# US 2022/0282354 A1 · Method of making magnetically soft intermediate product

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282354 A1
- Document ID: US20220282354A1
- Status: Published application
- Kind: A1
- Application number: 17/195,008
- Filed: 2021-03-08
- Published: 2022-09-08
- Earliest claimed: 2021-03-08
- Assignees: Bilstein GmbH & Co. KG
- Inventors: Dieter KRECH; Thomas Kloss
- Web page: https://patentgrep.com/patent/US20220282354A1

## CPC

- C21D 9/52: for wires; for strips {; for rods of unlimited length}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- H01F 1/147: Alloys characterised by their composition {(treatment thereof for enhancing their electromagnetic properties C21D8/12)}
- H01F 1/16: in the form of sheets (H01F1/147 takes precedence)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

A method of making a soft magnetic intermediate product of metal with particularly good magnetization behavior, the method comprising the following method steps: production or provision of a metallic, rollable blank of a metallic product, preliminary rolling of the metallic blank with a defined degree of deformation to an intermediate thickness, the degree of deformation being matched to a critical or postcritical degree of rolling to be observed during subsequent rolling, heat treatment of the prerolled blank, preferably annealing of the prerolled blank, rolling of the blank with a critical or postcritical degree of rolling to a final thickness and subsequent annealing to set a defined grain size and finishing of the intermediate product.

## Claims

### Claim 1

A method of making a soft, metallic, and magnetic intermediate product, the method comprising the steps of:
manufacturing or providing a metallic, rollable blank of a metallic product,
prerolling the metallic blank with a defined degree of deformation to an intermediate thickness, the degree of deformation being matched to a critical or postcritical degree of rolling to be maintained during subsequent rolling,
heat treating the prerolled blank,
rolling the blank with a critical or postcritical degree of rolling to a final thickness and thereafter annealing the blank to set a defined grain size, and
finishing the intermediate product.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the blank is a hot strip made of a ferritic or unalloyed steel.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the blank is prerolled during rough rolling with a degree of deformation of 30-80%.

### Claim 4 (depends on 1)

The method according to claim 1 wherein the annealing of the prerolled blank takes place at a temperature of 550° C.-700° C.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the annealing is carried out for up to 50 hours.

### Claim 6 (depends on 1, 2, 3, 4, 5)

The method according to any one of claims 1 to 5, claim 1, wherein the critical degree of rolling is between 8 and 25%.

### Claim 7 (depends on 1)

The method according to claim 1. wherein the annealing connected to the rolling with the critical degree of rolling takes place at a temperature of up to 710° C.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the annealing connected to the rolling with the critical degree of rolling takes place over a period of up to 80 hours.

### Claim 9 (depends on 1)

The method according to claim 1, further comprising:
an upstream heat treatment is carried out before the prerolling of the blank.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the upstream annealing takes place at a temperature between 650 and 800° C.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the upstream annealing is carried out over a period of up to 60 hours.

### Claim 12 (depends on 1)

The method according to claim 1, further comprising the step of:
finish rolling the blank before completion and after the final heat treatment.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the finish rolling takes place with a degree of deformation between 0.1 and 2%.