# US 2022/0280694 A1 · Detergent-free decellularized extracellular matrix preparation methods and bioinks for 3d printing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0280694 A1
- Document ID: US20220280694A1
- Status: Published application
- Kind: A1
- Application number: 17/628,429
- Filed: 2020-07-21
- Published: 2022-09-08
- Earliest claimed: 2019-07-22
- Assignees: Polbionica Sp. z o. o.
- Applicants: Polbionica Sp. z o. o.
- Inventors: Michal WSZOLA; Marta KLAK; Andrzej BERMAN; Katarzyna KOSOWSKA; Tomasz BRYNIARSKI; Tomasz DOBRZANSKI; Grzegorz TYMICKI; Magdalena GOMÓLKA; Patrycja KOWALSKA; Piotr CYWONIUK; Pawel TUROWSKI; Igor ZAMORA; Ewa OLENDER; Radoslaw OLKOWSKI; Artur KAMINSKI
- Web page: https://patentgrep.com/patent/US20220280694A1

## CPC

- A61L 27/3687: {characterised by the use of chemical agents in the treatment, e.g. specific enzymes, detergents, capping agents, crosslinkers, anticalcification agents}
- A61L 27/26: Mixtures of macromolecular compounds
- A61L 27/3633: {Extracellular matrix [ECM]}
- A61L 27/3683: {subjected to a specific treatment prior to implantation, e.g. decellularising, demineralising, grinding, cellular disruption/non-collagenous protein removal, anti-calcification, crosslinking, supercritical fluid extraction, enzyme treatment}
- A61L 27/3691: {characterised by physical conditions of the treatment, e.g. applying a compressive force to the composition, pressure cycles, ultrasonic/sonication or microwave treatment, lyophilisation}
- A61L 27/3808: {Endothelial cells}
- A61L 27/54: Biologically active materials, e.g. therapeutic substances {(A61L27/227 takes precedence)}
- B33Y 10/00: Processes of additive manufacturing
- B33Y 40/20: Post-treatment, e.g. curing, coating or polishing
- B33Y 70/00: Materials specially adapted for additive manufacturing
- B33Y 80/00: Products made by additive manufacturing
- C09D 4/06: {Organic non-macromolecular compounds having at least one polymerisable carbon-to-carbon unsaturated bond} in combination with a macromolecular compound other than an unsaturated polymer of groups C09D159/00 - C09D187/00
- C09D 7/63: organic
- C09D 7/65: macromolecular (C09D7/41-C09D7/48 take precedence)
- C09D 133/14: of esters containing halogen, nitrogen, sulfur or oxygen atoms in addition to the carboxy oxygen
- A61L 2300/414: Growth factors
- A61L 2300/426: Immunomodulating agents, i.e. cytokines, interleukins, interferons
- A61L 2300/428: Vitamins, e.g. tocopherol, riboflavin
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

A detergent-free decellularized ECM preparation method, a detergent-free decellularized ECM in a powder form and in a liquid form, a method of preparation of a primary bioink, the primary bioink, a method of preparation of a vascular bioink, the vascular bioink, a three dimensional structure including the primary bioink and/or the vascular bioink and a method of preparation of the three-dimensional structure.

## Claims

### Claim 1

A detergent-free decellularized extracellular matrix (dECM) preparation method comprising the following steps:
mechanical fragmentation, preferably by mechanical extrusion, of an organ of animal origin selected form pancreas, liver, kidneys, heart, skin, lungs, large intestine, small intestine, blood arteries and veins, adipose tissue and placenta, wherein the organ is separate from the body of the animal,
incubation of the fragmented organ in a buffered detergent solution, preferably comprising 1×PBS, whereby the buffered detergent solution comprises 0.5%-1.5%, preferably 1% (v/v), octoxynol-9, wherein the detergent solution is supplemented with an antimicrobial agent, preferably streptomycin, preferably at a concentration of 0.01% (w/v), and the incubation is performed at a temperature below room temperature, preferably at 4° C., for at least 72 h with agitation, wherein the fragmented organ is transferred to a fresh detergent solution every 4 to 12 hours;
incubation of the fragmented organ in a first buffered washing solution, preferably comprising 1×PBS, whereby the first buffered washing solution comprises an antimicrobial agent, preferably streptomycin, preferably at a concentration of 0.01% (w/v), for at least 72 h at a temperature below room temperature, preferably at 4° C. with agitation, wherein the fragmented organ is transferred to a fresh washing solution every 4 to 12 hours;
incubation of the fragmented organ in a deoxyribonuclease solution comprising DNAse, preferably at a concentration of 0.0001 to 0,0003% (w/v), most preferably 0.0002% (w/v), preferably for at least 8 hours at a temperature suitable for the DNAse performance;
incubation of the fragmented organ in a second buffered washing solution, preferably comprising 1×PBS, whereby the second buffered washing solution comprises an antimicrobial agent, preferably streptomycin, preferably at a concentration of 0.01% (w/v), for at least 72 h at a temperature below room temperature, preferably at 4° C. with agitation, wherein the fragmented organ is transferred to a fresh washing solution every 4 to 12 hours;
freezing of the fragmented organ and crushing the frozen fragmented organ into fragments
freeze-drying of the frozen fragmented organ, preferably at −32° C., preferably under a pressure of 0.31 mbar (31 Pa);
optional final drying for 5 to 15 minutes at 0.0010 mbar (0.1 Pa) and −76° C.;
grinding the crushed and dried product into 25-500 μm dECM powder; and
optional sterilization of the product, preferably by radiation and/or ethylene oxide.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the grinding step is followed by a step of checking the amount of octoxynol-9 in dECM powder, wherein preferably before dECM powder is checked for the presence of octoxynol-9, it is treated with collagenase, preferably at a concentration of 43,953 PZ/g dECM.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the grinding step is followed by the following steps:
dissolving of the dECM powder in hydrochloric acid solution, preferably 0.01 M, supplemented with 0-10 mg/ml of pepsin;
mixing for 48-72 h, preferably for 72 h, at room temperature;
neutralizing on ice, preferably using 0.1 M sodium base and PBS solution.

