# US 2022/0282133 A1 · Method of improving shear stability of highly concentrated aqueous adhesive polymer compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282133 A1
- Document ID: US20220282133A1
- Status: Published application
- Kind: A1
- Application number: 17/631,936
- Filed: 2020-07-28
- Published: 2022-09-08
- Earliest claimed: 2019-08-05
- Assignees: BASF SE
- Applicants: BASF SE
- Inventors: Matthias GERST; Stephan MOEBIUS; Michael GROSS; Dirk WULFF
- Web page: https://patentgrep.com/patent/US20220282133A1

## CPC

- C09J 133/064: {containing anhydride, COOH or COOM groups, with M being metal or onium-cation}
- C09J 133/066: {containing -OH groups}
- C08F 2/22: Emulsion polymerisation
- C08F 220/1804: {C4-(meth)acrylate, e.g. butyl (meth)acrylate, isobutyl (meth)acrylate or tert-butyl (meth)acrylate}
- C08F 220/1808: {C8-(meth)acrylate, e.g. isooctyl (meth)acrylate or 2-ethylhexyl (meth)acrylate}
- C09J 7/243: {Ethylene or propylene polymers}
- C09J 7/245: {Vinyl resins, e.g. polyvinyl chloride [PVC]}
- C09J 7/255: {Polyesters}
- C09J 7/385: {Acrylic polymers}
- C08F 2800/20: as weight or mass percentages
- C08F 2810/50: wherein the polymer is a copolymer and the modification is taking place only on one or more of the monomers present in minority
- C09J 2301/414: presence of a copolymer
- C09J 2423/046: in the substrate
- C09J 2423/048: in the pretreated surface to be joined
- C09J 2423/106: in the substrate
- C09J 2423/108: in the pretreated surface to be joined
- C09J 2427/006: in the substrate
- C09J 2427/008: in the pretreated surface to be joined
- C09J 2433/00: Presence of (meth)acrylic polymer
- C09J 2467/006: in the substrate
- C09J 2467/008: in the pretreated surface to be joined
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Method of improving shear stability of highly concentrated aqueous adhesive polymer compositions comprising a specific adhesive polymer which has been prepared by emulsion polymerization and which is dispersed in the aqueous adhesive composition. Said method comprises treating the aqueous adhesive polymer composition with at least one anion exchange resin.

## Claims

### Claim at position 1

-16. (canceled)

### Claim 17

Method of improving shear stability of highly concentrated aqueous adhesive polymer compositions,
wherein the aqueous adhesive polymer composition comprises more than 50% by weight of at least one adhesive polymer which has been prepared by emulsion polymerization and which is dispersed in the aqueous adhesive composition,
wherein the adhesive polymer has been made by free-radical emulsion polymerization of a monomer mixture comprising
a) at least 60 wt. %, based on the total amount of monomers, of at least one monomer selected from the group consisting of C1 to C20 alkyl acrylates, C1 to C20 alkyl methacrylates, vinyl esters of carboxylic acids containing up to 20 carbons, vinylaromatics having up to 20 carbons, vinyl halides, vinyl ethers of alcohols containing 1 to 10 carbons, ethylenically unsaturated nitriles, aliphatic hydrocarbons having 2 to 8 carbons and one or two double bonds, and mixtures thereof,
b) from 0.1 to 10 wt. %, based on the total amount of monomers, of at least one monomer having at least one acid group;
c) optionally at least one further monomer, different from the monomers a) and b);
said method comprises treating the aqueous adhesive polymer composition with at least one anion exchange resin and not treating the aqueous adhesive polymer composition with a cation exchange resin or with a mixed bed ion exchange resin.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the adhesive polymer is a pressure-sensitive adhesive polymer and has a glass transition temperature of less than 10° C. measured by differential scanning calorimetry according to ASTM D 3418-08 as the midpoint temperature when evaluating the second heating curve at a heating rate of 20° C./min.

### Claim 19 (depends on 17)

The method according to claim 17, wherein the adhesive polymer has a bimodal or a multimodal particle size distribution.

