# US 2022/0282047 A1 · Method of making a homogeneous mixture of polyolefin solids and an organic peroxide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0282047 A1
- Document ID: US20220282047A1
- Status: Published application
- Kind: A1
- Application number: 17/635,720
- Filed: 2020-08-26
- Published: 2022-09-08
- Earliest claimed: 2019-08-29
- Assignees: Dow Global Technologies LLC
- Applicants: Dow Global Technologies LLC
- Inventors: Saurav S. Sengupta; Timothy J. Person; Paul J. Caronia; Neil W. Dunchus
- Web page: https://patentgrep.com/patent/US20220282047A1

## CPC

- B29B 7/286: {measuring properties of the mixture, e.g. temperature, density (B29B7/283 takes precedence)}
- C08J 3/203: {Solid polymers with solid and/or liquid additives}
- B01F 23/551: {using vibrations}
- B29B 7/08: shaking, oscillating or vibrating
- B29B 7/823: {Temperature control}
- B29B 7/826: {Apparatus therefor}
- B29B 7/90: Fillers or reinforcements {, e.g. fibres}
- B29K 2023/06: {PE, i.e. polyethylene}
- B29K 2023/0633: {LDPE, i.e. low density polyethylene}
- B29K 2023/12: {PP, i.e. polypropylene}
- B29K 2105/0044: {Stabilisers, e.g. against oxydation, light or heat}
- B29L 2031/3462: {Cables}
- C08J 2323/06: Polyethene
- C08J 2323/08: Copolymers of ethene (C08J2323/16 takes precedence)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B01F: MIXING, e.g. DISSOLVING, EMULSIFYING OR DISPERSING (mixing paints B44D3/06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A method of making a homogeneous mixture of polyolefin solids and an organic peroxide without melting the polyolefin solids during the making. The method comprises applying acoustic energy at a frequency of from 20 to 100 hertz to a heterogeneous mixture comprising the polyolefin solids and the organic peroxide for a period of time sufficient to substantially intermix the polyolefin solids and the organic peroxide together while maintaining temperature of the heterogeneous mixture below the melting temperature of the polyolefin solids, thereby making the homogeneous mixture without melting the polyolefin solids.

## Claims

### Claim 1

A method of making a homogeneous mixture of polyolefin solids and organic peroxide without melting the polyolefin solids during the making, the method comprising applying acoustic energy at a frequency of from 20 to 100 hertz (Hz) to a heterogeneous mixture comprising (A) polyolefin solids and (B) organic peroxide for a period of time sufficient to substantially intermix the (A) polyolefin solids and the (B) organic peroxide together while maintaining temperature of the heterogeneous mixture (and, for that matter, the temperature of the homogeneous mixture made therefrom) below the melting temperature of the (A) polyolefin solids, thereby making the homogeneous mixture without melting the (A) polyolefin solids; wherein the (A) polyolefin solids are from 95.0 to 99.9 weight percent (wt %) and the (B) organic peroxide is from 0.1 to 5.0 wt %, respectively, of the combined weights of the constituents (A) and (B).

### Claim 2 (depends on 1)

The method of claim 1 wherein the applying acoustic energy step is characterized by any one of limitations (i) to (v): (i) the frequency is from 50 to 70 Hz; (ii) the period of time is from 0.5 minute to 4 hours; (iii) both (i) and (ii); (iv) the maintaining temperature of the heterogeneous mixture below the melting temperature of the (A) polyolefin solids comprises maintaining temperature of the heterogeneous mixture at from −20° to 109° C.; and (v) both (iv) and any one of (i) to (iii).

### Claim 3 (depends on 1)

The method of claim 1 wherein the (A) polyolefin solids are characterized by a physical form (i.e., solid particulate form) that is a powder, granules, pellets, or a blend of any two or more thereof, and by a melting temperature that is from 61° to 180° C.; and the (B) organic peroxide is a liquid organic peroxide or a solid organic peroxide.

### Claim 4 (depends on 1)

The method of claim 1 wherein the polyolefin of the (A) polyolefin solids consists essentially of one or more ethylene-based polymers; wherein each ethylene-based polymer is a low-density polyethylene (LDPE) polymer or a combination of the LDPE polymer and a polyolefin selected from the group consisting of: a second LDPE polymer; a linear low-density polyethylene polymer; and a high-density polyethylene polymer. In other embodiments the polyolefin of the (A) polyolefin solids consists essentially of an LDPE and a polypropylene polymer.

### Claim 5 (depends on 1)

The method of claim 1 wherein the organic peroxide is a solid organic peroxide.

### Claim 6 (depends on 1)

The method of claim 1 wherein the heterogeneous mixture further comprises one or more additives that is/are not the (A) polyolefin solids or the (B) organic peroxide, and the applying acoustic energy step comprises applying acoustic energy at a frequency of from 20 to 100 hertz (Hz) to the heterogeneous mixture comprising the (A) polyolefin solids, the (B) organic peroxide, and the one or more additives that do not include a peroxide for a period of time sufficient to substantially intermix (thoroughly or completely homogenize) the (A) polyolefin solids, the (B) organic peroxide, and the one or more additives together while maintaining temperature of the heterogeneous mixture below the melting temperature of the (A) polyolefin solids, thereby making the homogeneous mixture further comprising the one or more additives, without melting the (A) polyolefin solids.

### Claim 7 (depends on 6)

The method of claim 6 wherein at least one of the one or more additives that is not constituents (A) or (B) is independently a liquid additive or particulate solid additive independently selected from additives (C) to (D): a liquid or particulate solid (C) antioxidant; and a liquid or particulate solid (D) stabilizer for stabilizing the homogeneous mixture against effects of ultraviolet light and/or heat.

### Claim 8 (depends on 7)

The method of claim 7 wherein the one or more additives include one or more of solid antioxidant (C)-1: tris[(4-tert-butyl-3-hydroxy-2,6-dimethylphenyl)methyl]-1,3,5-triazine-2,4,6-trione; solid antioxidant (C)-2: distearyl thiodipropionate; and solid stabilizer (D)-1: N,N′-bisformyl-N,N′-bis(2,2,6,6-tetramethyl-4-piperidinyl)-hexamethylenediamine.

### Claim 9 (depends on 1)

The method of claim 1 further comprising, before the applying acoustic energy step, a step of melting the (A) polyolefin solids to make a melt thereof, and mechanically blending the melt of (A) with one or more additives that are not (B) organic peroxide to give a melt mixture that is free of (B) organic peroxide; shaping the melt mixture to give a shaped melt mixture; and cooling the shaped melt mixture to give the (A) polyolefin solids containing one or more additives; and combining the (A) polyolefin solids containing one or more additives with the (B) organic peroxide to give the heterogeneous mixture.

### Claim 10 (depends on 1)

The method of claim 1 further comprising curing the homogeneous mixture to give a crosslinked homogeneous product.