# US 2022/0282098 A1 · Method for preparing cationic electrodeposition coating composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282098 A1
- Document ID: US20220282098A1
- Status: Published application
- Kind: A1
- Application number: 17/614,435
- Filed: 2020-05-25
- Published: 2022-09-08
- Earliest claimed: 2019-05-29
- Assignees: Nippon Paint Automotive Coatings Co., Ltd.
- Applicants: Nippon Paint Automotive Coatings Co., Ltd.
- Inventors: Sari NAKASHIMA; Nobuhiro MIYAMAE; Taku KANAZAWA; Hirohisa KANO
- Web page: https://patentgrep.com/patent/US20220282098A1

## CPC

- C09D 5/4438: {Binder based on epoxy/amine adducts, i.e. reaction products of polyepoxides with compounds containing amino groups only}
- C09D 5/4496: {characterised by the nature of the curing agents}
- C08G 18/227: {of antimony, bismuth or arsenic}
- C08G 18/2825: {having at least 6 carbon atoms}
- C08G 18/2855: {Lactams}
- C08G 18/286: {Oximes}
- C08G 18/643: {Reaction products of epoxy resins with at least equivalent amounts of amines}
- C08G 18/73: acyclic
- C08G 18/7671: {containing only one alkylene bisphenyl group}
- C08G 18/8025: {Masked aliphatic or cycloaliphatic polyisocyanates}
- C08G 18/8064: {with monohydroxy compounds}
- C08G 18/8074: {Lactams}
- C08G 18/8077: {Oximes}
- C08K 3/22: of metals
- C08K 5/092: Polycarboxylic acids
- C09D 5/4453: {characterised by the nature of the curing agent}
- C09D 5/4457: {containing special additives, e.g. pigments, polymeric particles}
- C09D 5/4465: {Polyurethanes}
- C09D 7/20: Diluents or solvents
- C09D 7/45: Anti-settling agents
- C09D 7/61: inorganic
- C09D 7/63: organic
- C09D 7/80: Processes for incorporating ingredients
- C09D 17/007: {Metal oxide}
- C09D 175/04: Polyurethanes
- C09D 175/12: from compounds containing nitrogen and active hydrogen, the nitrogen atom not being part of an isocyanate group
- C08K 5/09: Carboxylic acids; Metal salts thereof; Anhydrides thereof
- C08K 2003/221: {of rare earth metal}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

An object of the present invention is to provide a preparation method for improving the edge part rust prevention property in the preparation of a cationic electrodeposition coating composition containing a bismuth compound as a curing catalyst. The present invention provides a method for preparing a cationic electrodeposition coating composition, including a step of preparing a resin emulsion (i) containing an aminated resin (A) and a blocked isocyanate curing agent (B), a step of preparing a pigment dispersion paste (ii) containing a bismuth-metal oxide mixture liquid (C) containing a bismuth compound (c1), a metal oxide (c2), a monohydroxycarboxylic acid (c3) having 3 to 5 carbon atoms in total and a solvent; a pigment dispersion resin (D); a polyvalent acid (E); and a pigment (F), and a step of mixing the resin emulsion (i) and the pigment dispersion paste (ii).

## Claims

### Claim 1

A method for preparing a cationic electrodeposition coating composition,
comprising the following steps:
a step of preparing a resin emulsion (i) comprising an aminated resin (A) and a blocked isocyanate curing agent (B);
a step of preparing a pigment dispersion paste (ii) comprising a bismuth-metal oxide mixture liquid (C) comprising a bismuth compound (c1), a metal oxide (c2), a monohydroxycarboxylic acid (c3) having 3 to 5 carbon atoms in total and a solvent; a pigment dispersion resin (D); a polyvalent acid (E); and a pigment (F); and
a step of mixing the resin emulsion (i) and the pigment dispersion paste (ii) to prepare a cationic electrodeposition coating composition, wherein
the pigment dispersion paste (ii) is prepared by the following steps:
a bismuth-metal oxide mixture liquid (C) preparation step of mixing the bismuth compound (c1), the metal oxide (c2), the monohydroxycarboxylic acid (c3) having 3 to 5 carbon atoms in total and the solvent to prepare the bismuth-metal oxide mixture liquid (C); and
a pigment dispersion paste (ii) preparation step of mixing the obtained bismuth-metal oxide mixture liquid (C) and the polyvalent acid (E), and then mixing the obtained mixture, the pigment dispersion resin (D) and the pigment (F) to prepare the pigment dispersion paste (ii);
the metal oxide (c2) contains one or more metal elements selected from the group consisting of La, Nd, Y, Pr, Yb and Ce,
the monohydroxycarboxylic acid (c3) having 3 to 5 carbon atoms in total has an asymmetric carbon atom, the monohydroxycarboxylic acid (c3) containing 80% or more of an L-form among its optical isomers, and
in the bismuth-metal oxide mixture liquid (C) preparation step, the viscosity of the bismuth-metal oxide mixture liquid (C) is within a range of 2.5 mPa·s to 15 mPa·s.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein
in the bismuth-metal oxide mixture liquid (C) preparation step, the bismuth-metal oxide mixture liquid (C) is prepared by performing mixing of the bismuth compound (c1) with the monohydroxycarboxylic acid (c3) and mixing of the metal oxide (c2) with the monohydroxycarboxylic acid (c3), and then mixing the mixtures obtained by the respective mixings with a solvent,
the mixing of the bismuth compound (c1) with the monohydroxycarboxylic acid (c3) is performed at a pH within a range of 2.0 to 4.1, and
the ratio of the number of moles of the metal element of the bismuth compound (c1) contained in the bismuth-metal oxide mixture liquid (C) to the number of moles of the monohydroxycarboxylic acid (c3) is in a range of (c1):(c3)=1:0.5 to 1:4.0.

