# US 2022/0281006 A1 · Metal alloys with improved processability for direct metal laser sintering

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0281006 A1
- Document ID: US20220281006A1
- Status: Published application
- Kind: A1
- Application number: 17/594,974
- Filed: 2020-05-06
- Published: 2022-09-08
- Earliest claimed: 2019-05-06
- Assignees: EOS GmbH Electro Optical Systems
- Applicants: EOS GmbH Electro Optical Systems
- Inventors: Hannu Heikkinen; Antti Mutanen; Tiina Riskilae; Maija Nystroem; Jukka Simola; Eero Virtanen; Antti Poerhoenen; Tatu Syvaenen; Olli Nyrhilae
- Web page: https://patentgrep.com/patent/US20220281006A1

## CPC

- C22C 21/003: {containing at least 2.6% of one or more of the elements: tin, lead, antimony, bismuth, cadmium, and titanium}
- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 7/008: {characterised by the composition}
- B22F 10/28: Powder bed fusion, e.g. selective laser melting [SLM] or electron beam melting [EBM]
- B22F 10/34: of powder characteristics, e.g. density, oxidation or flowability
- B33Y 10/00: Processes of additive manufacturing
- B33Y 70/00: Materials specially adapted for additive manufacturing
- B33Y 70/10: Composites of different types of material, e.g. mixtures of ceramics and polymers or mixtures of metals and biomaterials
- C22C 19/055: {with the maximum Cr content being at least 20% but less than 30%}
- C22C 21/08: with silicon
- C22C 21/10: with zinc as the next major constituent
- C22C 21/12: with copper as the next major constituent
- C22C 21/16: with magnesium
- C22C 33/0285: {with Cr, Co, or Ni having a minimum content higher than 5%}
- C22C 33/0292: {with more than 5% preformed carbides, nitrides or borides}
- C22C 38/22: with molybdenum or tungsten
- B22F 2301/052: Aluminium
- B22F 2301/35: Iron
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- B33Y 30/00: Apparatus for additive manufacturing; Details thereof or accessories therefor
- Y02P 10/25: Process efficiency
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed are mixtures for use in additive manufacturing, wherein the powder mixture comprises first and second materials. The first material includes a metal alloy or a mixture of elemental precursors thereof, and is in powder form. The second material includes a reinforcement material comprising powder particles having a particle diameter of from 1 to less than 30 μm (as determined by laser scattering or laser diffraction). The inventive powder mixtures allows for the processing to three dimensions objects which are free of cracking and which thus have favourable mechanical characteristics. Further disclosed are processes for the preparation of corresponding powder mixtures and three dimensional objects, three dimensional objects prepared accordingly and devices for implementing processes for the preparation of such objects, as well as the use of a corresponding powder mixture to suppress crack formation in a three-dimensional object, which is prepared by additive manufacturing.

## Claims

### Claim 1

Powder mixture for use in the manufacture of a three-dimensional object by an additive manufacturing method, wherein the powder mixture comprises a first material of a metal alloy or a mixture of elemental precursors thereof and a second material of a reinforcement material comprising powder particles having a particle diameter of from 1 to less than 30 μm (as determined by laser scattering or laser diffraction), wherein the mixture comprises about 0.1 to about 10.0 wt.-% of the second material.

### Claim 2 (depends on 1)

Powder mixture according to claim 1, wherein the second material comprises at least one reinforcement material selected from the group of borides, carbides, nitrides, oxides and silicides.

### Claim 3 (depends on 1)

Powder mixture according to claim 1 comprising about 0.15 wt.-% or more, and/or about 7.0 wt.-% or less of the second material.

### Claim 4 (depends on 1)

Powder mixture according to claim 1, wherein the particles of the second material include at least one member selected from the group consisting of substantially spherical and substantially irregular.

### Claim 5 (depends on 1)

Powder mixture according to of claim 1, wherein the first material comprises iron and 4.75 to 5.5 wt.-% Cr, 1.0 to 1.75 wt.-% of Mo and 0.32 to 0.45 wt.-% of C and further comprises one or more of 0.8 to 1.25 wt.-% of Si, 0.8 to 1.2 wt.-% of V, 0.2 to 0.6 wt.-% of Mn, up to 0.05 wt.-% of P and 0.05 wt.-% of S.

### Claim 6 (depends on 1)

Powder mixture according to of claim 1, wherein the first material comprises aluminium and 4.0 to 5.0 wt.-% Cu, 0.15 to 0.35 wt.-% Ti and 0.15 to 0.35 wt.-% Mg and 0.4 to 1.0 wt.-% Ag.

