# US 2022/0279792 A1 · Antimicrobial nanostructured silver perovskite oxides

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0279792 A1
- Document ID: US20220279792A1
- Status: Published application
- Kind: A1
- Application number: 17/177,202
- Filed: 2021-02-17
- Published: 2022-09-08
- Earliest claimed: 2020-02-17
- Inventors: Cyrus Talebpour; Houshang Alamdari; Hossein Salimnia
- Web page: https://patentgrep.com/patent/US20220279792A1

## CPC

- A01N 59/00: Biocides, pest repellants or attractants, or plant growth regulators containing elements or inorganic compounds
- A01N 59/16: Heavy metals; Compounds thereof
- C01G 33/00: Compounds of niobium
- C09D 5/14: Paints containing biocides, e.g. fungicides, insecticides or pesticides (C09D5/16 takes precedence)
- C01P 2002/34: perovskite-type (ABO3)
- A01N: PRESERVATION OF BODIES OF HUMANS OR ANIMALS OR PLANTS OR PARTS THEREOF (preservation of food or foodstuff A23); BIOCIDES, e.g. AS DISINFECTANTS, AS PESTICIDES OR AS HERBICIDES (preparations for medical, dental or toiletry purposes which kill or prevent the growth or proliferation of unwanted organisms A61K); PEST REPELLANTS OR ATTRACTANTS; PLANT GROWTH REGULATORS
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

The subject matter of the present invention is providing nanostructured silver perovskite oxides, which upon contact with microbial cells prevent their proliferation without releasing significant amounts of silver ions to the environment. These nanostructured oxides may be used as antimicrobial agents on exposed surfaces.

## Claims

### Claim 1

An antimicrobial silver perovskite oxide, wherein the antimicrobial silver perovskite oxide has a specific surface area of at least 1 m2/g.

### Claim 2 (depends on 1)

The method according to claim 1, where and a silver release rate of less than 0. 1% of its weight over 24 hours into deionized water at room temperature.

### Claim 3 (depends on 1)

The method according to claim 1, where antimicrobial silver perovskite oxide is selected from the group consisting of at least one of the group AgNbO3 and AgNbO3.

### Claim 4 (depends on 1)

A method of preparing the antimicrobial silver perovskite oxide of claim 1 comprising:
mixing the Ag2O powder with appropriate amounts of either Nb2O5 or Ta2O5;
heating the mixture to a formation temperature in the range of 800° C. and 1100° C.;
maintaining the mixture at the formation temperature for at least 30 minutes;
cooling down the product to ambient temperature to obtain a polycrystalline solid;
subjecting the polycrystalline solid to high energy ball milling to obtain a nanostructured silver perovskite oxide.

### Claim 5 (depends on 4)

The method according to claim 4, where the high energy ball milling is performed for a duration of at least 5 minutes.

### Claim 6 (depends on 4)

The method according to claims 4 where the nanostructured silver perovskite oxide is subjected to further treatment by subjecting it to low energy ball milling for a duration of at least 10 minutes.

### Claim 7 (depends on 6)

The method according to claim 6 where the low energy ball mill is performed in an attrition mill using a media of beads of diameters ranging between 1 mm and 5 mm.

### Claim 8 (depends on 6)

The method according to claim 6 where the milling media comprises at least one of ceramic beads, metallic beads and quartz beads.

### Claim 9 (depends on 6)

The method according to claim 6 where the treatment by low energy ball milling is performed until the specific surface area of the nanostructured silver perovskite oxide exceeds 2 m2/g.

### Claim 10 (depends on 6)

The method according to claim 6 where the treatment by low energy ball milling is performed by adding water into the milling media.

### Claim 11 (depends on 6)

The method according to claim 6 where the treatment by low energy ball milling is performed by adding alcohol into the milling media.

### Claim 12 (depends on 1)

A method of prevention of microbial proliferation in a cooling tower by adding antimicrobial silver perovskite oxide of claims 1 to the water reservoir of the cooling tower.

### Claim 13 (depends on 12)

The method according to claim 12 where the amount of the antimicrobial silver perovskite oxide added to the water is selected such that its concentration in a sludge within the water reservoir is at least 10 times higher than the minimum inhibitory concentration against Pseudomonas aeruginosa ATCC 27853.

### Claim 14 (depends on 10)

The method according to claim 10 where the amount of the antimicrobial silver perovskite oxide added to the water is selected such that its concentration in the sludge is at least 5 times higher than the minimum inhibitory concentration against Pseudomonas aeruginosa ATCC 27853.

### Claim 15 (depends on 1)

A method of preparing an antimicrobial surface, the method comprising:
dispersing the antimicrobial silver perovskite oxide of claim 1 within a matrix;
mixing the dispersion with a binder; and
treating the mixture to form a solid with an antibacterial surface.

### Claim 16 (depends on 15)

The method according to claim 15, where the matrix is glass powder with a w/w ratio of at most 99/1 relative to the antimicrobial silver perovskite oxide.

### Claim 17 (depends on 15)

The method according to claim 15, where the matrix is a polymer with a w/w ratio of at most 99/1 relative to the antimicrobial silver perovskite oxide.

### Claim 18 (depends on 15)

The method according to claim 15 where the dispersing process is performed using a ball mill.

### Claim 19 (depends on 15)

The method according to claim 15 where the dispersing process is performed in an attrition mill.

### Claim 20 (depends on 15)

The method according to claim 15, where the dispersed nanostructured mixed oxide is coated on a solid substrate to form an antimicrobial surface.