### Claim 20 (depends on 19)

The method according to claim 19, wherein a first particle mode has a weight average particle diameter in the range of 50 to 200 nm, a second particle mode has a weight average particle diameter in the range of 250 to 1200 nm and the weight average particle diameters of the first and second mode differ by at least 50 nm.

### Claim 21 (depends on 17)

The method according to claim 17, wherein the anion exchange resin has a total anion exchange capacity of at least 0.9 eq/L and is used in an amount of more than 1 wt.-%, based on the amount of adhesive polymer.

### Claim 22 (depends on 17)

The method according to claim 17, wherein the anion exchange resin is selected from the group consisting of copolymers of styrene and divinyl benzene with quaternary ammonium functional groups, copolymers of styrene and divinyl benzene with tertiary amine functional groups, crosslinked acrylic polymers with quaternary ammonium functional groups and crosslinked acrylic polymers with tertiary amine functional groups.

### Claim 23 (depends on 17)

The method according to claim 17, wherein the monomers a) are selected from the group consisting of C1 to C10 alkyl acrylates, C1 to C10 alkyl methacrylates, styrene, and mixtures thereof.

### Claim 24 (depends on 17)

The method according to claim 17, wherein the monomers b) having at least one acid group are selected from the group consisting of acrylic acid, methacrylic acid, itaconic acid, maleic acid, fumaric acid, crotonic acid, vinylacetic acid, vinyllactic acid, vinylsulfonic acid, styrenesulfonic acid, acrylamidoglycolic acid, acrylamidomethylpropane sulfonic acid, sulfopropyl acrylate, sulfopropyl methacrylate, anhydrides thereof and mixtures thereof.

### Claim 25 (depends on 17)

The method according to claim 17, wherein the monomers a) are used in an amount of at least 80 wt. %, based on the total amount of the monomers, and are selected from the group consisting of C1 to C10 alkyl acrylates, C1 to C10 alkyl methacrylates, styrene, and a mixture thereof; and the monomers b) are used in an amount of 0.5 to 7 wt. %, based on the total amount of the monomers, and are selected from the group consisting of acrylic acid, methacrylic acid, itaconic acid, and a mixture thereof.

### Claim 26 (depends on 17)

The method according to claim 17, wherein monomer a) comprises no ethyl acrylate or less than 10 wt.-% ethyl acrylate, based on the total amount of the monomers.

### Claim 27 (depends on 17)

The method according to claim 17, wherein the monomers c) are used in an amount of 0.1 to 10 wt. %, based on the total amount of the monomers, and are selected from the group consisting of amides of ethylenically unsaturated carboxylic acids, N-alkylolamides of ethylenically unsaturated carboxylic acids, phenyloxyethyl glycol mono(meth)acrylate, hydroxyalkyl esters of ethylenically unsaturated carboxylic acids, monomers containing amino groups, nitriles of unsaturated C3 to C8 carboxylic acids, bifunctional monomers which as well as an ethylenically unsaturated double bond have at least one glycidyl group, oxazoline group, ureido group, ureido-analogous group or carbonyl group, and crosslinking monomers which have more than one radically polymerizable group.

### Claim 28 (depends on 17)

The method according to claim 17, wherein the aqueous adhesive polymer composition comprises at least one additive selected from the group consisting of crosslinkers, wetting agents, fillers, dyes, flow agents, thickeners, light stabilizers, biocides, defoamers, tackifiers and mixtures thereof.

### Claim 29 (depends on 17)

Aqueous adhesive polymer compositions obtained by a method according to claim 17.

### Claim 30 (depends on 29)

A method comprising utilizing the aqueous adhesive polymer composition according to claim 29 for making self-adhesive articles or for bonding substrates wherein the substrate of the self-adhesive article or at least one of the substrates to be bonded is a transparent substrate.

### Claim 31 (depends on 30)

The method according to claim 30, wherein the transparent substrate comprises is polymer film comprising a film of PVC, polyethylene terephthalate, polyethylene or polypropylene.

### Claim 32 (depends on 30)

A self-adhesive article obtained by the method of claim 30.