# US 2022/0280920 A1 · Nitrogen-phosphorus-modified granular carbon-supported bimetallic catalyst, preparation method therefor and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0280920 A1
- Document ID: US20220280920A1
- Status: Published application
- Kind: A1
- Application number: 17/637,922
- Filed: 2020-11-27
- Published: 2022-09-08
- Earliest claimed: 2019-11-29
- Assignees: Zhejiang Lantian Environmental Protection Hi-Tech Co., Ltd.; Zhejiang Research Institute of Chemical Industry Co., Ltd; Sinochem Lantian Co., Ltd.
- Applicants: Zhejiang Lantian Environmental Protection Hi-Tech Co., Ltd.; Zhejiang Research Institute of Chemical Industry Co., Ltd.; Sinochem Lantian Co., Ltd.
- Inventors: Wucan LIU; Ling LI; Chaofeng MA; Nengfu SHI; Jiamin JIN; Xiaonian LI; Chunshan LU; Juanjuan NIE
- Web page: https://patentgrep.com/patent/US20220280920A1

## CPC

- B01J 23/40: of the platinum group metals
- B01J 37/345: {of ultraviolet wave energy}
- B01J 21/18: Carbon
- B01J 23/06: of zinc, cadmium or mercury
- B01J 23/14: of germanium, tin or lead
- B01J 23/60: with zinc, cadmium or mercury
- B01J 23/626: {with tin}
- B01J 23/72: Copper
- B01J 23/8926: {Copper and noble metals}
- B01J 35/393: {Metal or metal oxide crystallite size}
- B01J 35/617: {500-1000 m2/g}
- B01J 35/618: {more than 1000 m2/g}
- B01J 35/647: {2-50 nm}
- B01J 35/66: Pore distribution
- B01J 37/0203: {the impregnation liquid containing organic compounds}
- B01J 37/0207: {Pretreatment of the support}
- B01J 37/024: {Multiple impregnation or coating}
- B01J 37/084: {Decomposition of carbon-containing compounds into carbon}
- B01J 37/18: with gases containing free hydrogen
- C07C 17/23: by dehalogenation
- C07C 17/25: by splitting-off hydrogen halides from halogenated hydrocarbons
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

Provided are a nitrogen-phosphorus-modified granular carbon-supported bimetallic catalyst, a preparation method thereof and the use thereof. The catalyst comprises a nitrogen-phosphorus-modified carbon carrier and metal particles supported on the carbon carrier. The metal particles include first metal elementary substance particles, second metal elementary substance particles and bimetallic alloy phase particles. The percentage of the bimetallic alloy phase particles in the metal particles is ≥80%, and at least 90% of the alloy phase particles have a size of 1 nm to 20 nm. The catalyst has advantages such as a high proportion of alloy phase particles, a uniform particle size distribution, a high metal utilization rate, low costs, high stability and a high catalytic activity.

## Claims

### Claim 1

A nitrogen-phosphorus-modified granular carbon-supported bimetallic catalyst, wherein the catalyst comprises a nitrogen-phosphorus-modified carbon carrier and metal particles supported on the carbon carrier, and the metal particles include first metal elementary substance particles, second metal elementary substance particles and bimetallic alloy phase particles, the percentage of the bimetallic alloy phase particles in the metal particles is ≥80%, and at least 90% of the alloy phase particles have a size of 1 nm to 20 nm.

### Claim 2 (depends on 1)

The granular carbon-supported bimetallic catalyst according to claim 1, wherein the percentage of the bimetallic alloy phase particles in the metal particles is 85-95%, and at least 95% of the alloy phase particles have a size of 2 nm to 10 nm.

### Claim 3 (depends on 1)

The granular carbon-supported bimetallic catalyst according to claim 1, wherein the nitrogen content in the carbon carrier is 0.5-10 wt %, and the phosphorus content in the carbon carrier is 0.1-5.0 wt %.

### Claim 4 (depends on 1)

The granular carbon-supported bimetallic catalyst according to claim 1, wherein the carbon carrier is selected from coconut shell or wooden activated carbon, the specific surface area of the carbon carrier is ≥800 m2/g, the metal ash content is ≤3.0 wt %, and the mesopore ratio is ≥50%.

### Claim 5 (depends on 4)

The granular carbon-supported bimetallic catalyst according to claim 4, wherein the carbon carrier is a cylindrical particle with a particle diameter of 0.1-0.5 cm and a length of 0.1-5 cm.

### Claim 6 (depends on 1)

The granular carbon-supported bimetallic catalyst according to claim 1, wherein a first metal is selected from at least one of palladium, platinum or ruthenium, with a loading content of 0.01-4.0%; a second metal is selected from copper, zinc and/or tin, with a loading content of 0.01-10.0%; and the mass ratio of the first metal to the second metal is (0.01-5):1.