### Claim 4 (depends on 1)

A detergent-free decellularized ECM in a powder form, obtainable by the method according to claim 1.

### Claim 5 (depends on 3)

A detergent-free decellularized ECM in form of a solution, obtainable by the method according to claim 3.

### Claim 6

A method of preparation of a primary bioink comprising the following steps:
preparation of a paste comprising 5-50% (w/v), preferably 15-25% (w/v), of a dECM powder, and 1-10% (w/v), preferably 8-10% (w/v), of a dECM solution by mixing;
incubation of the paste at a temperature of 7-10° C. for at least 24 hours;
addition of 1.46-7.32% (w/v) methacrylated gelatin, 0.15-1.10% (w/v) methacrylated hyaluronic acid and 5 to 10% (w/v) glycerol, and a photoinitiator, preferably 0.03-0.17% (w/v) lithium phenyl-2,4,6-trimethylbenzoylphosphinate, followed by gentle mixing.

### Claim 7

A primary bioink comprising a dECM paste and 1.46-7.32% (w/v) methacrylated gelatin, 0.15-1.10% (w/v) methacrylated hyaluronic acid and 5 to 10% (w/v) glycerol, and a photoinitiator, preferably 0.03-0.17% (w/v) lithium phenyl-2,4,6-trimethylbenzoylphosphinate, wherein the dECM paste comprises 5-50% (w/v), preferably 15-25% (w/v), of a dECM powder, and 1-10% (w/v), preferably 8-10% (w/v), of a dECM solution and wherein the viscosity of the primary bioink is at least 5 Pa·s, measured in a cone-plate system, at a constant shear rate of 21/s and a temperature of 37° C.

### Claim 8 (depends on 7)

The primary bioink according to claim 7, comprising at least one additive selected from: hyaluronic acid at a concentration of 0.001 to 0.100 mg/mL of the primary bioink, preferably, 0.007 mg/mL, laminin at a concentration of 0.005 to 0.100 mg/mL of the primary bioink, preferably, 0.084 mg/mL, collagen I at a concentration of 0.001 to 0.100 mg/mL of the primary bioink, preferably 0.041 mg/mL, collagen IV at a concentration of 0.005 to 0.175 mg/mL of the primary bioink, preferably, 0.122 mg/mL, fibronectin at a concentration of 3 to 300 μg/mL, preferably 100 μg/mL, human fibrinogen at a concentration of 10 to 100 mg/mL of the primary bioink, aprotinin at a concentration of 1 to 2 EPU/mL of the primary bioink, polysorbate at a concentration of 0.05 to 2 mg/mL of the primary bioink, human thrombin at a concentration of 5 to 55 mg/mL of the primary bioink, calcium chloride at a concentration of 20 to 60 mM/mL of the primary bioink; proangiogenic vitamins: vitamin A at a concentration of 1 nM-500 μM, preferably 100 μM, vitamin B1 at a concentration of 50-100 μM, preferably 100 μM, vitamin B3 at a concentration of 1 to 10 μM, preferably 10 μM, vitamin B12 at a concentration of 10 to 100 mg/mL of the primary bioink, vitamin D3 at a concentration of 0.1 to 10 nM, preferably 10 nM, growth factors supporting angiogenesis: VEGF at a concentration of 10 to 30 ng/mL of the primary bioink, preferably 30 ng/mL, FGF at a concentration of 10 to 20 ng/mL of the primary bioink, preferably 20 ng/mL, TGF-β at a concentration of 1 to 10 ng/mL of the primary bioink, preferably 20 ng/mL, interleukin (IL)-8 at a concentration of 0 to 100 ng/mL of the primary bioink, preferably 10 ng/mL, IL-17A at a concentration of 20 to 50 ng/mL of the primary bioink, preferably 20 ng/mL.