### Claim 3 (depends on 2)

The preparation method according to claim 2, wherein in the mixing of the metal oxide (c2) with the monohydroxycarboxylic acid (c3), the ratio of the number of moles of the metal element of the metal oxide (c2) contained in the bismuth-metal oxide mixture liquid (C) to the number of moles of the monohydroxycarboxylic acid (c3) is within a range of (c2):(c3)=1:0.5 to 1:3.25.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein the molar ratio of the metal element of the bismuth compound (c1) to that of the metal oxide (c2) contained in the bismuth-metal oxide mixture liquid (C) is within a range of (c1):(c2)=0.1:1 to 10:1.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein the polyvalent acid (E) is one or more compounds selected from the group consisting of compounds having two or more carboxylic acid groups and compounds having a phosphoric acid group.

### Claim 6

A pigment dispersion paste to be used for the preparation of a cationic electrodeposition coating composition, wherein
the pigment dispersion paste comprises a bismuth-metal oxide mixture liquid (C) comprising a bismuth compound (c1), a metal oxide (c2), a monohydroxycarboxylic acid (c3) having 3 to 5 carbon atoms in total and a solvent; a pigment dispersion resin (D); a polyvalent acid (E); and a pigment (F); the metal oxide (c2) contains one or more metal elements selected from the group consisting of La, Nd, Y, Pr, Yb and Ce,
the monohydroxycarboxylic acid (c3) having 3 to 5 carbon atoms in total has an asymmetric carbon atom, the monohydroxycarboxylic acid (c3) containing 80% or more of an L-form among its optical isomers,
the polyvalent acid (E) is one or more compounds selected from the group consisting of compounds having two or more carboxylic acid groups and compounds having a phosphoric acid group, and
the ratio of the total number of moles of the metal elements of the bismuth compound (c1) and the metal oxide (c2) contained in the bismuth-metal oxide mixture liquid (C) to the number of moles of the monohydroxycarboxylic acid (c3) is within a range of ((c1)+(c2)):(c3)=0.55:1 to 4:1.

### Claim 7 (depends on 6)

A cationic electrodeposition coating composition comprising the pigment dispersion paste according to claim 6.

### Claim 8

A method for preparing a pigment dispersion paste, wherein
the pigment dispersion paste comprises a bismuth-metal oxide mixture liquid (C) comprising a bismuth compound (c1), a metal oxide (c2), a monohydroxycarboxylic acid (c3) having 3 to 5 carbon atoms in total and a solvent; a pigment dispersion resin (D); a polyvalent acid (E); and a pigment (F); the method for preparing the pigment dispersion paste comprises the following steps:
a bismuth-metal oxide mixture liquid (C) preparation step of mixing the bismuth compound (c1), the metal oxide (c2), the monohydroxycarboxylic acid (c3) having 3 to 5 carbon atoms in total and the solvent to prepare the bismuth-metal oxide mixture liquid (C); and
a pigment dispersion paste (ii) preparation step of mixing the obtained bismuth-metal oxide mixture liquid (C) and the polyvalent acid (E), and then mixing the obtained mixture, the pigment dispersion resin (D) and the pigment (F) to prepare the pigment dispersion paste (ii);
the metal oxide (c2) contains one or more metal elements selected from the group consisting of La, Nd, Y, Pr, Yb and Ce,
the monohydroxycarboxylic acid (c3) having 3 to 5 carbon atoms in total has an asymmetric carbon atom, the monohydroxycarboxylic acid (c3) containing 80% or more of an L-form among its optical isomers, and
in the bismuth-metal oxide mixture liquid (C) preparation step, the viscosity of the bismuth-metal oxide mixture liquid (C) is within a range of 2.5 mPa·s to 15 mPa·s.

### Claim 9 (depends on 8)

The preparation method according to claim 8, wherein
in the bismuth-metal oxide mixture liquid (C) preparation step, the bismuth-metal oxide mixture liquid (C) is prepared by performing mixing of the bismuth compound (c1) with the monohydroxycarboxylic acid (c3) and mixing of the metal oxide (c2) with the monohydroxycarboxylic acid (c3), and then mixing the mixtures obtained by the respective mixings with a solvent,
the mixing of the bismuth compound (c1) with the monohydroxycarboxylic acid (c3) is performed at a pH within a range of 2.0 to 4.1, and
the ratio of the number of moles of the metal element of the bismuth compound (c1) contained in the bismuth-metal oxide mixture liquid (C) to the number of moles of (c3) is within a range of (c1):(c3)=1:0.5 to 1:4.0.

### Claim 10 (depends on 8)

The preparation method according to claim 8, wherein in the mixing of the metal oxide (c2) with the monohydroxycarboxylic acid (c3), the ratio of the number of moles of the metal element of the metal oxide (c2) contained in the bismuth-metal oxide mixture liquid (C) to the number of moles of the monohydroxycarboxylic acid (c3) is within a range of (c2):(c3)=1:0.5 to 1:3.25.