# US 2022/0280692 A1 · Surface hardening for a dental implant

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0280692 A1
- Document ID: US20220280692A1
- Status: Published application
- Kind: A1
- Application number: 17/631,851
- Filed: 2020-08-21
- Published: 2022-09-08
- Earliest claimed: 2019-08-23
- Applicants: Elos Medtech Pinol A/S
- Inventors: Thomas Lundin CHRISTIANSEN; Morten Stendahl JELLESEN; Marcel A.J. SOMERS; Andreas Frederik Kielsholm KÖRKEL
- Web page: https://patentgrep.com/patent/US20220280692A1

## CPC

- A61L 27/30: Inorganic materials
- C23C 8/16: using oxygen-containing compounds, e.g. water, carbon dioxide
- C23C 8/34: more than one element being applied in more than one step
- C23C 28/042: {including a refractory ceramic layer, e.g. refractory metal oxides, ZrO2, rare earth oxides}
- A61L 2400/18: Modification of implant surfaces in order to improve biocompatibility, cell growth, fixation of biomolecules, e.g. plasma treatment
- A61L 2430/12: for dental implants or prostheses
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

The present invention relates to a Group IV metal or alloy component having a protective oxide surface layer, the Group IV metal or alloy component having a core hardness, a diffusion zone having oxygen in solid solution in the range of a level providing a hardness of 120% of the hardness of the material core to the saturation level of the Group IV metal or alloy, and a Group IV metal oxide layer at the surface of the component, the diffusion zone being between the Group IV metal oxide layer and the material core. In another aspect, the invention relates to a method of producing a protective oxide surface layer on a Group IV metal or alloy comprising: providing a workpiece of a Group IV metal or alloy, oxidising the Group IV metal or alloy in a first and a second oxidation step.

## Claims

### Claim 1

A Group IV metal or alloy component having a protective oxide surface layer, the Group IV metal or alloy component comprising a material core having a core hardness, a diffusion zone having oxygen in solid solution in the range of a level providing a hardness of 120% of the hardness of the material core to the saturation level of the Group IV metal or alloy, and a Group IV metal oxide layer at the surface of the component, the diffusion zone being between the Group IV metal oxide layer and the material core,
wherein the Group IV metal oxide layer has a thickness in the range of 5 μm to 100 μm, a carbon content and a cross-sectional hardness of at least 650 HV0.005.

### Claim 2 (depends on 1)

The Group IV metal or alloy component according to claim 1, wherein the diffusion zone contains carbon in solid solution at a level above a minimum carbon content of the Group IV metal oxide layer.

### Claim 3 (depends on 1)

The Group IV metal or alloy component according to claim 1, wherein the Group IV metal oxide layer contains nitrogen.

### Claim 4 (depends on 1)

The Group IV metal or alloy component according to claim 1, wherein the component has a volumetric loss of up to 5% of the volumetric loss of a component not having the Group IV metal oxide layer when analysed after sliding wear testing under identical conditions.

### Claim 5 (depends on 1)

The Group IV metal or alloy component according to claim 1, wherein the Group IV metal or alloy is selected from the list consisting of titanium, a titanium alloy, zirconium, and a zirconium alloy.

### Claim 6 (depends on 1)

The Group IV metal or alloy component according to claim 1, wherein the Group IV metal or alloy does not comprise aluminium.

### Claim 7 (depends on 1)

The Group IV metal or alloy component according to claim 1, wherein the component has a core of another material.

### Claim 8 (depends on 1)

The Group IV metal or alloy according to claim 1, wherein the component is a titanium alloy or pure titanium and has a titanium oxide layer with a cross-sectional hardness of at least 800 HV0.005.

### Claim 9 (depends on 1)

The Group IV metal or alloy according to claim 1, wherein the Group IV metal or alloy is a titanium/niobium alloy.

### Claim 10 (depends on 1)

The Group IV metal or alloy according to claim 1, wherein the Group IV metal or alloy is a zirconium alloy or pure zirconium, and the component has a zirconium oxide layer with a cross-sectional hardness of at least 1000 HV0.005.

### Claim 11

A method of producing a protective oxide surface layer on a Group IV metal or alloy, the method comprising the steps of:
providing a workpiece of a Group IV metal or alloy,
oxidising the Group IV metal or alloy in a first oxidation step at a temperature in the range of 500° C. to 900° C. using a carbon containing gaseous species having a first oxidising potential to provide an intermediary Group IV metal oxide,
oxidising the intermediary Group IV metal oxide in a second oxidation step at a temperature in the range of 300° C. to 900° C. using a second gaseous species having a second oxidising potential to provide the protective oxide surface layer, which second oxidising potential is higher than the first oxidising potential.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the carbon containing gaseous species is CO2 or a mixture of CO2 and CO.

### Claim 13 (depends on 12)

The method of claim 12, wherein the carbon containing gaseous species is a mixture of CO2 and CO, and wherein the ratio of CO2 to CO and CO2 is in the range of 0.4 to 0.9.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the second gaseous species is N2O or O2, or a combination of N2O and O2.

### Claim 15 (depends on 11)

The method according to claim 11, wherein the first gaseous species and/or the second gaseous species do not comprise hydrogen containing species.

### Claim 16 (depends on 11)

The method according to claim 11, wherein the first oxidation step is performed at a temperature in the range of 700° C. to 800° C.

### Claim 17 (depends on 11)

The method according to claim 11, wherein the second oxidation step is performed at a temperature in the range of 600° C. to 700° C.

### Claim 18 (depends on 11)

The method according to claim 11, wherein the oxidation step has a first reactive duration in the range of 0.2 hour to 24 hours.

### Claim 19 (depends on 11)

The method according to claim 11, wherein the second oxidation step has a second reactive duration in the range of 1 hour to 24 hours.

### Claim 20 (depends on 11)

The method according to claim 11, wherein the carbon containing gaseous species is CO2 or a mixture of CO2 and CO, the first oxidation step temperature is in the range of 700° C. to 800° C., and the first reactive duration is in the range of 12 hours to 24 hours, and the second gaseous species is N2O in N2 at a ratio of 20% to 40% N2O to the total of N2O in N2, the second oxidation step temperature is in the range of 600° C. to 700° C., and the second reactive duration is in the range of 12 hours to 24 hours.

### Claim 21 (depends on 11)

The method according to claim 11, wherein the first oxidation step is performed with the carbon containing gaseous species at ambient pressure and/or wherein the second oxidation step is performed with the second gaseous species at ambient pressure.

### Claim 22 (depends on 11)

The method according to claim 11, wherein the second gaseous species and/or the carbon containing gaseous species is contained in an atmosphere comprising N2 or an inert gas.

### Claim 23 (depends on 11)

The method according to claim 11, wherein the Group IV metal or alloy is selected from the list consisting of titanium, a titanium alloy, zirconium, and a zirconium alloy.

### Claim 24 (depends on 23)

The method according to claim 23, wherein the Group IV metal or alloy is titanium grade 1 to 4, Zr7022, or a titanium/niobium alloy.

### Claim 25 (depends on 11)

The method according to claim 11, wherein the Group IV alloy does not comprise aluminium.

### Claim at position 26

26-27. (canceled)