# US 2022/0281134 A1 · Method for producing a part from composite material by injecting a filled slip into a fibrous texture

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0281134 A1
- Document ID: US20220281134A1
- Status: Published application
- Kind: A1
- Application number: 17/624,997
- Filed: 2020-06-30
- Published: 2022-09-08
- Earliest claimed: 2019-07-11
- Assignees: Safran Aircraft Engines
- Applicants: Safran Aircraft Engines
- Inventors: Nicolas DROZ; Célia IGLESIAS CANO; Philippe Charles Alain LE BIEZ; Ludovic Philippe LIAIS
- Web page: https://patentgrep.com/patent/US20220281134A1

## CPC

- B28B 1/261: {Moulds therefor (absorbent moulds in general B28B7/344)}
- B28B 1/24: by injection moulding {(injection moulding of ceramic slips B28B1/265; of tubular articles B28B21/38)}
- B28B 1/262: {Mould materials; Manufacture of moulds or parts thereof}
- B28B 7/342: {which are at least partially destroyed, e.g. broken, molten, before demoulding; Moulding surfaces or spaces shaped by, or in, the ground, or sand or soil, whether bound or not; Cores consisting at least mainly of sand or soil, whether bound or not}
- B28B 7/348: {of plastic material or rubber}
- B28B 11/243: {Setting, e.g. drying, dehydrating or firing ceramic articles (B28B11/242 takes precedence)}
- B28B 23/0006: {the reinforcement consisting of aligned, non-metal reinforcing elements}
- C04B 35/117: Composites
- C04B 35/14: based on silica
- C04B 35/18: rich in aluminium oxide
- C04B 35/185: Mullite {3Al2O3-2SiO2}
- C04B 35/447: based on phosphates {, e.g. hydroxyapatite}
- C04B 35/565: based on silicon carbide
- C04B 35/58071: {based on titanium borides}
- C04B 35/584: based on silicon nitride
- C04B 35/6263: {characterised by their solids loadings, i.e. the percentage of solids}
- C04B 35/62844: {Coating fibres}
- C04B 35/62892: {with a coating layer consisting of particles}
- C04B 35/638: Removal thereof
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C04B 35/80: Fibres, filaments, whiskers, platelets, or the like
- C04B 41/0072: {Heat treatment}
- C04B 2235/5224: Alumina or aluminates
- C04B 2235/5228: Silica and alumina, including aluminosilicates, e.g. mullite
- C04B 2235/5232: Silica or silicates other than aluminosilicates, e.g. quartz
- C04B 2235/5244: Silicon carbide
- C04B 2235/5248: Carbon, e.g. graphite
- C04B 2235/5252: having a specific pre-form
- C04B 2235/6022: Injection moulding
- C04B 2235/6027: Slip casting
- C04B 2235/606: Drying
- C04B 2235/616: Liquid infiltration of green bodies or pre-forms
- C04B 2235/6562: Heating rate
- C04B 2235/6567: Treatment time
- C04B 2235/661: Multi-step sintering
- B28B: SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER (foundry moulding B22C; working stone or stone-like material B28D; shaping of substances in a plastic state, in general B29C; making layered products not composed wholly of these substances B32B)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A manufacturing method for a composite material part includes injecting under pressure a slip containing a refractory ceramic particle powder into the moulding cavity of an injection tooling, draining the liquid from the slip that passed through the moulding cavity and retaining the particle powder inside the moulding cavity to obtain a blank including refractory particles, demoulding the blank, and heat treating the blank to form a part. The injection tooling includes a porous material mould consisting of a moulding cavity, an enclosure of rigid material in which the porous material mould is held, the enclosure further including an injection port, a discharge vent and an injection canal connecting the injection port to the moulding cavity of the porous mould for the injection of the slip into the moulding cavity. The injection tooling includes a sacrificial capsule of porous material placed in moulding cavity.

## Claims

### Claim 1

A manufacturing method for a part comprising:
injecting under pressure a slip containing a refractory ceramic particle powder into the moulding cavity of an injection tooling, draining the liquid from the slip that passed through the moulding cavity and retaining the particle powder inside said moulding cavity so as to obtain a blank comprising refractory particles,
demoulding the blank, and
heat treating the blank in order to form a part,
the injection tooling comprising a porous material mould consisting of a moulding cavity, an enclosure of rigid material in which the porous material mould is held, the enclosure further comprising at least one injection port, at least one discharge vent and at least one injection canal connecting said at least one injection port to the moulding cavity of the porous mould for the injection of the slip into the moulding cavity, wherein the injection tooling comprises a sacrificial capsule, the sacrificial capsule being placed in the moulding cavity, said capsule being made of a porous material and being formed by two part forming a closed internal volume in which the blank is located and allowing drainage of a liquid phase from the slip out of its closed internal volume, and demoulding the blank comprising the demoulding of the sacrificial capsule containing the blank.

### Claim 2 (depends on 1)

The manufacturing method according to claim 1, further comprising:
forming a fibrous texture from refractory ceramic fibres,
placing the fibrous texture in the internal volume of the sacrificial capsule before injecting the slip under pressure.

### Claim 3 (depends on 1)

The manufacturing method according to claim 1, further comprising the placement of glass beads in the internal volume of the sacrificial capsule.

### Claim 4 (depends on 1)

The manufacturing method according to claim 1, wherein the sacrificial capsule is made of a porous material identical to the porous material of the mould.

### Claim 5 (depends on 1)

The manufacturing method according to claim 1, wherein the sacrificial capsule is made of one of the following materials: porous resin, polytetrafluoroethylene or plaster.

### Claim 6 (depends on 1)

The manufacturing method according to claim 1, wherein the sacrificial capsule has a wall thickness comprised between 1 mm and 30 mm.

### Claim 7 (depends on 1)

The manufacturing method according to claim 1, wherein the sacrificial capsule comprises a first and second part assembled together, the first part consisting of a first cavity corresponding to one portion of the shape of the part to be manufactured, the second part comprising a second cavity corresponding to the other portion of the shape of the part to be manufactured.

### Claim 8 (depends on 1)

The manufacturing method according to claim 1, wherein the heat treatment of the blank comprises a first stage performed at a temperature between 40° C. and 95° C. so as to dry the liquid of the slip present in the sacrificial capsule and a second stage performed at a temperature comprised between 1000° C. and 1100° C. so as to bind the refractory ceramic particles together and form a part from the blank.

### Claim 9 (depends on 8)

The manufacturing method according to claim 8, wherein the first stage is performed according to a gentle elevation gradient comprised between 1° C./min and 6° C./min to reach a temperature comprised between 40° C. and 95° C. maintained for a duration comprised between 30 min and 90 min.

### Claim 10 (depends on 8)

The manufacturing method according to claim 8, wherein the heat treatment also comprises a third stage performed after the first stage and before the second stage, the third stage being performed at a temperature comprised between 450° C. and 600° C. so as to burn the sacrificial capsule.

### Claim 11 (depends on 10)

The manufacturing method according to claim 10, wherein the third stage is performed according to a gentle elevation gradient comprised between 1° C./min and 7° C./min to reach a temperature comprised between 450° C. and 600° C. maintained for a duration comprised between 30 min and 4 h.