# US 2022/0282356 A1 · Method and apparatus for preparing aluminum matrix composite with high strength, high toughness, and high neutron absorption

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282356 A1
- Document ID: US20220282356A1
- Status: Published application
- Kind: A1
- Application number: 17/630,169
- Filed: 2020-10-22
- Published: 2022-09-08
- Earliest claimed: 2020-01-19
- Assignees: Jiangsu University
- Applicants: Jiangsu University
- Inventors: Xizhou KAI; Yutao ZHAO; Yanjie PENG; Gang CHEN; Xiaojing XU; Lin WU; Shuoming HUANG; Ruikun CHEN
- Web page: https://patentgrep.com/patent/US20220282356A1

## CPC

- C22C 21/00: Alloys based on aluminium
- C22C 1/1036: {starting from a melt}
- C22C 1/1052: {by mixing and casting metal matrix composites with reaction}
- C22C 32/0057: {based on B4C}
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present invention relates to an aluminum matrix composite (AMC), and particularly to a method and apparatus for preparing an AMC with a high strength, a high toughness, and a high neutron absorption. The present invention combines a high-neutron-absorption and highly stable micro-B4C extrinsic reinforcement with an in-situ nano-reinforcement containing elements B, Cd, and Hf and having high neutron capture ability, achieves efficient absorption of neutrons by using the large cross-sectional area of the micro-reinforcement, achieves effective capture of rays penetrating gaps of the micro-reinforcement by means of the highly dispersed in-situ nano-reinforcement, and significantly improves the toughness of the composite material by means of the high-dispersion toughening effect of the nano-reinforcement, obtaining a particle-reinforced aluminum matrix composite (PAMC) having high toughness and high neutron absorption.

## Claims

### Claim 1

(canceled)

### Claim 2

(canceled)

### Claim 3

A method for preparing an aluminum matrix composite with a high strength, a high toughness, and a high neutron absorption, wherein through a siphon channel in a center of a melt surface generated by a radial magnetic field, a micro-B4C extrinsic ceramic reinforcement and an intermediate alloy or compound with B, Cd, Hf, Ti, and Zr are introduced into a melt, and a high temperature and a high pressure caused by cavitation and acoustic streaming generated through a high-energy ultrasonic field below a liquid surface of the siphon channel help to achieve infiltration and dispersion of the micro-B4C extrinsic ceramic reinforcement and promote generation of an in-situ nano-reinforcement from the intermediate alloy or compound with B, Cd, Hf, Ti, and Zr and uniform dispersion of the in-situ nano-reinforcement, such that the aluminum matrix composite reinforced by a cross-scale hybrid of the micro-B4C extrinsic ceramic reinforcement and the in-situ nano-reinforcement is prepared, wherein a micro-B4C powder of the micro-B4C extrinsic ceramic reinforcement comprises B4C microparticles with a B4C content of 98.8 wt % or more and an average particle size of 10 μm to 300 μm, and a volume fraction of the B4C microparticles in the AMC is 5 vol % to 30 vol %, and wherein the in-situ nano-reinforcement with B, Cd, Hf, Ti, and Zr comprises one or more selected from the group consisting of ZrB2, TiB2, CdB, and HfB2 that are generated by introducing different intermediate alloys or reactants in the melt for an in-situ reaction, the in-situ nano-reinforcement comprises in-situ nano-reinforcement particles with a particle size of 2 nm to 100 nm; and a volume fraction of the in-situ nano-reinforcement particles in the AMC is 0.2 vol % to 25 vol %,
the method specifically comprises the following steps:
step 1: melting a matrix aluminum alloy in a crucible of an integrated composite preparation apparatus at 850° C. to 950° C. to obtain a melt;
step 2: turning on a radial magnetic field device and an ultrasonic device of the integrated composite preparation apparatus, and adding the intermediate alloy or compound with B, Cd, Hf, Ti, and Zr mixed in a predetermined ratio through a feed pipe to conduct a reaction for 20 min to 30 min, to generate the in-situ nano-reinforcement; and
step 3: cooling the melt to 780° C. to 800° C., adding the B4C microparticles through the feed pipe, and applying a strong radial magnetic field and a strong ultrasonic field to promote infiltration and dispersion of the B4C microparticles in the composite melt; and stirring for 10 min to 30 min, cooling to 720° C. to 750° C., followed by casting.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the matrix aluminum alloy is heated by an electromagnetic induction heating device, and the radial magnetic field device and the ultrasonic device are used to promote synthesis of the in-situ nano-reinforcement particles and the infiltration and dispersion of the B4C microparticles.

### Claim 5 (depends on 3)

The method according to claim 3, wherein the siphon channel in the center of the melt surface generated by the radial magnetic field is generated due to flow inside the melt caused by the radial magnetic field; and the radial magnetic field has a power of 80 kW to 160 kW and a current of 10 A to 100 A, and the siphon channel has a depth of 5 cm to 15 cm.

### Claim 6 (depends on 3)

The method according to claim 3, wherein the high-energy ultrasonic field is generated by the ultrasonic device at a bottom of the integrated composite preparation apparatus, with an ultrasonic power of 5 kW to 20 kW; and an amplitude transformer has a length of 10 cm, and there is a distance of 8 cm to 15 cm between a top of the amplitude transformer and a bottom of the siphon channel, and the amplitude transformer is made of a high-temperature and corrosion-resistant niobium alloy.

### Claim 7

(canceled)

### Claim 8

(canceled)

### Claim 9 (depends on 3)

The method according to claim 3, wherein the matrix aluminum alloy in the step 1 is selected from the group consisting of different 2 series, 5 series, 6 series, and 7 series aluminum matrices according to different uses of thermal conduction, electric conduction, high strength, low expansion, and wear resistance; and in the step 2, a feed speed of the feed pipe is controlled at 5 g/min to 50 g/min by a mechanical device.

### Claim 10 (depends on 3)

The method according to claim 3, wherein the melting at 850° C. to 950° C. in the step 1 is adjusted according to a specific reaction system; the in-situ reaction is conducted for 20 min to 30 min to introduce the intermediate alloy or compound for forming the in-situ nano-reinforcement particles into the melt, and the in-situ reaction is accompanied by radial cyclic stirring, such that the in-situ nano-reinforcement is synthesized in-situ in the melt; the intermediate alloy or compound for forming the in-situ nano-reinforcement particles comprises one or more selected from the group consisting of Al—Zr, Al—Ti, Al—B, Al—Cd, Al—Hf, K2ZrF6, K2TiF6, KBF4, Na2B4O7, ZrO2, and B2O3; and the crucible is made of a heat-resistant die steel undergoing a surface passivation treatment.