### Claim 9 (depends on 7)

The primary bioink according to claim 7, comprising one or more animal- or human-derived additives selected from endothelial cells at a density of 0.1-10×105/mL of the primary bioink, primary microvascular endothelial cells at a concentration of 0.1 to 10×105/mL of the primary bioink, animal- or human-derived α cells at a concentration of 3 to 9×106/mL of the bioink, animal- or human-derived β cells at a concentration of 1.1 to 3.4×107/mL of the bioink, animal- or human-derived pancreatic islets, preferably in the amount of 20,000 iEq/mL of the primary bioink.

### Claim 10 (depends on 1)

A method of preparation of a vascular bioink comprising the steps of:
a) optional preparation of a solution of microbiological gelatin supplemented with CMC comprising preparation of a 1-2% (w/v) solution of microbiological gelatin in a buffer solution, preferably PBS, by suspending microbiological gelatin in the buffer solution with agitation at a temperature between 50 and 65° C., preferably at 60° C., addition of a 2-5% (v/v) carboxymethyl cellulose (CMC) aqueous solution to obtain a final concentration of 0.2-1% (v/v) of CMC in the vascular bioink and cooling the solution to a temperature equal or below 40° C.;
b) preparation of a 5-10% (w/v) dECM solution by addition of dECM powder obtainable according to claim 1, preferably sterilized by radiation, to (i) the solution of microbiological gelatin supplemented with CMC obtained in step a) or (ii) a buffer solution or (iii) a solution of cell medium with gentle agitation;
c) sonication of the obtained solution at a temperature not exceeding 37° C. for 0.5-2.0 hours;
d) optional addition of at least one animal- or human-derived additive selected from: fibronectin at a concentration of 3 to 300 μg/mL, preferably 100 μg/mL, VEGF at a concentration of 10 to 30 ng/mL, preferably 30 ng/mL, FGF at a concentration of 10 to 20 ng/mL, preferably 20 ng/mL, PGE2 at a concentration between 100 and 300 nM, preferably 100 nM, endothelial cells at a density between 0.1 and 10×107 cells/mL of the bioink, fibroblasts at a density of between 0.1 and 10×106 cells/mL of the bioink.

### Claim 11 (depends on 1)

A method of preparation of a vascular bioink comprising the steps of:
a) optional preparation of a solution of microbiological gelatin supplemented with CMC comprising preparation of a 1-2% (w/v) solution of microbiological gelatin in a buffer solution, preferably PBS, by suspending microbiological gelatin in the buffer solution with agitation at a temperature between 50 and 65° C., preferably at 60° C., addition of a 2-5% (v/v) carboxymethyl cellulose (CMC) aqueous solution to obtain a final concentration of 0.2-1% (v/v) of CMC in the vascular bioink and cooling the solution to a temperature equal or below 40° C.;
b) preparation of a 5-10% (w/v) dECM solution by addition of dECM powder obtainable according to claim 1, preferably sterilized by radiation, to (i) the solution of microbiological gelatin supplemented with CMC obtained in step a) or (ii) a buffer solution or (iii) a solution of cell medium with gentle agitation;
c) boiling the mixture at 100° C. for 15-30 minutes;
d) optional addition of at least one animal- or human-derived additive selected from: fibronectin at a concentration of 3 to 300 μg/mL, preferably 100 μg/mL, VEGF at a concentration of 10 to 30 ng/mL, preferably 30 ng/mL, FGF at a concentration of 10 to 20 ng/mL, preferably 20 ng/mL, PGE2 at a concentration between 100 and 300 nM, preferably 100 nM, endothelial cells at a density between 0.1 and 10×107 cells/mL of the bioink, fibroblasts at a density of between 0.1 and 10×106 cells/mL of the bioink.

### Claim 12 (depends on 5)

A vascular bioink comprising the sonicated or boiled dECM solution according to claim 5 at a concentration of 2-10% (w/v), preferably supplemented with microbiological gelatin at a concentration of 1 to 5% (w/v) and/or CMC at a concentration of 0.2 to 2% (v/v).

### Claim 13 (depends on 12)

The vascular bioink according to claim 12, comprising at least one animal- or human-derived additive selected from: fibronectin at a concentration of 3 to 300 μg/mL, preferably 100 μg/mL, VEGF at a concentration of 10 to 30 ng/mL, preferably 30 ng/mL, FGF at a concentration of 10 to 20 ng/mL, preferably 20 ng/mL, PGE2 at a concentration between 100 and 300 nM, preferably 100 nM, endothelial cells at a density between 0.1 and 10×107 cells/mL of the vascular bioink, fibroblasts at a density of between 0.1 and 10×106 cells/mL of the vascular bioink.

### Claim 14 (depends on 12)

A three-dimensional structure comprising at least three adjacent bioink layers, wherein a layer of a vascular bioink according to claim 12 is arranged between two layers of a primary bioink.

### Claim 15 (depends on 7)

A method of preparation of a three-dimensional structure, wherein a primary bioink according to claim 7 and a vascular bioink are deposited layer by layer in a 3D-bioprinting process at a printing speed from 5 to 50 mm/s, pressure from 4 to 300 kPa and temperature from 4 to 37° C. and wherein during or after deposition the primary bioink is exposed to UV light and/or visible light, preferably of the wavelength from 365 to 405 nm, more preferably at 405 nm, for at least 5 seconds.