# US 2022/0282350 A1 · Austenitic steel alloy having an improved corrosion resistance under high-temperature loading and method for producing a tubular body therefrom

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282350 A1
- Document ID: US20220282350A1
- Status: Published application
- Kind: A1
- Application number: 17/637,857
- Filed: 2020-08-26
- Published: 2022-09-08
- Earliest claimed: 2019-08-29
- Assignees: Mannesmann Stainless Tubes GmbH
- Applicants: Mannesmann Stainless Tubes GmbH
- Inventors: Michael Spiegel; Patrik Schraven
- Web page: https://patentgrep.com/patent/US20220282350A1

## CPC

- C21D 9/08: for tubular bodies or pipes
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C22C 38/001: {containing N}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/44: with molybdenum or tungsten
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/52: with cobalt
- C22C 38/58: with more than 1.5% by weight of manganese
- F24S 20/20: Solar heat collectors for receiving concentrated solar energy, e.g. receivers for solar power plants
- F24S 40/40: Preventing corrosion; Protecting against dirt or contamination
- F24S 70/12: made of metallic material
- F28F 21/083: {from stainless steel}
- C21D 2211/001: Austenite
- F24S 70/30: Auxiliary coatings, e.g. anti-reflective coatings
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F24S: SOLAR HEAT COLLECTORS; SOLAR HEAT SYSTEMS (for producing mechanical power from solar energy F03G6/00)
- F28F: DETAILS OF HEAT-EXCHANGE AND HEAT-TRANSFER APPARATUS, OF GENERAL APPLICATION (water and air traps, air venting F16)

## Abstract

An austenitic steel alloy is provided having excellent corrosion resistance under high-temperature loading of more than 600° C. and up to 800° C., with the alloy having the following proposed chemical composition (in wt. %), consisting essentially of: C: 0.01 to 0.10; Si: max. 0.75; Mn: max. 2.00; P: max. 0.03; S: max. 0.03; Cr: 23 to 27; Ni: 17 to 23; Nb: 0.2 to 0.6; N: 0.15 to 0.35; the remainder being Fe and melting-related impurities. In a particular configuration a tubular body is made from this steel alloy, where an absorber pipe of a solar receiver of a solar power installation may be made from the tubular body. Still further, a solar receiver comprising this absorber pipe is provided, as well as a method for producing a tubular body from the steel alloy.

## Claims

### Claim 1

An austenitic steel alloy for operating temperatures of at least 600° C. to 800° C. substantially consisting of the following chemical composition in wt. %:
C: 0.01 to 0.10;
Si: max. 0.75;
Mn: max. 2.00;
P: max. 0.03;
S: max. 0.03;
Cr: 23 to 27;
Ni: 17 to 23;
Nb: 0.2 to 0.6; and
N: 0.15 to 0.35;
with the remainder being iron and melt-induced impurities.

### Claim 2 (depends on 1)

The steel alloy as claimed in claim 1, having in wt. %:
C: 0.04 to 0.10;
Si: min. 0.1;
Mn: min. 0.6;
Cr: 23 to 25;
Ni: min. 20; and
N: 0.20 to 0.30.

### Claim 3 (depends on 2)

The steel alloy as claimed in claim 2, having in wt. %:
0.3<Nb/(C+N)<3.8.

### Claim 4 (depends on 3)

The steel alloy as claimed in claim 3, having in wt. %:
0.4<Nb/(C+N)<2.5.

### Claim 5 (depends on 1)

A tubular body, said tubular body produced from a steel alloy as claimed in claim 1.

### Claim 6 (depends on 5)

The tubular body as claimed in claim 5, wherein the tubular body is a seamless tube.

### Claim 7 (depends on 5)

The tubular body as claimed in claim 5, wherein the steel alloy has in wt. % 0.4<Nb/(C+N)<2.5, and wherein the tubular body is a welded tube.

### Claim 8 (depends on 5)

An absorber tube of a solar receiver of a solar power plant for transporting a liquid heating medium, wherein said absorber tube is produced from a tubular body as claimed in claim 5.

### Claim 9 (depends on 8)

The absorber tube as claimed in claim 8, wherein the absorber tube has an outer surface, and wherein the absorber tube comprises a heat-absorbing coating applied to the outer surface.

### Claim 10 (depends on 9)

The absorber tube as claimed in claim 9, wherein the coating is a lacquer application or a sol-gel coating.

### Claim 11 (depends on 8)

A solar receiver comprising an absorber tube as claimed in claim 8.

### Claim 12 (depends on 1)

A method for producing a tubular body from a steel alloy as claimed in claim 1, said method comprising:
annealing a tubular body at annealing temperatures between 800° C. and 900° C. for an annealing time of 0.1 h to 24 h in an atmosphere containing oxygen and/or nitrogen in such a manner that a cover layer having a thickness of at least 2 μm is produced on the tubular body during the annealing.

### Claim 13 (depends on 12)

The method as claimed in claim 12, wherein the annealing time comprises 2 to 4 h.

### Claim 14 (depends on 12)

The method as claimed in claim 12, wherein the cover layer produced on the tubular body during the annealing has a thickness of at least at least 5 μm and at most 20 μm.

### Claim 15 (depends on 8)

The absorber tube of claim 8, wherein the liquid heating medium comprises a molten salt.

### Claim 16 (depends on 2)

The steel alloy as claimed in claim 2, having in wt. %:
C: 0.05 to 0.08; and
Ni: min. 21.

### Claim 17 (depends on 16)

The steel alloy as claimed in claim 16, having in wt. %:
0.4<Nb/(C+N)<2.5.

### Claim 18 (depends on 1)

The steel alloy as claimed in claim 1, having in wt. %:
0.3<Nb/(C+N)<3.8.

### Claim 19 (depends on 1)

The steel alloy as claimed in claim 1, having in wt. %:
0.4<Nb/(C+N)<2.5.

### Claim 20 (depends on 2)

The steel alloy as claimed in claim 2, having in wt. %:
0.4<Nb/(C+N)<2.5.