# US 2022/0280998 A1 · Anti-fretting coating composition and coated components

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0280998 A1
- Document ID: US20220280998A1
- Status: Published application
- Kind: A1
- Application number: 17/473,281
- Filed: 2021-09-13
- Published: 2022-09-08
- Earliest claimed: 2021-03-03
- Assignees: General Electric Company
- Applicants: General Electric Company
- Inventors: Paul Mathew; Mohandas Nayak; Sathisha Chikkabikkodu Hanum; Monty Lee Shelton
- Web page: https://patentgrep.com/patent/US20220280998A1

## CPC

- C22C 32/0026: {Matrix based on Ni, Co, Cr or alloys thereof}
- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 1/09: {Mixtures of metallic powders}
- B22F 1/12: Metallic powder containing non-metallic particles (containing lubricating or binding agents or organic material B22F1/10)
- C23C 4/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas
- C23C 4/04: characterised by the coating material
- C23C 4/06: Metallic material
- C23C 4/11: Oxides
- C23C 4/134: Plasma spraying
- C23C 4/18: After-treatment
- C23C 24/04: Impact or kinetic deposition of particles
- C23C 24/08: by application of heat or pressure and heat (C23C24/04 takes precedence)
- C23C 28/04: only coatings of inorganic non-metallic material
- C23C 28/321: {with at least one metal alloy layer}
- C23C 28/345: {with at least one oxide layer}
- F01D 5/288: {Protective coatings for blades}
- B22F 7/06: of composite workpieces or articles from parts, e.g. to form tipped tools {(B22F7/002 takes precedence)}
- B22F 2301/15: Nickel or cobalt
- B22F 2301/20: Refractory metals
- B22F 2302/253: Aluminum oxide (Al2O3)
- F05D 2230/90: Coating; Surface treatment
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

An anti-fretting coating composition that is operationally stable at temperatures of 800° F. to 2650° F. is provided. The anti-fretting coating composition primarily includes cobalt and aluminum oxide and may also include other modifying phases that enhance the overall tribological performance. A component coated with the anti-fretting coating composition is also provided. The component includes a substrate having a first contact surface shaped to cooperate with a second contact surface of an abutting member in a manner which can develop wear between the first contact surface and the second contact surface. The first contact surface includes an anti-fretting coating thereon formed from the disclosed anti-fretting coating composition.

## Claims

### Claim 1

An anti-fretting coating composition, comprising:
from about 5 weight % to about 80 weight % of a cobalt-containing powder; and
from about 1 weight % to about 80 weight % of an aluminum-oxide powder.

### Claim 2 (depends on 1)

The anti-fretting coating composition of claim 1, further comprising from about 1 weight % to about 20 weight % of a tantalum-containing powder.

### Claim 3 (depends on 1)

The anti-fretting coating composition of claim 1, comprising a viscoelasticity-modifying composition comprising calcium oxide, aluminum oxide, and silicon dioxide.

### Claim 4 (depends on 3)

The anti-fretting coating composition of claim 3, wherein the viscoelasticity-modifying composition comprises from about 25 weight % to about 50 weight % calcium oxide, from about 10 weight % to about 40 weight % of aluminum oxide, and from about 20 weight % to about 65 weight % of silicon dioxide.

### Claim 5 (depends on 3)

The anti-fretting coating composition of claim 3, comprising from about 5 weight % to about 20 weight % of the viscoelasticity-modifying composition.

### Claim 6 (depends on 3)

The anti-fretting coating composition of claim 3, wherein the viscoelasticity-modifying composition further comprises one or more additive, the one or more additives including iron oxide, titanium dioxide, nickel oxide, boron oxide, or a combination thereof, wherein the weight % of these additives does not exceed 10 wt. % of the total weight of the viscoelasticity-modifying composition.

### Claim 7 (depends on 1)

The anti-fretting coating composition of claim 1, comprising a median particle size of from about from about 0.025 μm to about 30 μm.

### Claim 8 (depends on 1)

The anti-fretting coating composition of claim 1, wherein the anti-fretting coating composition is applied to a substrate to form an anti-fretting coating that is operationally stable at temperatures of from about 800° F. to about 2650° F.

### Claim 9

A component, comprising:
a substrate having a first contact surface shaped to cooperate with a second contact surface of an abutting member in a manner which can develop wear between the first contact surface and the second contact surface, wherein one or both of the first contact surface and the second contact surface have an anti-fretting coating thereon formed from an anti-fretting coating composition, the anti-fretting coating composition comprising from about 5 weight % to about 80 weight % of a cobalt-containing powder and from about 1 weight % to about 80 weight % of an aluminum-oxide powder.

### Claim 10 (depends on 9)

The component of claim 9, wherein the anti-fretting coating composition comprises from about 50 weight % to about 80 weight % of a cobalt-containing powder and from about 20 weight % to about 40 weight % of an aluminum-oxide powder.

### Claim 11 (depends on 9)

The component of claim 9, wherein the anti-fretting coating composition further comprises from about 1 weight % to about 20 weight % of a tantalum-containing powder.

### Claim 12 (depends on 9)

The component of claim 9, wherein the anti-fretting coating composition further comprises silicon dioxide, calcium oxide, iron oxide, titanium dioxide, or combinations thereof.

### Claim 13 (depends on 9)

The component of claim 9, wherein the substrate comprises a nickel-based superalloy, a cobalt-based superalloy, or combinations thereof.

### Claim 14 (depends on 9)

The component of claim 9, wherein the substrate comprises a non-metallic substrate.

### Claim 15 (depends on 9)

The component of claim 9, wherein the anti-fretting coating composition is applied to the substrate via a plasma spray process, powder spray process, slurry spray process, and combinations thereof

### Claim 16 (depends on 9)

The component of claim 9, wherein the anti-fretting coating has a thickness of from about 0.5 mils to about 20 mils.

### Claim 17 (depends on 9)

The component of claim 9, wherein one or more additional coatings are disposed on the substrate and are sandwiched between the substrate and the anti-fretting coating.

### Claim 18 (depends on 9)

The component of claim 9, wherein the component is suitable for use in an oxidizing atmosphere at a temperature of about 800° F. to about 2650° F.

### Claim 19 (depends on 9)

The component of claim 9, wherein the component is a gas turbine engine component.

### Claim 20 (depends on 19)

The component of claim 19, wherein the component is at least one of a nozzle, shroud, shroud hanger, pressure balance seal, low pressure turbine blade, high pressure turbine blade, and combustor component.