# US 2022/0282054 A1 · Super-wet surface and preparation method therefor and application thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282054 A1
- Document ID: US20220282054A1
- Status: Published application
- Kind: A1
- Application number: 17/753,209
- Filed: 2020-08-04
- Published: 2022-09-08
- Earliest claimed: 2019-08-23
- Assignees: China Petroleum & Chemical Corporation; Beijing Research Institute of Chemical Industry, China Petroleum & Chemical Corporation
- Applicants: China Petroleum & Chemical Corporation; Beijing Research Institute of Chemical Industry, China Petroleum & Chemical Corporation
- Inventors: Jinliang QIAO; Songhe WANG; Xiaohong ZHANG; Guicun QI; Zhihai SONG; Chuanlun CAI; Xiang WANG; Jinmei LAI; Binghai LI; Haibin JIANG; Yue RU; Jiangru ZHANG; Jianming GAO; Hongbin ZHANG; Peng HAN; Chao JIANG; Zhaoyan GUO
- Web page: https://patentgrep.com/patent/US20220282054A1

## CPC

- B01D 67/00931: {by introduction of specific groups after membrane formation, e.g. by grafting}
- B01D 17/02: Separation of non-miscible liquids
- B01D 67/0006: {by chemical reactions (in-situ polymerisation, polycondensation, cross-linking or reaction for manufacturing composite membranes B01D69/125)}
- B01D 67/009: {with wave-energy, particle-radiation or plasma}
- B01D 69/02: characterised by their properties
- B01D 71/262: {Polypropylene}
- C02F 1/40: Devices for separating or removing fatty or oily substances or similar floating material (cleaning or keeping clear the surface of open water from oil or like materials E02B15/04; devices in sewers for separating liquid or solid substances from sewage E03F5/14, e.g. for use in drains leading to the sewer E03F5/16)
- C02F 1/44: by dialysis, osmosis or reverse osmosis {(general membrane separation processes B01D61/00, membrane modules B01D63/00, electrodialysis C02F1/4693, combination of membrane modules and bioreactors C02F3/1268)}
- C08J 7/18: using wave energy or particle radiation
- B01D 2323/02: Hydrophilization
- B01D 2323/38: Graft polymerization
- B01D 2323/385: involving radiation
- B01D 2325/02: Details relating to pores or porosity of the membranes
- B01D 2325/36: Hydrophilic membranes
- C02F 2101/32: Hydrocarbons, e.g. oil
- C08J 2323/12: Polypropene
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

A super-wet surface is a polypropylene surface, on which a hydrophilic side group is grafted, having a micro-nano structure. The super-wet surface is at least super-hydrophilic and does not contain an initiator residue. The super-wet surface is prepared by grafting, in the absence of an initiator, by means of microwave irradiation, a monomer for forming a side group, on the polypropylene surface, as a grafting base, having a micro-nano structure. In the preparation of the super-wet surface, the molecular weight of polypropylene does not decrease after grafting, there is no residual monomer or initiator residue, and the super-wetting effect of the obtained surface is lasting and stable. The super-wet surface can be used in bonding, spraying, oil-water separation, water treatment, biology, medicine and energy fields.

## Claims

### Claim 1

A superwetting surface, which is a polypropylene surface having a micro-nano structure and grafted with a hydrophilic side group, wherein the superwetting surface is at least super-hydrophilic and does not contain an initiator residue.

### Claim 2 (depends on 1)

The superwetting surface according to claim 1, characterized in that the water contact angle of the superwetting surface is less than or equal to 10°, preferably less than or equal to 8°, more preferably less than or equal to 5°, even more preferably less than or equal to 1°, and most preferably about 0°.

### Claim 3 (depends on 1)

The superwetting surface according to claim 1, characterized in that the feature size of the micro-nano structure of the polypropylene surface as the grafting base is 1 nm-100 μm; preferably the micro-nano structure is a structure produced on the polypropylene surface by a thermally-induced phase separation process, photolithography technology, femtosecond laser processing technology, plasma etching technology, electrospinning method, nano-imprinting, nano-casting, ultra-precision micro-milling technology or by an electric arc.

### Claim 4 (depends on 3)

The superwetting surface according to claim 3, characterized in that the polypropylene surface as the grafting base is a polypropylene porous membrane, a polypropylene flat membrane or a polypropylene hollow fiber microporous membrane, wherein the polypropylene porous membrane preferably has an average pore diameter of less than 100 preferably 10 nm-80 and preferably has a porosity of 50-90%, more preferably 60-80%.

