# US 2022/0282052 A1 · Laminate, method for manufacturing laminate, and method for manufacturing flexible electronic device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282052 A1
- Document ID: US20220282052A1
- Status: Published application
- Kind: A1
- Application number: 17/633,482
- Filed: 2020-09-30
- Published: 2022-09-08
- Earliest claimed: 2019-10-08
- Assignees: Toyobo Co., Ltd.
- Applicants: Toyobo Co., Ltd.
- Inventors: Naoki WATANABE; Harumi YONEMUSHI; Kousuke SASAI (deceased); Hiroyuki WAKUI
- Web page: https://patentgrep.com/patent/US20220282052A1

## CPC

- B32B 27/281: {comprising polyimides}
- B32B 7/06: permitting easy separation
- B32B 17/10: of synthetic resin
- B32B 2307/412: Transparent
- B32B 2457/14: Semiconductor wafers
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

The purpose is to provide a laminate useful as a temporary support for producing a large-area, high-definition flexible electronic device, the laminate having stably low adhesive strength between a colorless and highly transparent polyimide film and an inorganic substrate even in the case of a large surface area and having few blister defects. The laminate that attains the purpose is obtained by initially wetting either one of an inorganic substrate coated with the silane coupling agent and a colorless polyimide film with an aqueous medium, and then laminating while pressing out the aqueous medium.

## Claims

### Claim 1

A laminate comprising:
an inorganic substrate;
a silane coupling agent layer; and
a polyimide film of which a yellow index is 10 or less, a light transmittance at a wavelength of 400 nm is 70% or more, a tensile elasticity in both a MD direction and a TD direction is 3 GPa or more, and CTE in both a MD direction and a TD direction is −5 ppm/° C. to +55 ppm/° C.
in this order, wherein an initial adhesive strength by a 90-degree peeling method when the polyimide film is peeled off from the laminate is 0.06 N/cm or more and 0.25 N/cm or less.

### Claim 2 (depends on 1)

The laminate according to claim 1, wherein a blister defect density is 5 spots or less per 1 square meter.

### Claim 3 (depends on 1)

The laminate according to claim 1, wherein the polyimide film is rectangular, has an area of 0.65 square meter or more, and has a rectangular side of at least 700 mm or more.

### Claim 4 (depends on 1)

The laminate according to claim 1, wherein the silane coupling agent layer is a silane coupling agent.

### Claim 5 (depends on 1)

A method for manufacturing the laminate according to claim 1, the method comprising at least:
(1) a step of coating at least one surface of an inorganic substrate with a silane coupling agent;
(2) a step of wetting either or both of a silane coupling agent-coated surface of the inorganic substrate and a bonding surface side of a polyimide film with an aqueous medium;
(3) a step of stacking a polyimide film on the silane coupling agent-coated surface of the inorganic substrate; and
(4) a step of pressurizing the inorganic substrate and the polyimide film while extruding the aqueous medium from between the silane coupling agent-coated surface of the inorganic substrate and the bonding surface of the polyimide film.

### Claim 6 (depends on 1)

A method for manufacturing the laminate according to claim 1, the method comprising at least:
(1) a step of coating at least one surface of a heat-resistant polyimide film with a silane coupling agent;
(2) a step of wetting either or both of a bonding surface side of an inorganic substrate and a silane coupling agent-coated surface of the polyimide film with an aqueous medium;
(3) a step of stacking the silane coupling agent-coated surface of the heat-resistant polyimide film on the inorganic substrate; and
(4) a step of pressurizing the inorganic substrate and the polyimide film while extruding the aqueous medium from between the bonding surface of the inorganic substrate and the silane coupling agent-coated surface of the polyimide film.

### Claim 7 (depends on 5)

A method for manufacturing a flexible device, the method comprising a step of forming a functional element on a surface on an opposite side to a bonding surface with an inorganic substrate of a polyimide film of a laminate obtained in the manufacturing process according to claim 5.