# US 2022/0282075 A1 · Polymer blends having improved thermal properties

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282075 A1
- Document ID: US20220282075A1
- Status: Published application
- Kind: A1
- Application number: 17/637,729
- Filed: 2020-08-27
- Published: 2022-09-08
- Earliest claimed: 2019-08-29
- Assignees: Dow Global Technologies LLC
- Applicants: Dow Global Technologies LLC
- Inventors: Xian Jiang; Yushan Hu
- Web page: https://patentgrep.com/patent/US20220282075A1

## CPC

- C08L 23/0876: Salts thereof, i.e. ionomers
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08L 23/142: {at least partially crystalline copolymers of propene with other olefins}
- C08L 53/00: Compositions of block copolymers containing at least one sequence of a polymer obtained by reactions only involving carbon-to-carbon unsaturated bonds; Compositions of derivatives of such polymers
- C08L 2205/03: containing three or more polymers in a blend
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Embodiments are directed to polymer blends and molded articles including polymer blends. Embodiments of the polymer blend may include 1 to 40 wt. % of a crystalline block composite and from 60 wt. % to 99 wt. % of an ionomer formed from a partially neutralized precursor acid copolymer. The crystalline block composite may include an EP-iPP diblock polymer, an isotactic polypropylene homopolymer, and a copolymer of ethylene and propylene. The crystalline block composite may include greater than 50 wt. % of the isotactic polypropylene homopolymer. The precursor acid copolymer may include copolymerized units of ethylene and 5 wt. % to 30 wt. %, based on the total weight of the precursor acid copolymer, of copolymerized units of an α,β-ethylenically unsaturated carboxylic acid having 3 to 8 carbon atoms. About 25% to about 65% of the acid groups derived from the α,β-ethylenically unsaturated carboxylic acid of the precursor acid copolymer may be neutralized.

## Claims

### Claim 1

A polymer blend comprising:
1 to 40 wt. % of a crystalline block composite comprising an EP-iPP diblock polymer, iPP, and EP, wherein iPP is isotactic polypropylene homopolymer and EP is a copolymer of ethylene and propylene, and wherein the crystalline block composite comprises greater than 50 wt. % iPP; and
from 60 wt. % to 99 wt. % of an ionomer formed from a partially neutralized precursor acid copolymer, wherein the precursor acid copolymer (a) comprises copolymerized units of ethylene and 5 wt. % to 30 wt. %, based on the total weight of the precursor acid copolymer, of copolymerized units of an α,β-ethylenically unsaturated carboxylic acid having 3 to 8 carbon atoms, and wherein about 25% to about 65% of the acid groups derived from the α,β-ethylenically unsaturated carboxylic acid of the precursor acid copolymer are neutralized.

### Claim 2 (depends on 1)

The polymer blend of claim 1, wherein the ionomer has a melt index, I2, (according to ASTM D1238 at 190° C., 2.16 kg) of 0.1 g/10 min to 50 g/10 min.

### Claim 3 (depends on 1)

The polymer blend of claim 1, wherein the crystalline block composite has a melt flow rate, MFR, (according to ASTM D1238 at 230° C., 2.16 kg) of 2 g/10 min to 50 g/10 min.

### Claim 4 (depends on 1)

The polymer blend of claim 1, wherein the crystalline block composite comprises greater than 60 wt. % iPP.

### Claim 5 (depends on 1)

The polymer blend of claim 1, wherein the acid groups are neutralized by one or more of a zinc ion-containing base, a magnesium ion-containing base, and a sodium-ion-containing base.

### Claim 6 (depends on 1)

The polymer blend of claim 1, wherein the polymer blend comprises 5 to 15 wt. % of the crystalline block composite, and 85 to 95 wt. % of the ionomer.

### Claim 7 (depends on 1)

The polymer blend of claim 1, wherein the α,β-ethylenically unsaturated carboxylic acid comprises acrylic acid, methacrylic acid, or combinations thereof.

### Claim 8 (depends on 1)

A molded article comprising the polymer blend of claim 1.

### Claim 9 (depends on 8)

The molded article of claim 8, wherein the molded article is an injection molded article, or a compression molded article.

### Claim 10 (depends on 8)

The molded article of claim 8, wherein the molded article exhibits an internal haze of less than or equal to 20%.

### Claim 11 (depends on 8)

The molded article of claim 8, wherein the molded article exhibits an oven creep of less than 150% elongation after 160 minutes.

### Claim 12 (depends on 8)

The molded article of claim 8, wherein the molded article exhibits a tensile strength of at least 30 MPa.

### Claim 13 (depends on 8)

The molded article of claim 8, wherein the molded article exhibits at a heat deflection temperature (HDT) of greater than 35° C. according ISO 75 using a 0.45 MPa load.

### Claim 14 (depends on 8)

The molded article of claim 8, wherein the crystalline block composite exhibits a refractive index (RI) of 1.49 to 1.52.