# US 2022/0280999 A1 · Method for preparing a metal powder for an additive manufacturing process and use of such powder

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0280999 A1
- Document ID: US20220280999A1
- Status: Published application
- Kind: A1
- Application number: 17/632,359
- Filed: 2020-07-31
- Published: 2022-09-08
- Earliest claimed: 2019-08-02
- Assignees: Hydromecanique Et Frottement
- Applicants: Hydromecanique Et Frottement
- Inventors: Sébastien BUCHER; Christophe Gérard PUPIER
- Web page: https://patentgrep.com/patent/US20220280999A1

## CPC

- B01J 13/04: by physical processes, e.g. drying, spraying
- B01J 13/22: Coating
- B22F 1/065: Spherical particles
- B22F 1/145: Chemical treatment, e.g. passivation or decarburisation
- B22F 1/17: Metallic particles coated with metal
- B22F 10/28: Powder bed fusion, e.g. selective laser melting [SLM] or electron beam melting [EBM]
- B22F 10/34: of powder characteristics, e.g. density, oxidation or flowability
- B33Y 40/10: Pre-treatment
- B33Y 70/00: Materials specially adapted for additive manufacturing
- B22F 2301/052: Aluminium
- B22F 2301/10: Copper
- B22F 2301/25: Noble metals, i.e. Ag Au, Ir, Os, Pd, Pt, Rh, Ru
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- Y02P 10/25: Process efficiency
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention relates to a method for preparing a metal powder intended for an additive manufacturing process, of the type that involves scanning a bed of powder by a near-infrared laser beam, characterized in that the method comprises: an initial step for selecting a powder, which has an optical reflectivity of higher than 70% for a wavelength ranging between 800 and 1500 nm; then a step for treating said powder, which is different from particle grafting, and which induces a physical and/or chemical surface modification of the grains of said powder, making it possible to lower its optical reflectivity, at the given wavelength. The invention also relates to the use of such a powder, the grains having, after treatment, a median grain size d50 of between 5 and 50 μm.

## Claims

### Claim 1

A method for preparing a metal powder intended for an additive manufacturing process, of the type that involves scanning a bed of powder by a near-infrared laser beam, characterized in that the method comprises:
an initial step for selecting a powder, that has an optical reflectivity of more than 70% for a wavelength ranging between 800 and 1500 nm; then
a step for treating said powder, which is different from grafting particles, and which induces a physical and/or chemical surface modification of the grains of said powder, making it possible to lower its optical reflectivity, at the given wavelength, the grains having, after treatment, a median grain size d50 of between 5 and 50 μm.

### Claim 2 (depends on 1)

The method according to claim 1, wherein in the initial step, the powder selected comprises at least support particles of a first material, having a first optical reflectivity at the given wavelength, and in that the treatment step comprises at least partial functionalization of the surface of the support particles of the first material, by diffusion, by germination-growth or by precipitation, without resulting in deposition of nanoparticles, by forming a surface layer of at least one second material having a second optical reflectivity, lower than the first optical reflectivity, thus lowering the optical reflectivity of the powder, at the given wavelength.

### Claim 3 (depends on 1)

The method according to claim 1, wherein in the initial step, the powder selected comprises at least particles of a first material, having a first optical reflectivity at the given wavelength, and in that the treatment step comprises physical and/or chemical etching causing an increase in the surface roughness of the particles, thus lowering the optical reflectivity of the powder, at the given wavelength.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the treatment step comprises functionalization, after which the powder consists of functionalized particles (10+20) each comprising a support particle of the first material and a surface layer consisting of at least a second material, then a second treatment comprising physical and/or chemical etching causing an increase in the surface roughness of the functionalized particles (10+20), thus lowering the optical reflectivity of the powder, at the given wavelength.

### Claim 5 (depends on 2)

The method according to claim 2, wherein that functionalization comprises diffusion of at least one second material selected from the families of metals, metalloids and heteroatoms.

### Claim 6 (depends on 2)

The method according to claim 2, wherein that functionalization comprises germination-growth of a deposit of at least one second material on the particles of the first material.

### Claim 7 (depends on 2)

The method according to claim 2, wherein that functionalization comprises precipitation of at least one second material, in the form of a compound ensuring the role of flux during the lasing operation.

### Claim 8 (depends on 2)

The method according to claim 2, wherein that functionalization does not modify the composition of the grains by more than 10% by mass.

### Claim 9 (depends on 2)

The method according to claim 2, wherein that the functionalization surface layer consisting of at least the second material has a maximum thickness of 1 μm on each grain.

### Claim 10 (depends on 1)

The method according to claim 1, wherein that treatment does not modify the composition of the grains by more than 10% by mass.

### Claim 11 (depends on 1)

The method according to claim 1, wherein that surface modification affects a maximum thickness of 1 μm of each grain.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the particles of the first material are chosen from the families of copper and its alloys, aluminum and its alloys, or precious metals and their alloys.

### Claim 13 (depends on 1)

The method according to claim 1, wherein after treatment, surface modification covers between 10 and 100% of the surface of each particle of the first material.

### Claim 14 (depends on 1)

A method of additive manufacturing comprising using metal powder obtained by the method according to claim 1.