# US 2022/0282351 A1 · Steel sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282351 A1
- Document ID: US20220282351A1
- Status: Published application
- Kind: A1
- Application number: 17/426,592
- Filed: 2020-03-12
- Published: 2022-09-08
- Earliest claimed: 2019-03-29
- Assignees: Nippon Steel Corporation
- Applicants: Nippon Steel Corporation
- Inventors: Kengo TAKEDA; Hiroyuki KAWATA; Takafumi YOKOYAMA; Katsuya NAKANO
- Web page: https://patentgrep.com/patent/US20220282351A1

## CPC

- C21D 9/46: for sheet metals
- C22C 38/04: containing manganese
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0273: {Final recrystallisation annealing}
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/06: containing aluminium
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/52: with cobalt
- C22C 38/54: with boron
- C22C 38/58: with more than 1.5% by weight of manganese
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C21D 1/19: by interrupted quenching
- C21D 1/22: Martempering
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 1/26: Methods of annealing
- C21D 8/00: Modifying the physical properties of ferrous metals or ferrous alloys by deformation combined with, or followed by, heat treatment (hardening articles or materials formed by forging or rolling with no further heating beyond that required for the formation C21D1/02)
- C21D 8/0231: {Warm rolling}
- C21D 8/0247: characterised by the heat treatment
- C21D 8/0263: {following hot rolling}
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C21D 2211/009: Pearlite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided are: a steel sheet having a high strength and excellent hydrogen embrittlement resistance; and a method of producing the same. The steel sheet has prescribed chemical composition and structure, in which a standard deviation σ of Mn concentration satisfies σ≥0.15 Mnave (wherein, Mnave represents an average Mn concentration) and a region with a Mn concentration of higher than (Mnave+1.3σ) has a circle-equivalent diameter of less than 10.0 μm. The method of producing the steel sheet includes: the hot rolling step that includes finish rolling a slab having a prescribed chemical composition under prescribed conditions; the step of coiling the thus obtained hot-rolled steel sheet at a coiling temperature of 450 to 700° C.; and the step of cold rolling the hot-rolled steel sheet and subsequently annealing this steel sheet at 800 to 900° C.

## Claims

### Claim 1

A steel sheet, having a chemical composition comprising, by mass %:
C: 0.15 to 0.40%;
Si: 0.01 to 2.00%;
Mn: 0.10 to 5.00%;
P: 0.0001 to 0.0200%;
S: 0.0001 to 0.0200%;
Al: 0.001 to 1.000%;
N: 0.0001 to 0.0200%;
Co: 0 to 0.50%;
Ni: 0 to 1.00%;
Mo: 0 to 1.00%;
Cr: 0 to 2.000%;
0: 0 to 0.0200%;
Ti: 0 to 0.500%;
B: 0 to 0.0100%;
Nb: 0 to 0.500%;
V: 0 to 0.500%;
Cu: 0 to 0.500%;
W: 0 to 0.100%;
Ta: 0 to 0.100%;
Sn: 0 to 0.050%;
Sb: 0 to 0.050%;
As: 0 to 0.050%;
Mg: 0 to 0.0500%;
Ca: 0 to 0.050%;
Y: 0 to 0.050%;
Zr: 0 to 0.050%;
La: 0 to 0.050%;
Ce: 0 to 0.050%; and
a balance of Fe and impurities,
wherein
the steel sheet comprises, by area ratio:
ferrite: 5.0% or less; and
a total of martensite and tempered martensite: 90.0% or more, wherein when there is a balance structure, the balance structure is composed of at least one of bainite, pearlite, and retained austenite,
a standard deviation σ of Mn concentration satisfies a 0.15 Mnave (wherein, Mnave represents an average Mn concentration), and
a region with a Mn concentration of higher than (Mnave+1.3σ) has a circle-equivalent diameter of less than 10.0 μm.

### Claim 2 (depends on 1)

The steel sheet according to claim 1, comprising one or more of:
Co: 0.01 to 0.50%;
Ni: 0.01 to 1.00%;
Mo: 0.01 to 1.00%;
Cr: 0.001 to 2.000%;
0: 0.0001 to 0.0200%;
Ti: 0.001 to 0.500%;
B: 0.0001 to 0.0100%;
Nb: 0.001 to 0.500%;
V: 0.001 to 0.500%;
Cu: 0.001 to 0.500%;
W: 0.001 to 0.100%;
Ta: 0.001 to 0.100%;
Sn: 0.001 to 0.050%;
Sb: 0.001 to 0.050%;
As: 0.001 to 0.050%;
Mg: 0.0001 to 0.0500%;
Ca: 0.001 to 0.050%;
Y: 0.001 to 0.050%;
Zr: 0.001 to 0.050%;
La: 0.001 to 0.050%; and
Ce: 0.001 to 0.050%.