### Claim 7 (depends on 1)

A method for preparing the granular carbon-supported bimetallic catalyst according to claim 1, wherein the granular carbon-supported bimetallic catalyst is prepared by the following steps:
A1. preparing nitrogen-phosphorus co-doped carbon particles;
A2. loading the nitrogen-phosphorus co-doped carbon particles onto the carbon carrier;
A3. loading the second metal onto the carbon carrier by using nitrogen-phosphorus co-doped carbon particles as a first anchor point under the irradiation with an ultraviolet lamp;
A4. loading the first metal on the carbon carrier.

### Claim 8 (depends on 7)

The method for preparing the granular carbon-supported bimetallic catalyst according to claim 7, wherein in the step A3, the irradiation is performed with a 200-500 w ultraviolet lamp once to three times, 3-10 min each time, preferably, the irradiation with an ultraviolet lamp is performed twice, with wavelengths of 280-320 nm and 200-280 nm respectively.

### Claim 9 (depends on 7)

The method for preparing the granular carbon-supported bimetallic catalyst according to claim 7, wherein the carbon particles have a size of 1 nm to 20 nm.

### Claim 10 (depends on 7)

The method for preparing the granular carbon-supported bimetallic catalyst according to claim 7, wherein the step A3 further comprises:
pyrolyzing carbon particles at a temperature of 120-300° C. in a hydrogen atmosphere after the second metal is loaded onto the carbon carrier, the binding sites of nitrogen and phosphorus elements, the carbon carrier and the second metal form a second anchor point for loading the first metal onto the carbon carrier.

### Claim 11 (depends on 1)

An application of the granular carbon-supported bimetallic catalyst of claim 1, wherein the granular carbon-supported bimetallic catalyst is used for hydrodechlorination of C1-C5 chlorofluoro alkanes in a fixed bed, the conversion rate of C1-C5 chlorofluoro alkanes is at least about 98% and the product selectivity is at least about 95%.

### Claim 12 (depends on 11)

The application of the granular carbon-supported bimetallic catalyst according to claim 11, wherein the granular carbon-supported bimetallic catalyst is used for preparing difluoromethane from difluorodichloromethane, preparing chlorotrifluoroethylene from trichlorotrifluoroethane, preparing 1,1,1,4,4,4-hexafluoro-2-butene from 2,3-dichloro-1,1,1,4,4,4-hexafluoro-2-butene, preparing pentafluoroethane from chloropentafluoroethane or preparing trichloromethane from carbon tetrachloride.

### Claim 13 (depends on 1)

A method for preparing chlorotrifluoroethylene, wherein trifluorotrichloroethane is used as a raw material, and the reaction is carried out in the presence of the granular carbon-supported bimetallic catalyst of claim 1, the conversion rate of trichlorotrifluoroethane is at least about 98%, the selectivity of chlorotrifluoroethylene is at least about 95%, and the product contains at least less than about 1% of chlorotrifluoroethane.

### Claim 14 (depends on 13)

The method for preparing chlorotrifluoroethylene according to claim 13, wherein the method comprises the following steps:
B1. feeding the granular carbon-supported bimetallic catalyst into a fixed-bed reactor, introducing a mixture of ammonia and chlorofluoroethane, wherein the molar ratio of ammonia to chlorofluoroethane is (50-100):1, the air speed is 10,000-50,000 h−1, heating to 300-400° C. at a rate of 0.5-3.5° C./min, keeping for 1-5 hours and then cooling to the reaction temperature;
B2. introducing a mixture composed of hydrogen and trichlorotrifluoroethane, wherein the molar ratio of H2 to trichlorotrifluoroethane is (1.5-4.0):1, the air speed is 120-500 h−1 and the reaction temperature is 150-300° C.

### Claim 15 (depends on 1)

A method for preparing 1,1,1,4,4,4-hexafluoro-2-butene, wherein 2,3-dichloro-1,1,1,4,4,4-hexafluoro-2-butene is used as a raw material, and the reaction is carried out in the presence of the granular carbon-supported bimetallic catalyst of claim 1, the conversion rate of 2,3-dichloro-1,1,1,4,4,4-hexafluoro-2-butene is at least about 98%, and the selectivity of 1,1,1,4,4,4-hexafluoro-2-butene is at least about 95%, and the product contains at least less than about 1% of 2-chloro-1,1,1,4,4,4-hexafluoro-2-butene.

### Claim 16 (depends on 15)

The method for preparing 1,1,1,4,4,4-hexafluoro-2-butene according to claim 15, comprising:
C1. feeding the granular carbon-supported bimetallic catalyst into a fixed-bed reactor, introducing a mixture of hydrogen and dichlorodifluoroethane, wherein the molar ratio of H2 to dichlorodifluoroethane is (50-100):1, the air speed is 10,000-50,000 h−1, heating to 300-400° C. at a rate of 0.5-3.5° C./min, keeping for 1-5 hours and then cooling to the reaction temperature;
C2. introducing a mixture composed of hydrogen and 2,3-dichloro-1,1,1,4,4,4-hexafluoro-2-butene, wherein the molar ratio of H2 to 2,3-dichloro-1,1,1,4,4,4-hexafluoro-2-butene is (1.5-4.0):1, the air speed is 120-600 h−1 and the reaction temperature is 150-350° C.