### Claim 7 (depends on 1)

Powder mixture according to claim 1, wherein the first material comprises aluminium and 4.0 to 5.2 wt.-% Zn, 2.0 to 3.0 wt.-% Mg, up to 0.45 wt.-% Fe, up to 0.50 wt.-% Si, and one or more of up to 0.35 wt.-% of Cr, up to 0.5 wt.-% of Mn, up to 0.1 wt.-% of Ni, up to 0.15 wt.-% of Ti and up to 0.25 wt.-% of Zr, provided that the combined amount of Mn and Cr is >0.15 wt.-%.

### Claim 8 (depends on 1)

Powder mixture according to claim 1, wherein the first material comprises aluminium and 0.8 to 1.2 wt.-% Mg, 0.4 to 0.81 wt.-% Si, 0.15 to 0.4 wt.-% Cu, 0.04 to 0.35 wt.-% Cr, one or more of up to 0.7 wt.-% Fe, up to 0.15 wt.-% Mg, up to 0.25 wt.-% Zn and up to 0.15 wt.-% Ti.

### Claim 9 (depends on 1)

Powder mixture according to claim 1, wherein the first material comprises aluminium and 1 to 6 wt.-% Fe, 1.3 to 7.5 wt.-% of Cr, and 1.2 to 4 wt.-% of Ti, and up to 0.5 wt.-% of Si and up to 0.1 wt.-% of Mg.

### Claim 10 (depends on 1)

Powder mixture according to claim 1, wherein the first material comprises aluminium and 4.0 to 6.1 wt.-% Zn, 1.5 to 3.0 wt.-% Mg, up to 0.8 wt.-% Fe, up to 0.60 wt.-% Si, and one or more of up to 0.35 wt.-% of Cr, up to 0.5 wt.-% of Mn, up to 2.0 wt.-% of Cu, up to 0.30 wt.-% of Ti and 0.1 to 0.25 wt.-% of Zr.

### Claim 11 (depends on 10)

Powder mixture according to claim 10, wherein the first material comprises less than or equal to 0.25 wt.-% of Cu, less than or equal to 0.35 wt.-% of Cr, and 0.05 to 0.5 wt.-% of Mn, and wherein the combined amount of Mn and Cr is >0.15 wt.-%.

### Claim 12 (depends on 1)

Powder mixture according to claim 1, wherein the first powder has a particle size distribution with a d50 of from 20 to 100 μm.

### Claim 13 (depends on 1)

Process for the production of a powder mixture according to claim 1, wherein the powder mixture is produced by mixing the first powder and the second powder in a predetermined ratio, wherein the mixing is by dry mixing.

### Claim 14 (depends on 1)

Process for the manufacture of a three-dimensional object, comprising providing a powder mixture as defined in claim 1 and preparing the object by applying the mixture layer on layer and selectively consolidating the mixture, in particular by application of electromagnetic radiation, at positions in each layer, which correspond to the cross section of the object in this layer, wherein the positions are scanned in a radiation interaction zone of an energy beam bundle.

### Claim 15 (depends on 14)

Process according to claim 14, wherein the mixture prior to solidifying is heated to a temperature of 100° C. or more.

### Claim 16 (depends on 14)

Process according to claim 14, wherein the individual layers are applied at a thickness of 10 μm or more and/or 100 μm or less.

### Claim 17 (depends on 14)

Three-dimensional object prepared according to the process of claim 14.

### Claim 18 (depends on 5)

Three-dimensional object, which is constituted of a metal alloy as defined in claim 5 as a matrix comprising particles of a reinforcement material having a particle diameter of 1 μm to less than 30 μm, wherein the reinforcement material accounts for 0.1 to about 10.0 wt.-% of the three dimensional object.

### Claim 19 (depends on 17)

Three-dimensional object according to claim 17, having a relative density of 98% or more, wherein the relative density is defined as the ratio of the measured density and the theoretical density.

### Claim 20 (depends on 1)

Use of a powder mixture according to claim 1 for minimizing and/or suppressing crack formation of in a three-dimensional object, wherein the three-dimensional object is prepared in a process involving the step- and layerwise build-up of the three-dimensional object by additive manufacturing.

### Claim 21 (depends on 14)

Device for implementing a process according to claim 14, wherein the device comprises a laser sintering or laser melting device, a process chamber having an open container with a container wall, a support, which is inside the process chamber, wherein open container and support are moveable against each other in vertical direction, a storage container and a recoater, which is moveable in horizontal direction, and wherein the storage container is at least partially filled with a powder mixture.