# US 2022/0282366 A1 · High density, modulus, and hardness amorphous carbon films at low pressure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282366 A1
- Document ID: US20220282366A1
- Status: Published application
- Kind: A1
- Application number: 17/753,208
- Filed: 2020-08-28
- Published: 2022-09-08
- Earliest claimed: 2019-08-30
- Assignees: Lam Research Corporation
- Applicants: Lam Research Corporation
- Inventors: Matthew Scott Weimer; Ragesh Puthenkovilakam; Gordon Alex Macdonald; Shaoqing Zhang; Shih-Ked Lee; Jun Xue; Samantha S.H. Tan; Xizhu Zhao; Mary Anne Manumpil; Eric A. Hudson; Chin-Jui Hsu
- Web page: https://patentgrep.com/patent/US20220282366A1

## CPC

- C23C 16/26: Deposition of carbon only
- H01J 37/32165: {Plural frequencies}
- C23C 16/042: {using masks}
- C23C 16/402: {Silicon dioxide}
- C23C 16/46: characterised by the method used for heating the substrate (C23C16/48, C23C16/50 take precedence)
- C23C 16/505: using radio frequency discharges
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6532: {by exposure to a plasma}
- H10P 14/6902: {composed of carbon, e.g. alpha-C, diamond or hydrogen doped carbon}
- H10P 50/285: {of materials not containing Si, e.g. PZT or Al2O3}
- H10P 50/73: {using masks for insulating materials}
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided herein are methods and related apparatus for depositing an ashable hard mask (AHM) on a substrate in a low pressure chamber using a dual frequency radio frequency component. Low pressure plasma enhanced chemical vapor deposition may be used to increase the etch selectivity of the AHM, permitting the use of a thinner AHM for semiconductor processing operations.

## Claims

### Claim 1

A method comprising:
exposing a semiconductor substrate in a chamber to a process gas comprising a hydrocarbon precursor gas and helium gas, substantially without any other inert gas; and
depositing on the substrate an ashable hard mask (AHM) film by a plasma enhanced chemical vapor deposition (PECVD) process, wherein the PECVD process comprises:
maintaining the chamber pressure at less than 500 mTorr;
igniting a plasma generated by a dual radio frequency (RF) plasma source including a high frequency (HF) component and a low frequency (LF) component.

### Claim 2 (depends on 1)

The method of claim 1, wherein the chamber pressure is between about 3 and 30 mTorr.

### Claim 3 (depends on 1)

The method of claim 1, wherein the HF power is at least about 50 W.

### Claim 4 (depends on 1)

The method of claim 1, wherein the HF power is between about 50 W and 2500 W.

### Claim 5 (depends on 1)

The method of claim 1, wherein the HF power has a frequency between about 2 MHz and about 100 MHz.

### Claim 6

(canceled)

### Claim 7 (depends on 1)

The method of claim 1, wherein the LF power has a frequency between about 100 kHz and about 2.4 MHz.

### Claim 8

(canceled)

### Claim 9

(canceled)

### Claim 10 (depends on 1)

The method of claim 1, wherein the LF power is 0 W.

### Claim 11 (depends on 1)

The method of claim 1, wherein the LF power is between 50 and 500 W.

### Claim 12

(canceled)

### Claim 13 (depends on 1)

The method of claim 1, wherein the LF power is between 250 and 500 W.

### Claim 14 (depends on 1)

The method of claim 1, wherein the HF power is between about 50 and 150 W, and the LF power is between about 50 and 500 W.

### Claim 15 (depends on 1)

The method of claim 1, wherein a direct current bias is applied to an electrostatic chuck that the semiconductor substrate rests upon during the PECVD process, and the potential of the DC bias may be between 100V to 10000V.

### Claim 16 (depends on 15)

The method of claim 15, wherein the direct current bias has a duty cycle between about 10% and about 90%, and a repetition rate between about 100 Hz and 10 kHz.

### Claim 17 (depends on 1)

The method of claim 1, wherein a deposition rate of the AHM is at least 350 Å/min.

### Claim 18 (depends on 1)

The method of claim 1, wherein the chamber includes an electrostatic chuck that the semiconductor substrate rests upon during the PECVD process, and the electrostatic chuck temperature is between −20° C. and 175° C.

### Claim 19

(canceled)

### Claim 20 (depends on 1)

The method of claim 1, further comprising annealing the AHM at a temperature of at least 500° C.

### Claim 21 (depends on 1)

The method of claim 1, wherein the hydrocarbon precursor gas comprises compounds having a molecular weight of at most about 50 g/mol.

### Claim 22 (depends on 1)

The method of claim 1, wherein the hydrocarbon precursor gas comprises compounds having a C:H ratio of at least 0.5.

### Claim 23 (depends on 1)

The method of claim 1, wherein the hydrocarbon precursor gas comprises acetylene (C2H2).

### Claim 24 (depends on 1)

The method of claim 1, wherein the modulus of the AHM film is at least about 120 GPa.

### Claim 25 (depends on 1)

The method of claim 1, wherein the hardness of the AHM film is at least about 12 GPa.

### Claim 26 (depends on 1)

The method of claim 1, wherein the sp3 content of the AHM film is at least about 67%.

### Claim 27 (depends on 1)

The method of claim 1, wherein the density of the AHM film is at least about 1.8 g/cm3.

### Claim 28 (depends on 1)

The method of claim 1, wherein the thickness of the AHM film is at least about 0.1 μm.

### Claim 29

(canceled)

### Claim 30

(canceled)

### Claim 31 (depends on 1)

The method of claim 1, further comprising, before depositing the AHM film, depositing on the substrate an interfacial layer by a PECVD process, wherein depositing the interfacial layer comprises:
igniting a plasma generated by the dual RF plasma source, wherein the HF component and the LF are at a lower power than during deposition of the AHM film.

### Claim 32 (depends on 1)

The method of claim 1, further comprising treating the AHM to ash no more than 10 nm of the AHM to remove a crust layer.

### Claim 33 (depends on 1)

The method of claim 1, further comprising treating the AHM to densify a crust layer by bombarding the AHM with a process gas that does not include a hydrocarbon precursor.

### Claim 34 (depends on 1)

The method of claim 1, further comprising removing hydrocarbon precursor from the process chamber prior to lowering the power of the HF component and/or the LF component.

### Claim 35 (depends on 1)

The method of claim 1, further comprising cleaning the chamber using a discard-able wafer as a cover for an electrostatic chuck.

### Claim 36 (depends on 1)

The method of claim 1, further comprising depositing a layer of SiO2 on any plasma facing components within the process chamber.