# US 2022/0280910 A1 · Modified clay, its preparation and use

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0280910 A1
- Document ID: US20220280910A1
- Status: Published application
- Kind: A1
- Application number: 17/686,394
- Filed: 2022-03-03
- Published: 2022-09-08
- Earliest claimed: 2021-03-05
- Applicants: Mindbody Networks Inc.
- Inventors: Hossein KAZEMIAN; Robert C.W. CHEYNE
- Web page: https://patentgrep.com/patent/US20220280910A1

## CPC

- B01J 20/12: Naturally occurring clays or bleaching earth
- B01J 20/28004: {Sorbent size or size distribution, e.g. particle size}
- B01J 20/3085: {Chemical treatments not covered by groups B01J20/3007 - B01J20/3078}
- C02F 1/281: {using inorganic sorbents}
- B01J 20/3028: {Granulating, agglomerating or aggregating}
- B01J 20/3078: {Thermal treatment, e.g. calcining or pyrolizing}
- C02F 1/288: {using composite sorbents, e.g. coated, impregnated, multi-layered}
- C02F 2101/105: {Phosphorus compounds}
- C02F 2101/38: containing nitrogen
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)

## Abstract

The specification relates to a clay having kaolinite from 20-40 wt. %; illite from 15-30 wt. %; pigeonite from 5-15 wt. %; and quartz up to a maximum of 40 wt. %. The clay is for use as an agent for reducing concentration of phosphorous in a fluid. Also disclosed is a process for preparation of a modified clay, and a method of treatment of a fluid using the clay or modified clay.

## Claims

### Claim 1

A clay, the clay comprising:
kaolinite from 20-40 wt. %;
illite from 15-30 wt. %;
pigeonite from 5-15 wt. %; and
quartz up to a maximum of 40 wt. %,
wherein the clay is for use as an agent for reducing concentration of phosphorous in a fluid.

### Claim 2 (depends on 1)

The clay of claim 1, further comprising:
nontronite from 1-5 wt. %.

### Claim 3 (depends on 1)

The clay of claim 1, further comprising:
nontronite from 1-5 wt. %, and dolomite from 1-8 wt. %.

### Claim 4 (depends on 1)

The clay of claim 1, further comprising:
aluminum, calcium, iron potassium, magnesium or sulfur up to a maximum of 15 wt. %.

### Claim 5 (depends on 1)

The clay of claim 1, wherein the phosphorous is an inorganic ionic phosphorous species.

### Claim 6 (depends on 5)

The clay of claim 5, wherein the inorganic ionic phosphorous species is a phosphate ion.

### Claim 7 (depends on 1)

The clay of claim 1, wherein the phosphorous is glyphosate.

### Claim 8 (depends on 1)

The clay of claim 1, wherein the fluid is water.

### Claim 9 (depends on 1)

The clay of claim 1, wherein the clay is a zirconium modified clay or an iron modified clay.

### Claim 10 (depends on 1)

The clay of claim 1, wherein the clay has a Dx (90) of from 100-150 μm.

### Claim 11 (depends on 1)

The clay of claim 1, wherein the clay is heat treated at a temperature between 400° C. and 800° C. over a period between 30 minutes to 48 hour.

### Claim 12 (depends on 11)

The clay of claim 11, wherein the clay is granulated prior to heat treatment.

### Claim 13 (depends on 11)

The clay of claim 11, wherein the clay is granulated after heat treatment.

### Claim 14

A method of treatment for reducing the concentration of phosphorous in a fluid, the method comprising:
contacting the fluid with a clay, or modified clay, comprising:
kaolinite from 20-40 wt. %;
illite from 15-30 wt. %;
pigeonite from 5-15 wt. %; and
quartz up to a maximum of 40 wt. %.

### Claim 15

A method of manufacture of a modified clay, the modified clay having kaolinite from 20-40 wt. %; illite from 15-30 wt. %; pigeonite from 5-15 wt. %; and quartz up to a maximum of 40 wt. %, the method comprising:
calcinating clay at a temperature of from 400 to 700° C. to form the modified clay.

### Claim 16 (depends on 15)

The method of claim 15, comprising granulating the modified clay.