# US 2022/0281000 A1 · Sintered material and method for producing sintered material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0281000 A1
- Document ID: US20220281000A1
- Status: Published application
- Kind: A1
- Application number: 17/637,809
- Filed: 2019-08-30
- Published: 2022-09-08
- Earliest claimed: 2019-08-30
- Assignees: Sumitomo Electric Industries, Ltd.; Sumitomo Electric Sintered Alloy, Ltd.
- Applicants: Sumitomo Electric Industries, Ltd.; Sumitomo Electric Sintered Alloy, Ltd.
- Inventors: Tomoyuki ISHIMINE; Shigeki EGASHIRA; Kazunari SHIMAUCHI; Takayuki TASHIRO
- Web page: https://patentgrep.com/patent/US20220281000A1

## CPC

- C22C 38/04: containing manganese
- B22F 1/00: Metallic powder; Treatment of metallic powder, e.g. to facilitate working or to improve properties
- B22F 3/1103: {with particular physical characteristics}
- B22F 5/08: of toothed articles, e.g. gear wheels; of cam discs
- C22C 33/02: by powder metallurgy
- C22C 33/0264: {the maximum content of each alloying element not exceeding 5%}
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- B22F 2301/35: Iron
- B22F 2998/10: Processes characterised by the sequence of their steps
- F16H 55/06: Use of materials; Use of treatments of toothed members or worms to affect their intrinsic material properties
- F16H 55/17: Toothed wheels (worm wheels F16H55/22; chain wheels F16H55/30)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- F16H: GEARING

## Abstract

A sintered material containing a parent phase composed of a metal and a plurality of pores present in the parent phase, wherein the pores in a cross section have an average cross-sectional area of 500 μm2 or less, and the sintered material has a relative density in the range of 93% to 99.5%.

## Claims

### Claim 1

A sintered material comprising:
a parent phase composed of an iron-based alloy; and
a plurality of pores present in the parent phase,
wherein the pores in a cross section have an average cross-sectional area of 300 μm2 or less,
the pores in a cross section have an average perimeter of 55 μm or less,
the pores in a cross section have other shapes than circular or elliptical shape, and
the sintered material has a relative density in the range of 93% to 99.5%.

### Claim at position 2

-9. (canceled)

### Claim 10 (depends on 1)

The sintered material according to claim 1, wherein the relative density is 96.5% or more.

### Claim 11 (depends on 1)

The sintered material according to claim 1, wherein the pores have an average maximum diameter in the range of 5 μm to 30 μm.

### Claim 12 (depends on 10)

The sintered material according to claim 10, wherein the pores have an average maximum diameter in the range of 5 μm to 30 μm.

### Claim 13 (depends on 1)

The sintered material according to claim 1, wherein
the iron-based alloy contains at least one element selected from the group consisting of C, Ni, Mo, Mn and B.

### Claim 14 (depends on 10)

The sintered material according to claim 10, wherein
the iron-based alloy contains at least one element selected from the group consisting of C, Ni, Mo, Mn and B.

### Claim 15 (depends on 11)

The sintered material according to claim 11, wherein
the iron-based alloy contains at least one element selected from the group consisting of C, Ni, Mo, Mn and B.

### Claim 16 (depends on 12)

The sintered material according to claim 12, wherein
the iron-based alloy contains at least one element selected from the group consisting of C, Ni, Mo, Mn and B.

### Claim 17

A method for producing a sintered material, comprising the steps of:
compressing a raw powder to produce a green compact with a relative density in the range of 93% to 99.5%; and
sintering the green compact and producing the sintered material,
wherein the raw powder contains a powder composed of an iron-based alloy with a Vickers hardness Hv in the range of 80 to 200,
the powder composed of the iron-based alloy has an average particle size in the range of 100 μm to 200 μm,
a sintering temperature in the step of sintering the green compact is below a liquid phase temperature and 1000° C. or more and less than 1200° C.,
the pores in a cross section of the sintered material have an average cross-sectional area of 300 μm2 or less,
the pores in a cross section of the sintered material have an average perimeter of 55 μm or less.

### Claim 18 (depends on 17)

The method for producing a sintered material according to claim 17, further comprising the step of cutting the green compact before sintering the green compact.

### Claim 19 (depends on 17)

The method for producing a sintered material according to claim 17, wherein
the iron-based alloy contains at least one element selected from the group consisting of 0.1% to 2.0% by mass Mo, 0.5% to 5.0% by mass Ni, and 0.1% to 5.0% by mass Mn.

### Claim 20 (depends on 18)

The method for producing a sintered material according to claim 18, wherein
the iron-based alloy contains at least one element selected from the group consisting of 0.1% to 2.0% by mass Mo, 0.5% to 5.0% by mass Ni, and 0.1% to 5.0% by mass Mn.