### Claim 5 (depends on 1)

The superwetting surface according to claim 1, characterized in that the hydrophilic side group comprises a unit formed from one or more monomers containing a heteroatom selected from the group consisting of oxygen, sulfur, nitrogen, silicon, halogen and combinations thereof or a substituent thereof and containing a carbon-carbon double bond; preferably, the monomer is at least one selected from the group consisting of organic acids and derivatives thereof (for example, anhydrides, esters, and salts) and vinyl silanes; wherein the organic acid and derivative thereof is preferably selected from the group consisting of maleic anhydride and derivatives thereof, (meth)acrylic acid and derivatives thereof (e.g., glycidyl methacrylate), vinyl acetate, alkenyl sulfonic acid and derivatives thereof, vinyl benzoic acid and derivatives thereof, itaconic acid and derivatives thereof, oleic acid and derivatives thereof, arachidonic acid and derivatives thereof (in particular their salt forms) and combinations thereof; wherein the vinyl silane is preferably one or more of the compounds represented by Formula (1):
CH2═CH—(CH2)nSiX3 Formula (1),
wherein n=0 to 3, each X is the same or different and independently represents a chloro group, a methoxy group, an ethoxy group, and an acetoxy group; more preferably, the hydrophilic side group comprises or consists of a unit formed from a salt of an organic acid.

### Claim 6 (depends on 1)

The superwetting surface according to claim 1, characterized in that the polypropylene surface is further grafted with a lipophilic side group; the lipophilic side group is preferably selected from the group consisting of vinyl silicone oil side groups, styrene side groups and combinations thereof; the vinyl silicone oil is preferably selected from the group consisting of vinyl-terminated silicone oils, high-vinyl silicone oils and combinations thereof, and more preferably is selected from the group consisting of methyl vinyl silicone oil, vinyl hydrogen-containing silicone oil, divinyl silicone oil and combinations thereof; preferably, the oil contact angle of the superwetting surface is less than 90°, preferably less than or equal to 10°, more preferably less than or equal to 5°, still more preferably less than or equal to 1°, and most preferably about 0°.

### Claim 7 (depends on 1)

The superwetting surface according to claim 1, characterized in that the superwetting surface is prepared by the following method, wherein
a monomer for forming the side group and a polypropylene surface having a micro-nano structure as the grafting base are subjected to grafting reaction by microwave irradiation, in the absence of an initiator, optionally in the case of adding an inorganic microwave absorbing medium;
preferably, when the monomer comprises a monomer for forming a lipophilic side group, an inorganic microwave absorbing medium is added;
preferably, when the monomer is selected from the group consisting of organic acids or anhydrides thereof or esters thereof and combinations thereof, the method further comprises the step of reacting the product obtained after the grafting reaction with a base.

### Claim 8 (depends on 1)

A method for preparing the superwetting surface according to claim 1, comprising:
subjecting a monomer for forming the side group and a polypropylene surface having a micro-nano structure as the grafting base to grafting reaction by microwave irradiation, in the absence of an initiator.

### Claim 9 (depends on 8)

The method according to claim 8, characterized in that the method includes any one of the following approaches 1) to 4):
1) contacting and mixing the polypropylene surface with the monomer for forming the hydrophilic side group, wherein an inorganic microwave absorbing medium is optionally added; and then subjecting the resulting mixture to microwave irradiation grafting without the addition of an initiator; wherein the mixture optionally further comprises a monomer for lipophilic side group and an inorganic microwave absorbing medium;
2) contacting and mixing the polypropylene surface with the monomer for forming the hydrophilic side group, wherein an inorganic microwave absorbing medium is optionally added; then subjecting the resulting mixture to microwave irradiation grafting without the addition of an initiator; and then mixing the obtained grafted product with the monomer for forming the lipophilic side group and an inorganic microwave absorbing medium, and performing microwave irradiation grafting without the addition of an initiator;
3) contacting and mixing the polypropylene surface with the monomer for forming the lipophilic side group and an inorganic microwave absorbing medium, then subjecting the resulting mixture to microwave irradiation grafting without the addition of an initiator; then mixing the obtained grafted product with the monomer for forming the hydrophilic side group under the condition of optionally adding an inorganic microwave absorbing medium, and performing microwave irradiation grafting without the addition of an initiator;
4) in any one of the above 1)-3), when the monomer for forming the hydrophilic side group is at least one of an organic acid or an anhydride or ester thereof, further comprising the step of contacting and mixing the polypropylene surface grafted with at least one side group of an organic acid or an anhydride or ester thereof with a base; wherein, preferably, the base is one or more hydroxides, the hydroxide is preferably selected from the group consisting of metal hydroxides and ammonia water; wherein the metal hydroxide is preferably selected from the group consisting of sodium hydroxide, potassium hydroxide, barium hydroxide, lithium hydroxide, strontium hydroxide, calcium hydroxide, iron hydroxide, ferrous hydroxide, zinc hydroxide, magnesium hydroxide, cobalt hydroxide, gold hydroxide, aluminum hydroxide, copper hydroxide, beryllium hydroxide, rare earth hydroxide and combinations thereof, and preferably is selected from the group consisting of sodium hydroxide, potassium hydroxide, barium hydroxide, lithium hydroxide, strontium hydroxide, calcium hydroxide and combinations thereof; preferably, the amount of the base is 0.1-10% by weight based on the amount of the polypropylene surface; and preferably 1-8% by weight; preferably, the base is used in the form of an aqueous solution;
preferably, at least one of the above mixing processes is carried out under vacuum.

