 (depends on 1)

The method of claim 1, wherein the interior volume includes a fluid flow path within the housing.

### Claim 11 (depends on 1)

The method of claim 1, further comprising forming the one or more coating layers at a worksite at which the housing will subsequently be employed.

### Claim 12 (depends on 1)

The method of any of claim 1, wherein the housing comprises the well tool, wherein the well tool is a logging while drilling (LWD) tool, a measurements while drilling (MWD) tool, or a sampling while drilling (SWD) tool, and wherein the interior volume of the well tool comprises a fluid flow path configured for flow of a formation fluid from an exterior of the well tool through an interior of the well tool.

### Claim 13 (depends on 12)

The method of claim 12, further comprising placing the well tool in a wellbore and contacting the formation fluid with the coated surface.

### Claim 14 (depends on 13)

The method of claim 13, wherein the well tool is a formation sampling tool, and wherein contacting the formation fluid with the coated surface further comprises taking a formation fluid sample with the well tool.

### Claim 15 (depends on 14)

The method of claim 14, further comprising retrieving the formation fluid sample from the wellbore, performing a composition analysis of the formation fluid sample, and determining whether or not to recoat the well tool based on the analysis.

### Claim 16

A method of coating an interior surface adjacent an interior volume of a housing, wherein the interior volume has an inlet, the method comprising:
positioning a coating device of and the housing proximate each other,
wherein coating device comprises an elongated member coupled to a fluid delivery system and operable to supply a first reactant gas to a first zone within the interior volume and a second reactant gas to a second zone within the interior volume; and a barrier positioned to physically isolate the first zone from the second zone and prevent intermixing of the first reactant gas with the second reactant gas, wherein the surface coating unit is sized to fit within an inner diameter of the interior volume for moving through the interior volume;
placing the elongated member into the interior volume of the housing via the inlet, whereby the first barrier divides the interior volume into the first zone and the second zone;
introducing one or more reactant gases, plasma, or both to the first zone and the second zone via the elongated member;
forming one or more coating layers on all or a portion of the surface adjacent the interior volume of the housing within the first zone and the second zone via reaction of the one or more reactant gases, optionally in the presence of the plasma; and
optionally, activating a pump to evacuate an unreacted portion of the one or more reactant gases from the first zone, the second zone, or both.

### Claim 17

A method comprising: applying, by a surface coating unit, a surface coating process to an interior region of a well tool by expelling reactant gases into distinct zones inside the well tool while the surface coating unit is positioned inside the well tool; and preventing, by the surface coating unit, the reactant gases from intermixing with one another by physically isolating the distinct zones from one another.

### Claim 18 (depends on 17)

The method of claim 17, further comprising applying an atomic layer deposition (ALD) process along an inner length of the well tool by translating the surface coating unit through an interior region of the well tool while simultaneously expelling the reactant gases.

### Claim 19 (depends on 18)

The method of claim 18, wherein physically isolating the distinct zones from one another includes positioning a physical barrier between the distinct zones or expelling a buffer gas between the distinct zones.

### Claim 20 (depends on 17)

The method of claim 17, further comprising suctioning at least one of the reactant gases from a zone in the well tool while translating the surface coating unit through the well tool using a vacuum pump or applying the surface coating process at various angles to an interior region of the well tool by rotating the surface coating unit about a central axis.