# US 2022/0280687 A1 · Method for constructing bone morphogenetic protein slow-release system

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0280687 A1
- Document ID: US20220280687A1
- Status: Published application
- Kind: A1
- Application number: 17/637,804
- Filed: 2021-07-01
- Published: 2022-09-08
- Earliest claimed: 2020-07-14
- Assignees: The 2Nd Affiliated Hospital and Yuying Children's Hospital of Wenzhou Medical University
- Applicants: The 2Nd Affiliated Hospital and Yuying Children's Hospital of Wenzhou Medical University
- Inventors: Liyan SHEN; Wenfei NI; Yanlin CHEN; Chenqiang JIN
- Web page: https://patentgrep.com/patent/US20220280687A1

## CPC

- A61L 27/06: Titanium or titanium alloys
- A61L 27/10: Ceramics or glasses
- A61L 27/227: {Other specific proteins or polypeptides not covered by A61L27/222, A61L27/225 or A61L27/24}
- A61L 27/34: Macromolecular materials
- A61L 27/54: Biologically active materials, e.g. therapeutic substances {(A61L27/227 takes precedence)}
- A61L 2300/252: Polypeptides, proteins, e.g. glycoproteins, lipoproteins, cytokines
- A61L 2300/412: Tissue-regenerating or healing or proliferative agents
- A61L 2300/414: Growth factors
- A61L 2300/602: Type of release, e.g. controlled, sustained, slow
- A61L 2300/608: having two or more layers
- A61L 2420/02: Methods for coating medical devices
- A61L 2420/08: Coatings comprising two or more layers
- A61L 2430/02: for reconstruction of bones; weight-bearing implants
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)

## Abstract

To solve the problem that an excellent carrier material is absent in a storage and use process of the bone morphogenetic protein, based on self-polymerization universality of dopamine, the positively-charged polyelectrolyte, the negatively-charged polyelectrolyte and the ceramic powder with biological activity are integrated onto the titanium base material in a layer-by-layer assembly mode to construct a bone morphogenetic protein slow-release system, so that long-acting slow release, on a lesion part, of the bone morphogenetic protein is achieved. The slow-release system has the advantages of being high in surface modulus, stable, resistant to radiation, good in biocompatibility, and the like, can effectively promote osteogenic differentiation of the mesenchymal stem cells, and can be expected to effectively promote bone repair.

## Claims

### Claim 1

A method for constructing a bone morphogenetic protein slow-release system, comprising the following steps:
I: activating a titanium material: washing and drying the titanium material, soaking the dried titanium material into a buffer solution containing dopamine, and reacting for 12-72 hours to obtain a polydopamine (PDA)-modified Ti base material;
II: activating ceramic powder: dissolving the ceramic powder and the dopamine into the buffer solution, vibrating and dispersing, reacting for 12-72 hours under stirring, and centrifuging to remove large particles, thereby obtaining a polydopamine-modified ceramic particles (PDA@HA) solution;
III: constructing a multilayer film: sequentially soaking the PDA-modified Ti base material in a positively-charged polyelectrolyte solution, a negatively-charged polyelectrolyte solution, a positively-charged polyelectrolyte solution and the PDA@HA solution for 8-15 min, and washing with water after soaking; and
IV: soaking in a circulating mode: soaking and cleaning in step III by circulating operation with circulating times of n times, thereby obtaining a positively-charged polyelectrolyte, negatively-charged polyelectrolyte and PDA-modified ceramic particles [(+/−/+/PDA@HA)n] multilayer film.

### Claim 2 (depends on 1)

The method for constructing the bone morphogenetic protein slow-release system according to claim 1, wherein the (+/−/+/PDA@HA)n multilayer film is soaked in a cross-linking solution for 6-24 hours, then washed with water and dried to obtain a cross-linked multilayer film which is recorded as a x(+/−/+/PDA@HA)n multilayer film.

### Claim 3 (depends on 1)

The method for constructing the bone morphogenetic protein slow-release system according to claim 1, wherein the buffer solution containing dopamine in step I is a Tris-HCl buffer solution with a dopamine concentration of 0.3-5.0 mg/mL, and a pH value of 8-9.

### Claim 4 (depends on 1)

The method for constructing the bone morphogenetic protein slow-release system according to claim 1, wherein the ceramic powder in step II is any one of hydroxyapatite, bioactive glass, calcium phosphate, aluminum oxide or zirconium oxide, and a weight ratio of the ceramic powder to the dopamine is (8-15) to 1.

### Claim 5 (depends on 1)

The method for constructing the bone morphogenetic protein slow-release system according to claim 1, wherein the positively-charged polyelectrolyte solution in step III is any one of a chitosan solution or a polylysine solution, with a concentration of 0.3-5.0 mg/mL; and/or, the negatively-charged polyelectrolyte solution is any one of a glucan solution, a heparin solution, a heparan sulfate solution, an alginic acid solution, a hyaluronic acid solution, a collagen solution, a gelatin solution, a carrageenan solution or a cellulose acetate solution, with a concentration of 0.3-5.0 mg/mL; and/or, the PDA@HA solution is a solution with a PDA@HA concentration of 0.3-5.0 mg/mL.

### Claim 6 (depends on 1)

The method for constructing the bone morphogenetic protein slow-release system according to claim 1, wherein the circulating times n are greater than 3.

### Claim 7 (depends on 2)

The method for constructing the bone morphogenetic protein slow-release system according to claim 2, wherein the cross-linking solution is at least one of a carbodiimide solution with a concentration of 25-70 mg/mL, a thiosuccimide solution with a concentration of 5-25 mg/mL, a glutaraldehyde solution with a mass concentration of 2.5% or a genipin solution with a mass concentration of 1-4%.

### Claim 8 (depends on 1)

A protein slow-release system, wherein the bone morphogenetic protein slow-release system is prepared by the method according to claim 1.

### Claim 9 (depends on 8)

A construction method of the bone morphogenetic protein loaded slow-release system, comprising: soaking the bone morphogenetic protein slow-release system according to claim 8 into a solution containing the bone morphogenetic protein to load; or directly dropwise adding the solution containing the bone morphogenetic protein onto the bone morphogenetic protein slow-release system.

### Claim 10 (depends on 9)

A bone morphogenetic protein loaded slow-release system, wherein the bone morphogenetic protein loaded slow-release system is prepared by the construction method according to claim 9.

### Claim 11 (depends on 2)

A protein slow-release system, wherein the bone morphogenetic protein slow-release system is prepared by the method according to claim 2.

### Claim 12 (depends on 3)

A protein slow-release system, wherein the bone morphogenetic protein slow-release system is prepared by the method according to claim 3.

### Claim 13 (depends on 4)

A protein slow-release system, wherein the bone morphogenetic protein slow-release system is prepared by the method according to claim 4.

### Claim 14 (depends on 5)

A protein slow-release system, wherein the bone morphogenetic protein slow-release system is prepared by the method according to claim 5.

### Claim 15 (depends on 6)

A protein slow-release system, wherein the bone morphogenetic protein slow-release system is prepared by the method according to claim 6.

### Claim 16 (depends on 7)

A protein slow-release system, wherein the bone morphogenetic protein slow-release system is prepared by the method according to claim 7.