### Claim 10 (depends on 9)

The method according to claim 9, characterized in that the amount of the monomer for forming the hydrophilic side group is 0.1-10% by weight, preferably 1-8% by weight, based on the amount of the polypropylene surface; the monomer for forming the hydrophilic side group can be used in the form of a solution in which the monomer is dissolved in one or more solvents;
preferably, the solvent is selected from the group consisting of alcohols, ketones, esters, water and combinations thereof.

### Claim 11 (depends on 9)

The method according to claim 9, characterized in that the amount of the monomer for forming the lipophilic side group is 0.1-30% by weight, preferably 1-20% by weight, based on the amount of the polypropylene surface; the monomer for forming the lipophilic side group can be used in the form of a solution in which the monomer is dissolved in one or more solvents; preferably, the solvent is selected from the group consisting of alcohols, ketones, esters, water and combinations thereof.

### Claim 12 (depends on 8, 9, 10, 11)

The method according to claim 8 any one of claims 8 to 11, characterized in that an inorganic microwave absorbing medium is added; preferably, the inorganic microwave absorbing medium is selected from the group consisting of metal hydroxides, metal salts, metal oxides, graphite materials, ferroelectric materials, electrolytic stone, chalcopyrite and combinations thereof; preferably, the metal hydroxide is selected from the group consisting of potassium hydroxide, barium hydroxide, sodium hydroxide, lithium hydroxide, strontium hydroxide, calcium hydroxide, iron hydroxide, ferrous hydroxide, zinc hydroxide, magnesium hydroxide, cobalt hydroxide, gold hydroxide, aluminum hydroxide, copper hydroxide, beryllium hydroxide, rare earth hydroxide and combinations thereof; the metal salt is selected from the group consisting of ammonium nitrate, potassium nitrate, sodium nitrate, barium nitrate, calcium nitrate, magnesium nitrate, aluminum nitrate, manganese nitrate, zinc nitrate, ferric nitrate, ferrous nitrate, copper nitrate, silver nitrate, ammonium chloride, potassium chloride, sodium chloride, barium chloride, calcium chloride, magnesium chloride, aluminum chloride, manganese chloride, zinc chloride, ferric chloride, ferrous chloride, copper chloride, ammonium sulfate, potassium sulfate, sodium sulfate, calcium sulfate, magnesium sulfate, aluminum sulfate, manganese sulfate, zinc sulfate, iron sulfate, ferrous sulfate, copper sulfate, silver sulfate, ammonium carbonate, potassium carbonate, sodium carbonate, magnesium carbonate, calcium carbonate, barium carbonate, potassium dihydrogen phosphate, barium titanate, strontium titanate, copper calcium titanate and combinations thereof; the metal oxide is selected from the group consisting of ferric oxide, ferroferric oxide and combinations thereof; the graphite material is preferably selected from the group consisting of carbon black, graphite powder, graphene, reduction product of graphene oxide (the reducing agent is for example ascorbic acid), carbon nanotubes, activated carbon and combinations thereof; preferably, the amount of the inorganic microwave absorbing medium in single usage is 0.1-10% by weight, preferably 1-8% by weight of the amount of the polypropylene surface; preferably, the inorganic microwave absorbing medium is directly added, or is added in the form of a solution of dispersion in which it is dissolved or dispersed in one or more solvents; preferably, the one or more solvents are selected from the group consisting of alcohols, ketones, esters, water and combinations thereof; and
preferably, the dispersion comprises a surfactant.

### Claim 13 (depends on 8)

A superwetting surface prepared by the method according to claim 8.

### Claim 14 (depends on 1)

An article, constituted by the superwetting surface according to claim 1, or comprising the superwetting surface according to claim 1; wherein the article is preferably a film, sheet, plate, or molded article.

### Claim 15 (depends on 1)

A method of using the superwetting surface according to claim 1 in biology, medicine or energy field.

### Claim 16 (depends on 1)

Bonding, spraying, oil-water separation or water treatment method using the superwetting surface according to claim 1, wherein said method being for example bonding of plastic articles, spraying of the outer packaging of food bags, and spraying of the automobile bumper.

### Claim 17 (depends on 14)

A method of using the article according to claim 14 in biology, medicine or energy field.

### Claim 18 (depends on 14)

Bonding, spraying, oil-water separation or water treatment method using the article according to claim 14, said method being for example bonding of plastic articles, spraying of the outer packaging of food bags, and spraying of the automobile bumper.