# US 2022/0282352 A1 · Thin steel plate having excellent low-temperature toughness and ctod properties, and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282352 A1
- Document ID: US20220282352A1
- Status: Published application
- Kind: A1
- Application number: 17/632,364
- Filed: 2020-08-21
- Published: 2022-09-08
- Earliest claimed: 2019-08-23
- Assignees: Posco
- Applicants: Posco
- Inventors: Woo-Gyeom Kim; Sang-Ho Kim; Ki-Hyun Bang
- Web page: https://patentgrep.com/patent/US20220282352A1

## CPC

- C21D 9/46: for sheet metals
- C21D 1/02: Hardening articles or materials formed by forging or rolling, with no further heating beyond that required for the formation
- C21D 1/19: by interrupted quenching
- C21D 1/60: Aqueous agents
- C21D 1/613: Gases; Liquefied or solidified normally gaseous material
- C21D 1/84: Controlled slow cooling (cooling-beds for metal rolling B21B43/00)
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0263: {following hot rolling}
- C21D 11/005: {for cooling}
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C21D 2211/005: Ferrite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present invention relates to structural steel that can be desirably used in offshore structures and the like, more specifically, to a thin steel plate having excellent low-temperature toughness and CTOD properties, and to a method for manufacturing the same.

## Claims

### Claim 1

A thin steel plate having excellent low-temperature toughness and CTOD properties, the thin steel plate comprising, by weight:
0.05 to 0.1% of carbon (C), 0.05 to 0.3% of silicon (Si), 1.0 to 2.0% of manganese (Mn), 0.005 to 0.04% of aluminum (Sol. Al), 0.005 to 0.03% of niobium (Nb), 0.005 to 0.02% of titanium (Ti), 0.05 to 0.4% of copper (Cu), 0.3 to 1.0% of nickel (Ni), 0.001 to 0.008% of nitrogen (N), 0.01% or less of phosphorus (P), and 0.003% or less of sulfur (S), with a balance of Fe and other unavoidable impurities,
wherein the thin steel plate includes acicular ferrite (water-cooled ferrite) having an area fraction of 30 to 50% and polygonal ferrite (air-cooled ferrite) having an area fraction of 50 to 70% as a microstructure, and
has a thickness of 8 to 30 mm.

### Claim 2 (depends on 1)

The thin steel plate having excellent low-temperature toughness and CTOD properties of claim 1, wherein the acicular ferrite has an average crystal grain size of 20 μm or less and the polygonal ferrite has an average crystal grain size of 20 to 35 μm.

### Claim 3 (depends on 1)

The thin steel plate having excellent low-temperature toughness and CTOD properties of claim 1, wherein the thin steel plate further includes one or more of bainite and cementite in an area fraction of 2% or less.

### Claim 4 (depends on 1)

The thin steel plate having excellent low-temperature toughness and CTOD properties of claim 1, wherein the thin steel plate has a thickness of 8 to 15 mm.

### Claim 5 (depends on 1)

The thin steel plate having excellent low-temperature toughness and CTOD properties of claim 1, wherein the thin steel plate has a yield strength of 460 MPa or more, an elongation of 17% or more, an impact toughness at −40° C. of 50 J or more, and a CTOD value at −20° C. of 0.4 mm or more.

### Claim 6

A manufacturing method of a thin steel plate having excellent low-temperature toughness and CTOD properties, the method comprising:
heating a steel slab including, by weight: 0.05 to 0.1% of carbon (C), 0.05 to 0.3% of silicon (Si), 1.0 to 2.0% of manganese (Mn), 0.005 to 0.04% of aluminum (Sol. Al), 0.005 to 0.03% of niobium (Nb), 0.005 to 0.02% of titanium (Ti), 0.05 to 0.4% of copper (Cu), 0.3 to 1.0% of nickel (Ni), 0.001 to 0.008% of nitrogen (N), 0.01% or less of phosphorus (P), and 0.003% or less of sulfur (S), with a balance of Fe and other unavoidable impurities to 1200° C. or higher;
rough rolling the heated steel slab at 1000° C. or higher;
after the rough rolling, finish-hot-rolling the steel slab at a temperature equivalent to or higher than Ar3 to manufacture a hot-rolled steel plate;
air-cooling the hot-rolled steel plate; and
after the air cooling, cooling the hot-rolled steel plate at a cooling rate of 10 to 30° C./s,
wherein the cooling is water cooling, and starts in a temperature range of 660 to 690° C. and ends in a temperature range of 550 to 590° C., and the thin steel plate has a thickness of 8 to 30 mm.

### Claim 7 (depends on 6)

The manufacturing method of a thin steel plate having excellent low-temperature toughness and CTOD properties of claim 6, wherein the finish hot rolling is performed in a temperature range of 850 to 900° C.

### Claim 8 (depends on 6)

The manufacturing method of a thin steel plate having excellent low-temperature toughness and CTOD properties of claim 6, wherein the rough rolling is performed at a reduction ratio of 15 to 20% in 2 passes at a rear end and the finish hot rolling is performed at a cumulative reduction ratio of 70 to 90%.

### Claim 9 (depends on 6)

The manufacturing method of a thin steel plate having excellent low-temperature toughness and CTOD properties of claim 6, wherein the thin steel plate has a thickness of 8 to 15 mm.